Putsadeeporn Thammajaruk
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Putsadeeporn Thammajaruk has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
Massimiliano Guazzato
Discipline of Prosthodontics, School of Dentistry, Faculty of Medicine and Health, The University of Sydney, NSW 2145, Australia
10 shared publicationsSupanee Buranadham
Department of Prosthetic Dentistry, Faculty of Dentistry, Prince of Songkla University, Hat-Yai, Songkhla, Thailand
4 shared publicationsYu Wang
Mark Wainwright Analytical Centre, Chemical Sciences Building (F10), University Mall, The University of New South Wales, Sydney, Australia
3 shared publications- Chaimongkon Peampring
Department of Prosthetic Dentistry, Research Center of Excellence for Oral Health Faculty of Dentistry, Prince of Songkla University, Hat Yai, Thailand
2 shared publications Michael V. Swain
AMME, Biomechanics Engineering, The University of Sydney, NSW 2145, Australia
2 shared publicationsChanya Chuenarrom
Department of Prosthetic Dentistry, Faculty of Dentistry, Prince of Songkla University, Songkhla 90110, Thailand
1 shared publication
Latest Publications
- 10 June 2026
- Published by Elsevier in Dental Materials
- Vol. 42 (11) , 2119-2125
Comparative wear behavior of lithium disilicate CAD/CAM ceramics under simulated mastication
- 10 June 2026
- Published by Elsevier in Dental Materials
- Vol. 42 (11) , 2119-2125
Comparative wear behavior of lithium disilicate CAD/CAM ceramics under simulated mastication
- Open Access
- 1 January 2026
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 70 (2) , 183-191
Cleaning methods of contaminated lithium disilicate ceramics: A systematic review and network meta-analysis
Purpose: To evaluate the effects of various cleaning methods on the bond strength between lithium disilicate (LS2) ceramics and resin cement under short- and long-term aging conditions using network meta-analysis (NMA) and pairwise meta-analysis (PMA).Study selection: An electronic search of seven databases (PubMed, Scopus, Embase, Web of Science, Google Scholar, Defense Technical Information Center, and LILACS) with a manual search of the reference lists was conducted for articles published up to March 10, 2025. Eligible studies included those that assessed the bond strength of LS2, either uncontaminated or contaminated with human saliva, fit-checking materials, try-in paste, or their combinations, using different cleaning methods. Risk of bias was evaluated using the RoBDEMAT tool. A frequentist multivariable random-effects model was used to calculate the effect sizes.Results: Fifteen studies met the inclusion criteria. Under short-term aging conditions, NMA showed higher bond strengths in the uncontaminated LS2 group and the contaminated groups cleaned with hydrofluoric acid etching, commercial ceramic cleaning agents, or phosphoric acid etching than those uncleaned or cleaned with water or alcohol. In long-term aging, PMA and NMA exhibited higher bond strengths in the uncontaminated LS2 group and contaminated group cleaned with phosphoric acid etching than those contaminated groups cleaned with water or alcohol.Conclusions: Phosphoric acid etching effectively eliminates contaminants, whereas the application of water or alcohol is ineffective. Although ceramic cleaning agents effectively decontaminate surfaces under short-term aging conditions, their performance deteriorates over time, potentially compromising long-term bond durability.
