Gao Yue
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Gao Yue has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
- Fei Liu
School of Mechanical and Electrical Engineering, Guilin University of Electronic Technology, Guilin 541004, China
2 shared publications - Jingjing Qu
School of Mechanical and Electrical Engineering, Guilin University of Aerospace Technology, Guilin 541004, China
2 shared publications - Siliang He
School of Mechanical and Electrical Engineering, Guilin University of Electronic Technology, Guilin 541004, China
2 shared publications - Yu-Cheng Luo
Guilin Fuda Co., Ltd., Guilin 541199, China
2 shared publications - Bifu Xiong
Guangxi Education Department Key Laboratory of Microelectronic Packaging & Assembly Technology, School of Mechanical & Electrical Engineering, Guilin University of Electronic Technology, Guilin 541004, China
1 shared publication Bin Huang
1 shared publication
Latest Publications
- Open Access
Oxidation Behavior and Failure Mechanism of MoSi2/WSi2/NbSi2 Compound Coating on Nb-Si-Based Alloy at 1250 °C
The oxidation behavior of a MoSi2/WSi2/NbSi2 compound coating prepared on a Nb-Si-based alloy through a two-step method upon oxidation at 1250 °C was investigated, and its possible failure mechanism after long-term oxidation was also discussed. In this study, the MoSi2, WSi2 and NbSi2 layers were assigned as the outermost anti-oxidation layer, the middle diffusion barrier layer and the innermost buffering layer, respectively. The oxidation results indicated that this coating had admirable oxidation resistance at 1250 °C. After oxidation for 100 h, a dense SiO2-based scale with thickness of about 6.5 μm formed on the coating surface, and the parabolic rate constant of scale growth is about 0.42 μm2/h within 100 h. The presence of the NbSi2 layer could suppress the fast degradation of WSi2 into W5Si3 by providing sufficient Si, while migration of W could cause the formation of Kirkendall voids in the WSi2 layer and then impair its diffusion performance. Due to the diffusion of Si and internal oxidation, there was massive formation of Nb5Si3 phases in the NbSi2 layer. During the oxidation process, oxidation of NbSi2 and reactive elements like Hf and Al also occurred inside the vertical cracks, and this process might promote formation and expansion of penetrable cracks through the compound coating. The persistent internal oxidation inside the penetrable cracks and at the WSi2/NbSi2 layer interface was ultimately likely to induce fracture and spallation of the MoSi2/WSi2 layer after long-term oxidation at 1250 °C.
Open AccessOxidation Behavior and Failure Mechanism of MoSi2/WSi2/NbSi2 Compound Coating on Nb-Si-Based Alloy at 1250 °C
The oxidation behavior of a MoSi2/WSi2/NbSi2 compound coating prepared on a Nb-Si-based alloy through a two-step method upon oxidation at 1250 °C was investigated, and its possible failure mechanism after long-term oxidation was also discussed. In this study, the MoSi2, WSi2 and NbSi2 layers were assigned as the outermost anti-oxidation layer, the middle diffusion barrier layer and the innermost buffering layer, respectively. The oxidation results indicated that this coating had admirable oxidation resistance at 1250 °C. After oxidation for 100 h, a dense SiO2-based scale with thickness of about 6.5 μm formed on the coating surface, and the parabolic rate constant of scale growth is about 0.42 μm2/h within 100 h. The presence of the NbSi2 layer could suppress the fast degradation of WSi2 into W5Si3 by providing sufficient Si, while migration of W could cause the formation of Kirkendall voids in the WSi2 layer and then impair its diffusion performance. Due to the diffusion of Si and internal oxidation, there was massive formation of Nb5Si3 phases in the NbSi2 layer. During the oxidation process, oxidation of NbSi2 and reactive elements like Hf and Al also occurred inside the vertical cracks, and this process might promote formation and expansion of penetrable cracks through the compound coating. The persistent internal oxidation inside the penetrable cracks and at the WSi2/NbSi2 layer interface was ultimately likely to induce fracture and spallation of the MoSi2/WSi2 layer after long-term oxidation at 1250 °C.
