    Effect of the Chemical Properties of Silane Coupling Agents on Interfacial Bonding Strength with Thermoplastics in the Resizing of Recycled Carbon Fibers

    by Hyunkyung Lee, Minsu Kim, Gyungha Kim, Daeup Kim

    Upcycling recycled carbon fibers recovered from waste carbon composites can reduce the price of carbon fibers while improving disposal-related environmental problems. This study assessed and characterized recycled carbon fibers subjected to sizing treatment using N-(2-aminoethyl)-3-aminopropyltrimethoxysilane (APS) chemically coordinated with polyamide 6 (PA6) and polypropylene (PP) resins. Sizing treatment with 1 wt.% APS for 10 s yielded O=C-O on the surface of the carbon fiber, and the -SiOH in the APS underwent a dehydration–condensation reaction that converted O=C-O (lactone groups) into bonds of C-O (hydroxyl groups) and C=O (carbonyl groups). The effects of C-O and C=O on the interfacial bonding force increased to a maximum, resulting in an oxygen-to-carbon ratio (O/C) of 0.26. The polar/surface energy ratio showed the highest value of 32.29% at 10 s, and the interfacial bonding force showed the maximum value of 32 MPa at 10 s, which is about 15% better than that of commercial carbon fiber (PA6-based condition). In 10 s resizing treatments with 0.5 wt.% 3-methacryloxypropyltrimethoxysilane (MPS), C-O, C=O, and O=C-O underwent a dehydration–condensation reaction with -SiOH, which broke the bonds between carbon and oxygen and introduced a methacrylate group (H2C=C(CH3)CO2H), resulting in a significant increase in C-O and C=O, with an O/C of 0.51. The polar/surface free energy ratio was about 38% at 10 s, with the interfacial bonding force increasing to 27% compared to commercial carbon fiber (PP-based conditions). MPS exhibited a superior interfacial shear strength improvement, two times higher than that of APS, with excellent coordination with PP resin and commercial carbon fiber, although the interfacial bonding strength of the PP resin was significantly lower.


  • Open Access

    Effect of the Chemical Properties of Silane Coupling Agents on Interfacial Bonding Strength with Thermoplastics in the Resizing of Recycled Carbon Fibers

    by Hyunkyung Lee, Min-Su Kim, Gyungha Kim, Daeup Kim

    Upcycling recycled carbon fibers recovered from waste carbon composites can reduce the price of carbon fibers while improving disposal-related environmental problems. This study assessed and characterized recycled carbon fibers subjected to sizing treatment using N-(2-aminoethyl)-3-aminopropyltrimethoxysilane (APS) chemically coordinated with polyamide 6 (PA6) and polypropylene (PP) resins. Sizing treatment with 1 wt.% APS for 10 s yielded O=C-O on the surface of the carbon fiber, and the -SiOH in the APS underwent a dehydration-condensation reaction that converted O=C-O (lactone groups) into bonds of C-O (hydroxyl groups) and C=O (carbonyl groups). The effects of C-O and C=O on the interfacial bonding force increased to a maximum, resulting in an oxygen-to-carbon ratio (O/C) of 0.26. The polar/surface energy ratio showed the highest value of 32.29% at 10 s, and the interfacial bonding force showed the maximum value of 32 MPa at 10 s, which is about 15% better than that of commercial carbon fiber (PA6-based condition). In 10-s resizing treatments with 0.5 wt.% 3-methacryloxypropyltrimethoxysilane (MPS), C-O, C=O, and O=C-O underwent a dehydration-condensation reaction with -SiOH, which broke the bonds between carbon and oxygen and introduced a methacrylate group (H2C=C(CH3)CO2H), resulting in a significant increase in C-O and C=O, with an O/C of 0.51. The polar/surface free energy ratio was about 38% at 10 s, with the interfacial bonding force increasing to 27% compared to commercial carbon fiber (PP-based conditions). The MPS exhibited a superior interfacial shear strength improvement, two times higher than that of APS, with excellent coordination with PP resin and commercial carbon fiber, although the interfacial bonding strength of the PP resin was significantly lower.


  • Experimental study on the characteristics of a sherbet type seawater ice maker using scraper

    by Jung-In Yoon, Hyun-Kyung Lee, Min-Ju Jeon, Choon-Geun Moon, Kwang-Hwan Choi, Chang-Hyo Son

    어획물의 보관, 유통 과정에서 해수를 원수로 하는 샤베트형 얼음의 이용은 어획물의 선도 유지와 품질 면에서 좋은 방식으로 평가되고 있다. 하지만, 국내의 보관 및 유통 과정에서는 90% 이상이 담수 각 빙을 사용하며 이에 따라 품질과 신선도 측면에서 마이너스 효과를 보이고 있다. 본 연구에서는 소용량(0.55 Ton/day) 스크래퍼식 제빙기를 대상으로 해수의 입구 온도와 유량, 스크래퍼 회전수, 냉매의 증발온도, 염분 농도를 변화시켜가며 실험을 실시하여 샤베트형 해수빙의 형태와 제빙량, 빙충전율(IPF)을 알아보았으며, 그 결과는 다음과 같다. (1) 생성된 샤베트형 해수빙은 흰 색의 유동성을 가진 유체로, 얼음 입자의 크기는 직경 0.2 mm ~ 0.3 mm로 측정되었다. (2) 해수의 입구 온도가 낮을수록, 유량이 적을수록 IPF는 증가하며, 표준 조건에서 제빙량은 0.55 Ton/day를 보였다. (3) 스크래퍼 회전수가 증가할수록 IPF는 증가하며 해수의 염분 농도에 따른 IPF 변화는 미미하다. (4) 냉매의 증발온도가 낮아질수록 IPF는 증가하는 경향을 보인다. 이러한 결과는 샤베트형 해수 제빙장치 설계를 위한 중요한 자료가 되리라 판단된다.