Meng-Shung Yen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Meng-Shung Yen has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
Hsiang-Chin Tsai
Department of Polymer Engineering, National Taiwan University of Science and Technology, No. 43, Sec. 4, Keelung Rd., Taipei 106-72, Taiwan, Republic of China
1 shared publicationHsiang‐Chin Tsai
Department of Polymer Engineering, National Taiwan University of Science and Technology, Taipei 106-72, Taiwan, Republic of China
1 shared publicationPo-Da Hong
Department of Polymer Engineering, National Taiwan University of Science and Technology, No. 43, Sec. 4, Keelung Rd., Taipei 106-72, Taiwan, Republic of China
1 shared publicationPo‐Da Hong
Department of Polymer Engineering, National Taiwan University of Science and Technology, Taipei 106-72, Taiwan, Republic of China
1 shared publication
Latest Publications
- 1 September 2007
- Published by SAGE Publications in Textile Research Journal
- Vol. 77 (9) , 710-720
Preparation and Physical Properties of MDEA-based Polyurethane Cationomers and their Application to Textile Coatings
Cationic aqueous polyurethane (CAPU) coatings were prepared by the acetone process using 4,4-methylene bis (isocyantocyclohexane) (H12MDI), N-methyldiethyolamine (N-MDEA) and a series of various polydiols (polyethylene glycol (PEG), polypropylene glycol (PPG) and polytetramethylene glycol (PTMG) for ether-type polyols and polycaprolactone (PCL) for ester-type polyol) with different molecular weights (Mn =1000, 2000 and 3000 g/mole). The surface tension of CAPU dispersion, contact angle, thermal properties of CAPU casting film and its tensile strength were examined. The waterproof (WP) and water vapor permeability (WVP) of coated fabric and its washing durability were also studied. Our results showed the ether-based CAPU showed a higher surface tension value, contact angle and WVP with a sequence of PEG-PU > PTMG-PU > PPG-PU > PCL-PU, and it increased with increasing M n of the soft segment. As for the thermal properties, the PEG-PU had the highest glass transition temperatures of the soft segment (Tgs) and melting point (Tms) than those of PCL -PU, PTMG-PU and PPG-PU. For the thermal stability of CAPUs casting film, the PEG-PU had ideal thermal stability, followed by PTMG-PU and PCL -PU, and the CAPU with a larger M n of the soft segment had better thermal stability. The PTMG-PU had excellent tensile strength, followed by PCL -PU and PPG-PU. For coated fabric, the trend of WVP followed the order: PEG-PU > PTMG-PU > PPG-PU > PCL -PU, while the WP followed the order: PTMG-PU > PCLPU > PPG-PU > PEG-PU. Finally, the CAPUcoated fabric had an excellent performance after washing and its wash-durability was still 80 %.
- 1 September 2007
- Published by SAGE Publications in Textile Research Journal
- Vol. 77 (9) , 710-720
Preparation and Physical Properties of MDEA-based Polyurethane Cationomers and their Application to Textile Coatings
Cationic aqueous polyurethane (CAPU) coatings were prepared by the acetone process using 4,4-methylene bis (isocyantocyclohexane) (H12MDI), N-methyldiethyolamine (N-MDEA) and a series of various polydiols (polyethylene glycol (PEG), polypropylene glycol (PPG) and polytetramethylene glycol (PTMG) for ether-type polyols and polycaprolactone (PCL) for ester-type polyol) with different molecular weights (Mn =1000, 2000 and 3000 g/mole). The surface tension of CAPU dispersion, contact angle, thermal properties of CAPU casting film and its tensile strength were examined. The waterproof (WP) and water vapor permeability (WVP) of coated fabric and its washing durability were also studied. Our results showed the ether-based CAPU showed a higher surface tension value, contact angle and WVP with a sequence of PEG-PU > PTMG-PU > PPG-PU > PCL-PU, and it increased with increasing M n of the soft segment. As for the thermal properties, the PEG-PU had the highest glass transition temperatures of the soft segment (Tgs) and melting point (Tms) than those of PCL -PU, PTMG-PU and PPG-PU. For the thermal stability of CAPUs casting film, the PEG-PU had ideal thermal stability, followed by PTMG-PU and PCL -PU, and the CAPU with a larger M n of the soft segment had better thermal stability. The PTMG-PU had excellent tensile strength, followed by PCL -PU and PPG-PU. For coated fabric, the trend of WVP followed the order: PEG-PU > PTMG-PU > PPG-PU > PCL -PU, while the WP followed the order: PTMG-PU > PCLPU > PPG-PU > PEG-PU. Finally, the CAPUcoated fabric had an excellent performance after washing and its wash-durability was still 80 %.