- 1 January 2026
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 70 (2) , 183-191
Open AccessCleaning methods of contaminated lithium disilicate ceramics: A systematic review and network meta-analysis
Purpose: To evaluate the effects of various cleaning methods on the bond strength between lithium disilicate (LS2) ceramics and resin cement under short- and long-term aging conditions using network meta-analysis (NMA) and pairwise meta-analysis (PMA).Study selection: An electronic search of seven databases (PubMed, Scopus, Embase, Web of Science, Google Scholar, Defense Technical Information Center, and LILACS) with a manual search of the reference lists was conducted for articles published up to March 10, 2025. Eligible studies included those that assessed the bond strength of LS2, either uncontaminated or contaminated with human saliva, fit-checking materials, try-in paste, or their combinations, using different cleaning methods. Risk of bias was evaluated using the RoBDEMAT tool. A frequentist multivariable random-effects model was used to calculate the effect sizes.Results: Fifteen studies met the inclusion criteria. Under short-term aging conditions, NMA showed higher bond strengths in the uncontaminated LS2 group and the contaminated groups cleaned with hydrofluoric acid etching, commercial ceramic cleaning agents, or phosphoric acid etching than those uncleaned or cleaned with water or alcohol. In long-term aging, PMA and NMA exhibited higher bond strengths in the uncontaminated LS2 group and contaminated group cleaned with phosphoric acid etching than those contaminated groups cleaned with water or alcohol.Conclusions: Phosphoric acid etching effectively eliminates contaminants, whereas the application of water or alcohol is ineffective. Although ceramic cleaning agents effectively decontaminate surfaces under short-term aging conditions, their performance deteriorates over time, potentially compromising long-term bond durability.
- Open Access
- 1 January 2025
- Published by XMLink in The Journal of Advanced Prosthodontics
- Vol. 17 (3) , 146-157
Fracture strength and failure mode of implant-supported provisional resin composite crowns on hydroxyapatite-coated sulfonated PEEK abutments following thermomechanical loading
Htay TP, et al. J Adv Prosthodont. 2025 Jun;17(3):146-157. https://doi.org/10.4047/jap.2025.17.3.146
- 1 January 2025
- Published by XMLink in The Journal of Advanced Prosthodontics
- Vol. 17 (3) , 146-157
Open AccessFracture strength and failure mode of implant-supported provisional resin composite crowns on hydroxyapatite-coated sulfonated PEEK abutments following thermomechanical loading
Htay TP, et al. J Adv Prosthodont. 2025 Jun;17(3):146-157. https://doi.org/10.4047/jap.2025.17.3.146
- 26 August 2024
- Published by Wiley in Journal of Prosthodontics
- Vol. 35 (7) , 1086-1095
Investigating the impact of different cleaning techniques on bond strength between resin cement and zirconia and the resulting physical and chemical surface alterations
Purpose: To evaluate the effect of cleaning methods and thermocycling on the micro‐tensile bond strength between resin cement and contaminated zirconia and to characterize the physicochemical alterations at the zirconia surface resulting from contaminants and subsequent application of cleaning methods.Materials and Methods: Thirty‐two alumina air‐abraded zirconia blocks were divided into eight groups: (i) uncontaminated control followed by methacryloyloxydecyl dihydrogen phosphate (MDP) primer (G‐Multi Primer) application (CON). In groups ii–viii, the blocks were contaminated with saliva and silicone disclosing agents, followed by cleaning as follows: (ii) MDP primer applied, followed by contamination (GMP1); (iii) MDP primer applied before and after contamination (GMP2); (iv) cleaning with alumina air‐abrasion (APA); (v) cleaning with sodium hypochlorite (NaOCl); (vi) cleaning with Ivoclean (IVC); (vii) cleaning with ZirClean (ZC); and (viii) cleaning with Katana Cleaner (KC). After cleaning, the zirconia blocks in groups iv–viii were applied with MDP primer. The blocks in each group were cemented together with resin cement (G‐Cem Linkforce). Subsequently, each bonded zirconia block was sectioned using a water‐cooled diamond saw into microsticks (1 × 1 × 9 mm3). Micro‐tensile bond strength was measured after either 24 h or 10,000 thermal cycles (n = 20/subgroup). Data were analyzed using two‐way analysis of variance (ANOVA), followed by one‐way ANOVA, and Tukey's post‐hoc test. The contact angle measurements, energy dispersive X‐ray spectroscopy (EDS), and Fourier‐transform infrared (FTIR) spectrometer were used for physiochemical evaluation.Results: After 24 h of water storage, the highest bond strength was observed in the CON, NaOCl, APA, and GMP2 groups. After thermocycling, the bond strength significantly decreased in all groups except the GMP2 group, which maintained the highest bond strength. Commercial ceramic cleaning agents (IVC, ZC, and KC groups) exhibited lower bond strengths than the CON groups in both aging conditions.Conclusions: The application of MDP primer before and after contamination is a promising cleaning protocol for removing saliva and silicone disclosing agent contaminants from zirconia surfaces. This approach achieved the highest bond strength and maintained it even after artificial aging through thermocycling.