- Open Access
Effect of Scanning Electron Beam Pretreatment on Gas Carburization of 22CrMoH Gear Steel
22CrMoH was selected for the gear steel material in this work, and the temperature field change in the scanning electron beam was analyzed to determine the optimal scanning parameters and explored the effect of scanning electron beam pretreatment (Abbreviated as: SEBP) on gas-carburizing (GC) efficiency and organizational properties of gear steel. The results showed that the scanning electron beam caused the material to form a thermally deformed layer 110 μm thick, and it promoted the adsorption of carbon atoms on the surface and their inward diffusion. Under the same gas-carburizing conditions, the carburizing efficiency was improved, and the thickness of the carburized layer increased from 0.78 to 1.09 mm. Furthermore, the hardness of the GC specimens with the SEBP increased from 615 to 638 HV0.05 at 0.1 mm of the sample surface, whereas the hardness of the cross-sectional region decreased gradually, indicating that the scanning electron beam enhanced the adhesion between the carburized layer and matrix zone. A comparative analysis of the microstructures of the GC specimens with and without the SEBP showed that the carbide particles in the surface layer of the samples become smaller and that of volume fraction of residual austenite reduced in size. In terms of the mechanical properties, the surface friction coefficient decreased from 0.87 to 0.46 μ and the GC specimen with the SEBP had a higher cross-sectional hardness gradient. In this way, the amount of wear was reduced from 1.07 to 0.51 mg, which was only 47.7% of the amount of wear of the matrix specimen.
Open AccessEffect of Scanning Electron Beam Pretreatment on Gas Carburization of 22CrMoH Gear Steel
22CrMoH was selected for the gear steel material in this work, and the temperature field change in the scanning electron beam was analyzed to determine the optimal scanning parameters and explored the effect of scanning electron beam pretreatment (Abbreviated as: SEBP) on gas-carburizing (GC) efficiency and organizational properties of gear steel. The results showed that the scanning electron beam caused the material to form a thermally deformed layer 110 μm thick, and it promoted the adsorption of carbon atoms on the surface and their inward diffusion. Under the same gas-carburizing conditions, the carburizing efficiency was improved, and the thickness of the carburized layer increased from 0.78 to 1.09 mm. Furthermore, the hardness of the GC specimens with the SEBP increased from 615 to 638 HV0.05 at 0.1 mm of the sample surface, whereas the hardness of the cross-sectional region decreased gradually, indicating that the scanning electron beam enhanced the adhesion between the carburized layer and matrix zone. A comparative analysis of the microstructures of the GC specimens with and without the SEBP showed that the carbide particles in the surface layer of the samples become smaller and that of volume fraction of residual austenite reduced in size. In terms of the mechanical properties, the surface friction coefficient decreased from 0.87 to 0.46 μ and the GC specimen with the SEBP had a higher cross-sectional hardness gradient. In this way, the amount of wear was reduced from 1.07 to 0.51 mg, which was only 47.7% of the amount of wear of the matrix specimen.
- 13 October 2023
- Published by Elsevier in Engineering Failure Analysis
- Vol. 154
Fatigue fracture analysis of the 42CrMo4 crankshaft used for mining dump truck
- 13 October 2023
- Published by Elsevier in Engineering Failure Analysis
- Vol. 154
Fatigue fracture analysis of the 42CrMo4 crankshaft used for mining dump truck
- Open Access
Low-Temperature Transient Liquid Phase Bonding Technology via Cu Porous-Sn58Bi Solid–Liquid System under Formic Acid Atmosphere
This study proposes a low-temperature transient liquid phase bonding (TLPB) method using Sn58Bi/porous Cu/Sn58Bi to enable efficient power-device packaging at high temperatures. The bonding mechanism is attributed to the rapid reaction between porous Cu and Sn58Bi solder, leading to the formation of intermetallic compounds with high melting point at low temperatures. The present paper investigates the effects of bonding atmosphere, bonding time, and external pressure on the shear strength of metal joints. Under formic acid (FA) atmosphere, Cu6Sn5 forms at the porous Cu foil/Sn58Bi interface, and some of it transforms into Cu3Sn. External pressure significantly reduces the micropores and thickness of the joint interconnection layer, resulting in a ductile fracture failure mode. The metal joint obtained under a pressure of 10 MPa at 250 °C for 5 min exhibits outstanding bonding mechanical performance with a shear strength of 62.2 MPa.
Open AccessLow-Temperature Transient Liquid Phase Bonding Technology via Cu Porous-Sn58Bi Solid–Liquid System under Formic Acid Atmosphere
This study proposes a low-temperature transient liquid phase bonding (TLPB) method using Sn58Bi/porous Cu/Sn58Bi to enable efficient power-device packaging at high temperatures. The bonding mechanism is attributed to the rapid reaction between porous Cu and Sn58Bi solder, leading to the formation of intermetallic compounds with high melting point at low temperatures. The present paper investigates the effects of bonding atmosphere, bonding time, and external pressure on the shear strength of metal joints. Under formic acid (FA) atmosphere, Cu6Sn5 forms at the porous Cu foil/Sn58Bi interface, and some of it transforms into Cu3Sn. External pressure significantly reduces the micropores and thickness of the joint interconnection layer, resulting in a ductile fracture failure mode. The metal joint obtained under a pressure of 10 MPa at 250 °C for 5 min exhibits outstanding bonding mechanical performance with a shear strength of 62.2 MPa.