- 23 April 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (3) , 1391-1399
Effect of soft segment composition on the physical properties of nonionic aqueous polyurethane containing side chain PEGME
In this study, a series of nonionic waterborne polyurethanes containing side chain poly(ethylene glycol) monomethyl ether (PEGME) were synthesized using 4,4‐methylene bis(isocyanatocyclohexane), the nonionic dispersing center produced by isophorone diisocyanate, N‐diethanol amine, and PEGME, and a series of soft segments [polyethylene glycol (PEG), polypropylene glycol (PPG), polytetramethylene glycol (PTMG), and polycaprolactone (PCL)] with a different molecular weight. The solution properties of the polyurethane (PU) dispersions, thermal properties of the PU casting films, and the water vapor permeability (WVP) of the PU coated fabrics were investigated. Our results show that the surface tension of PU dispersion and its contact angle to untreated nylon fabric are higher for the ether‐based PU dispersion than for the ester‐based PU dispersion, with a sequence of PEG‐PU ≫ PTMG‐PU ≫ PPG‐PU ≫ PCL‐PU. Both the surface tension and the contact angle between PU dispersion and nylon fabric increase upon increasing the Mw of the soft segment. As for the thermal property of PU film, the Tgs of PCL‐PU is the highest, followed by PEG‐PU, PTMG‐PU, and PPG‐PU, and the Tgs decreases with the increase in the length of the soft segment. The Tms follows the order: PEG‐PU ≫ PCL‐PU ≫ PPG‐PU ≫ PTMG‐PU, and the Tms increases upon increasing the soft segment length. As regard to PU coated fabric, the trend of WVP is PEG‐PU ≫ PTMG‐PU ≫ PPG‐PU ≫ PCL‐PU, which increases with the increasing the soft segment length. With regarding to application for the coating, the Coated‐PU with PEG‐PU has an excellent WVP. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007
- 23 April 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (3) , 1391-1399
Effect of soft segment composition on the physical properties of nonionic aqueous polyurethane containing side chain PEGME
In this study, a series of nonionic waterborne polyurethanes containing side chain poly(ethylene glycol) monomethyl ether (PEGME) were synthesized using 4,4‐methylene bis(isocyanatocyclohexane), the nonionic dispersing center produced by isophorone diisocyanate, N‐diethanol amine, and PEGME, and a series of soft segments [polyethylene glycol (PEG), polypropylene glycol (PPG), polytetramethylene glycol (PTMG), and polycaprolactone (PCL)] with a different molecular weight. The solution properties of the polyurethane (PU) dispersions, thermal properties of the PU casting films, and the water vapor permeability (WVP) of the PU coated fabrics were investigated. Our results show that the surface tension of PU dispersion and its contact angle to untreated nylon fabric are higher for the ether‐based PU dispersion than for the ester‐based PU dispersion, with a sequence of PEG‐PU ≫ PTMG‐PU ≫ PPG‐PU ≫ PCL‐PU. Both the surface tension and the contact angle between PU dispersion and nylon fabric increase upon increasing the Mw of the soft segment. As for the thermal property of PU film, the Tgs of PCL‐PU is the highest, followed by PEG‐PU, PTMG‐PU, and PPG‐PU, and the Tgs decreases with the increase in the length of the soft segment. The Tms follows the order: PEG‐PU ≫ PCL‐PU ≫ PPG‐PU ≫ PTMG‐PU, and the Tms increases upon increasing the soft segment length. As regard to PU coated fabric, the trend of WVP is PEG‐PU ≫ PTMG‐PU ≫ PPG‐PU ≫ PCL‐PU, which increases with the increasing the soft segment length. With regarding to application for the coating, the Coated‐PU with PEG‐PU has an excellent WVP. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007