- 26 August 2024
- Published by Wiley in Journal of Prosthodontics
- Vol. 35 (7) , 1086-1095
Investigating the impact of different cleaning techniques on bond strength between resin cement and zirconia and the resulting physical and chemical surface alterations
Purpose: To evaluate the effect of cleaning methods and thermocycling on the micro‐tensile bond strength between resin cement and contaminated zirconia and to characterize the physicochemical alterations at the zirconia surface resulting from contaminants and subsequent application of cleaning methods.Materials and Methods: Thirty‐two alumina air‐abraded zirconia blocks were divided into eight groups: (i) uncontaminated control followed by methacryloyloxydecyl dihydrogen phosphate (MDP) primer (G‐Multi Primer) application (CON). In groups ii–viii, the blocks were contaminated with saliva and silicone disclosing agents, followed by cleaning as follows: (ii) MDP primer applied, followed by contamination (GMP1); (iii) MDP primer applied before and after contamination (GMP2); (iv) cleaning with alumina air‐abrasion (APA); (v) cleaning with sodium hypochlorite (NaOCl); (vi) cleaning with Ivoclean (IVC); (vii) cleaning with ZirClean (ZC); and (viii) cleaning with Katana Cleaner (KC). After cleaning, the zirconia blocks in groups iv–viii were applied with MDP primer. The blocks in each group were cemented together with resin cement (G‐Cem Linkforce). Subsequently, each bonded zirconia block was sectioned using a water‐cooled diamond saw into microsticks (1 × 1 × 9 mm3). Micro‐tensile bond strength was measured after either 24 h or 10,000 thermal cycles (n = 20/subgroup). Data were analyzed using two‐way analysis of variance (ANOVA), followed by one‐way ANOVA, and Tukey's post‐hoc test. The contact angle measurements, energy dispersive X‐ray spectroscopy (EDS), and Fourier‐transform infrared (FTIR) spectrometer were used for physiochemical evaluation.Results: After 24 h of water storage, the highest bond strength was observed in the CON, NaOCl, APA, and GMP2 groups. After thermocycling, the bond strength significantly decreased in all groups except the GMP2 group, which maintained the highest bond strength. Commercial ceramic cleaning agents (IVC, ZC, and KC groups) exhibited lower bond strengths than the CON groups in both aging conditions.Conclusions: The application of MDP primer before and after contamination is a promising cleaning protocol for removing saliva and silicone disclosing agent contaminants from zirconia surfaces. This approach achieved the highest bond strength and maintained it even after artificial aging through thermocycling.
- 22 November 2023
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 27 (12) , 7833-7840
Effect of glass–ceramic coating versus alumina air-abrasion on the bond strength and residual stress of zirconia
Objectives To assess the effect of glass–ceramic coated zirconia versus alumina air-abraded zirconia on the shear bond strength (SBS) of resin cement and investigate the residual stresses present on both mechanically pre-treated surfaces. Materials and Methods A total of 180 zirconia disks, with diameters of 10 mm and 5 mm, were divided into two groups: DCMhotbond glass–ceramic coated, followed by hydrofluoric acid etching (DCM), and alumina air-abraded (AB). All mechanically pre-treated disks were conditioned with G-Multi Primer and bonded using G-Cem Linkforce Cement. Ninety specimens were immersed in distilled water for 24 h and subsequently allocated into three groups based on aging conditions (n = 15/subgroups): immediate testing, 5000 thermal cycles, and 10,000 thermal cycles. Then, the shear bond strength was assessed, and the obtained data were subjected to analysis using a two-way ANOVA, followed by a one-way ANOVA and Tukey's HSD post hoc test (α = 0.05). The residual stresses present on both mechanically pre-treated surfaces were examined using X-ray diffraction analysis. Results The mean SBS values of the DCM and AB groups showed no significant difference under each aging condition. The SBS of DCM groups was not affected by thermal cycles, whereas the SBS of AB groups exhibited a significant decrease following thermal cycles. Glass–ceramic coated surfaces exhibited higher compressive stresses than alumina air-abrasion. Conclusions The DCMhotbond glass–ceramic coated zirconia showed comparable bond strength to the alumina air-abrasion technique. Clinical Relevance The DCMhotbond glass–ceramic coating technique is a promising alternative for zirconia surface pre-treatment. However, further investigations are needed before suggesting its clinical use.
- 22 November 2023
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 27 (12) , 7833-7840
Effect of glass–ceramic coating versus alumina air-abrasion on the bond strength and residual stress of zirconia
Objectives To assess the effect of glass–ceramic coated zirconia versus alumina air-abraded zirconia on the shear bond strength (SBS) of resin cement and investigate the residual stresses present on both mechanically pre-treated surfaces. Materials and Methods A total of 180 zirconia disks, with diameters of 10 mm and 5 mm, were divided into two groups: DCMhotbond glass–ceramic coated, followed by hydrofluoric acid etching (DCM), and alumina air-abraded (AB). All mechanically pre-treated disks were conditioned with G-Multi Primer and bonded using G-Cem Linkforce Cement. Ninety specimens were immersed in distilled water for 24 h and subsequently allocated into three groups based on aging conditions (n = 15/subgroups): immediate testing, 5000 thermal cycles, and 10,000 thermal cycles. Then, the shear bond strength was assessed, and the obtained data were subjected to analysis using a two-way ANOVA, followed by a one-way ANOVA and Tukey's HSD post hoc test (α = 0.05). The residual stresses present on both mechanically pre-treated surfaces were examined using X-ray diffraction analysis. Results The mean SBS values of the DCM and AB groups showed no significant difference under each aging condition. The SBS of DCM groups was not affected by thermal cycles, whereas the SBS of AB groups exhibited a significant decrease following thermal cycles. Glass–ceramic coated surfaces exhibited higher compressive stresses than alumina air-abrasion. Conclusions The DCMhotbond glass–ceramic coated zirconia showed comparable bond strength to the alumina air-abrasion technique. Clinical Relevance The DCMhotbond glass–ceramic coating technique is a promising alternative for zirconia surface pre-treatment. However, further investigations are needed before suggesting its clinical use.
- 14 October 2023
- Published by Elsevier in Dental Materials
- Vol. 39 (12) , 1180-1189
Effective luting agents for glass-fiber posts: A network meta-analysis
- 14 October 2023
- Published by Elsevier in Dental Materials
- Vol. 39 (12) , 1180-1189
Effective luting agents for glass-fiber posts: A network meta-analysis
- 6 February 2023
- Published by Elsevier in Dental Materials
- Vol. 39 (3) , 235-245
Cleaning methods of contaminated zirconia: A systematic review and meta-analysis
- 6 February 2023
- Published by Elsevier in Dental Materials
- Vol. 39 (3) , 235-245
Cleaning methods of contaminated zirconia: A systematic review and meta-analysis
- 19 August 2022
- Published by Elsevier in Journal of Dentistry
- Vol. 125, 104266
Comparison of different artificial landmarks and scanning patterns on the complete-arch implant intraoral digital scans
- 19 August 2022
- Published by Elsevier in Journal of Dentistry
- Vol. 125, 104266
Comparison of different artificial landmarks and scanning patterns on the complete-arch implant intraoral digital scans
- 4 January 2022
- Published by Elsevier in Dental Materials
- Vol. 38 (2) , e31-e42
Influence of ceramic-coating techniques on composite-zirconia bonding: Strain energy release rate evaluation
- 4 January 2022
- Published by Elsevier in Dental Materials
- Vol. 38 (2) , e31-e42
Influence of ceramic-coating techniques on composite-zirconia bonding: Strain energy release rate evaluation
- 1 May 2021
- Vol. 23 (3) , 267-275
Shear Bond Strength of Composite Cement to Lithium-Disilicate Glass-coated Zirconia Versus Alumina Air-abraded Zirconia
Purpose: To compare the shear bond strength of composite cement to lithium-disilicate glass-ceramic coated zirconia vs to alumina air-abraded zirconia and to analyze the residual stresses on both of lithium-disilicate glass-ceramic coated zirconia vs alumina air-abraded zirconia specimens. Materials and Methods: One hundred eighty zirconia disks (diameters 10 mm and 5 mm, 4.5 mm thick) were divided into two groups: lithium-disilicate glass-ceramic coating followed by hydrofluoric acid etching and Monobond N Primer (LiDi) or alumina air-abrasion (AA). For each group, two different sizes of identically pre-treated zirconia specimens were bonded with Multilink Speed Cement. A total of 90 specimens were stored in distilled water at 37 degrees C for 24 h and then assigned to three subgroups (n = 15/test group): 1. short-term test; 2. thermocycling for 5000 cycles; 3. thermocycling for 10,000 cycles. Bond strength was tested in shear mode and results were analyzed using two-way ANOVA, followed by one-way ANOVA and Tukey's HSD (alpha = 0.05). Failure mode and surfaces were analyzed with optical and scanning electron microscopy. X-ray diffraction was used to analyze t-m phase transformation and residual stresses on mechanically pre-treated LiDi and AA surfaces. Results: The LiDi groups recorded higher mean bond strength than AA groups after thermocycling (p < 0.05). Thermocycling did not affect the bond strength of either LiDi or AA groups (p > 0.05). Most of specimens in AA groups exhibited mixed failure. Alumina air-abraded surfaces exhibited higher residual compressive stresses than did surfaces with a lithium-disilicate glass-ceramic coating. Conclusion: Following thermocycling, composite-zirconia bond strength of specimens with a lithium-disilicate glass-ceramic coating was greater than that of alumina air-abraded specimens.
- 1 May 2021
- Vol. 23 (3) , 267-275
Shear Bond Strength of Composite Cement to Lithium-Disilicate Glass-coated Zirconia Versus Alumina Air-abraded Zirconia
Purpose: To compare the shear bond strength of composite cement to lithium-disilicate glass-ceramic coated zirconia vs to alumina air-abraded zirconia and to analyze the residual stresses on both of lithium-disilicate glass-ceramic coated zirconia vs alumina air-abraded zirconia specimens. Materials and Methods: One hundred eighty zirconia disks (diameters 10 mm and 5 mm, 4.5 mm thick) were divided into two groups: lithium-disilicate glass-ceramic coating followed by hydrofluoric acid etching and Monobond N Primer (LiDi) or alumina air-abrasion (AA). For each group, two different sizes of identically pre-treated zirconia specimens were bonded with Multilink Speed Cement. A total of 90 specimens were stored in distilled water at 37 degrees C for 24 h and then assigned to three subgroups (n = 15/test group): 1. short-term test; 2. thermocycling for 5000 cycles; 3. thermocycling for 10,000 cycles. Bond strength was tested in shear mode and results were analyzed using two-way ANOVA, followed by one-way ANOVA and Tukey's HSD (alpha = 0.05). Failure mode and surfaces were analyzed with optical and scanning electron microscopy. X-ray diffraction was used to analyze t-m phase transformation and residual stresses on mechanically pre-treated LiDi and AA surfaces. Results: The LiDi groups recorded higher mean bond strength than AA groups after thermocycling (p < 0.05). Thermocycling did not affect the bond strength of either LiDi or AA groups (p > 0.05). Most of specimens in AA groups exhibited mixed failure. Alumina air-abraded surfaces exhibited higher residual compressive stresses than did surfaces with a lithium-disilicate glass-ceramic coating. Conclusion: Following thermocycling, composite-zirconia bond strength of specimens with a lithium-disilicate glass-ceramic coating was greater than that of alumina air-abraded specimens.