Li-Cheng Teng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Li-Cheng Teng has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Chao-Hsin Chien
Institute of Electronics, National Yang Ming Chiao Tung University, Hsinchu, Taiwan
3 shared publications - Shin-Yuan Wang
Department of Electronics Engineering and the Institute of Electronics, National Yang Ming Chiao Tung University, Hsinchu, Taiwan
3 shared publications - Yu-Hsien Lin
Department of Electronic Engineering, National United University, Miaoli, Taiwan
3 shared publications Chao-Hsin Chien
Institute of Electronics, National Yang Ming Chiao Tung University, Hsinchu, Taiwan
1 shared publicationChi-Cheng Tian
Department of Electronics Engineering and the Institute of Electronics, National Yang Ming Chiao Tung University, Hsinchu, Taiwan
1 shared publicationChi-Chung Kei
National Applied Research Laboratories, Taiwan Instrument Research Institute, Hsinchu, Taiwan
1 shared publication
Latest Publications
- 5 January 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 73 (3) , 1381-1386
First Demonstration of Annealing-Free Atomic-Layer-Deposited In 2 O 3 Top-Gate Devices With Robust Positive/Negative Bias Temperature Instability
In this work, we present the first demonstration of ultrathin In2O3 top-gate (TG) transistors with a short-channel length of 100 nm, fabricated using back-end-of-line (BEOL)-compatible processing ( $\le$ 250 °C) and various TG oxide deposition techniques. Plasma-enhanced ZrO2-based TG devices exhibit impressive performance, with ${I}_{\text {on, {max}}} = {378}~\mu $ A/ $\mu $ m @ ${V}_{\text {D}} = {1}$ V, a minimum subthreshold swing (SS) of 70 mV/dec, and a threshold voltage ( ${V}_{\text {t}}$ ) shift of only 0.05 V under positive bias stress ( ${V}_{\text {G}} = {V}_{\text {t}}+2$ V) for 10 000 s. Notably, these devices exhibit excellent switching behavior without needing post-deposition annealing, making them highly promising candidates for monolithic 3-D (M3D) integration.
- 5 January 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 73 (3) , 1381-1386
First Demonstration of Annealing-Free Atomic-Layer-Deposited In 2 O 3 Top-Gate Devices With Robust Positive/Negative Bias Temperature Instability
In this work, we present the first demonstration of ultrathin In2O3 top-gate (TG) transistors with a short-channel length of 100 nm, fabricated using back-end-of-line (BEOL)-compatible processing ( $\le$ 250 °C) and various TG oxide deposition techniques. Plasma-enhanced ZrO2-based TG devices exhibit impressive performance, with ${I}_{\text {on, {max}}} = {378}~\mu $ A/ $\mu $ m @ ${V}_{\text {D}} = {1}$ V, a minimum subthreshold swing (SS) of 70 mV/dec, and a threshold voltage ( ${V}_{\text {t}}$ ) shift of only 0.05 V under positive bias stress ( ${V}_{\text {G}} = {V}_{\text {t}}+2$ V) for 10 000 s. Notably, these devices exhibit excellent switching behavior without needing post-deposition annealing, making them highly promising candidates for monolithic 3-D (M3D) integration.
- 7 July 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Materials for Electron Devices
- Vol. 2, 90-94
BEOL-Compatible 5.6 nm Ultrathin HZO With Molybdenum Nitride Electrode and IN 2 O 3 Channel Devices for Enhanced Ferroelectricity and Reliability
In this letter, we have successfully fabricated a metal-ferroelectricity-metal (MFM) capacitor of an ultrathin 5.6 nm HZO and ultrathin In2O3 back gate devices in a back-end-of-line (BEOL) compatible process. By proposing a novel atomic layer deposition (ALD) scheme and an alternative bottom electrode treatment, the MoN-HZO sample shows an average 2Pr value of 64 $\mu$C/cm2 (with a standard deviation of 0.52) and high endurance ($\Delta \, 2\rm {Pr}/2\rm {Pr}_\rm {pristine} \approx 2\, \%$ from pristine to 1010 cycles). The MoN.HZO stack integrated with an ultrathin In2O3 back gate exhibits a memory window (MW) greater than 2.5 V and excellent endurance and data retention characteristics. With a maximum process temperature of 400 $^{\circ }$C, our approach meets the stringent requirements for Back-End-of-Line (BEOL) integration.
- 7 July 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Materials for Electron Devices
- Vol. 2, 90-94
BEOL-Compatible 5.6 nm Ultrathin HZO With Molybdenum Nitride Electrode and IN 2 O 3 Channel Devices for Enhanced Ferroelectricity and Reliability
In this letter, we have successfully fabricated a metal-ferroelectricity-metal (MFM) capacitor of an ultrathin 5.6 nm HZO and ultrathin In2O3 back gate devices in a back-end-of-line (BEOL) compatible process. By proposing a novel atomic layer deposition (ALD) scheme and an alternative bottom electrode treatment, the MoN-HZO sample shows an average 2Pr value of 64 $\mu$C/cm2 (with a standard deviation of 0.52) and high endurance ($\Delta \, 2\rm {Pr}/2\rm {Pr}_\rm {pristine} \approx 2\, \%$ from pristine to 1010 cycles). The MoN.HZO stack integrated with an ultrathin In2O3 back gate exhibits a memory window (MW) greater than 2.5 V and excellent endurance and data retention characteristics. With a maximum process temperature of 400 $^{\circ }$C, our approach meets the stringent requirements for Back-End-of-Line (BEOL) integration.
- 31 May 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nanotechnology
- Vol. 23 (1536125X) , 474-477
BEOL-Compatible Ferroelectric Capacitor of 5 nm Ultrathin HZO With High Remanent Polarization and Excellent Endurance
In this letter, we have successfully fabricated a metal-ferroelectricity-metal (MFM) capacitor of an ultrathin 5 nm HZO utilizing Molybdenum (Mo) as the electrodes. By proposing a novel atomic layer deposition (ALD) scheme, we overcome the challenge of oxidation of the lower Mo electrode; a 2 nm HZO deposited by thermally enhanced ALD followed by a 3 nm HZO deposited by plasma enhanced ALD. The fabricated sample demonstrated a 2Pr value of 38.5 μC/cm 2 at an operating voltage of 2V. Furthermore, in endurance testing, the sample maintained a 2Pr value of 36.9 μC/cm 2 even after 10 10 cycles (△2Pr/2Pr pristine ≈ 7% from pristine to 10 10 cycles). With a maximum process temperature of 400°C, our approach thereby meets the stringent requirement of Back-End-of-Line (BEOL) integration.
- 31 May 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nanotechnology
- Vol. 23 (1536125X) , 474-477
BEOL-Compatible Ferroelectric Capacitor of 5 nm Ultrathin HZO With High Remanent Polarization and Excellent Endurance
In this letter, we have successfully fabricated a metal-ferroelectricity-metal (MFM) capacitor of an ultrathin 5 nm HZO utilizing Molybdenum (Mo) as the electrodes. By proposing a novel atomic layer deposition (ALD) scheme, we overcome the challenge of oxidation of the lower Mo electrode; a 2 nm HZO deposited by thermally enhanced ALD followed by a 3 nm HZO deposited by plasma enhanced ALD. The fabricated sample demonstrated a 2Pr value of 38.5 μC/cm 2 at an operating voltage of 2V. Furthermore, in endurance testing, the sample maintained a 2Pr value of 36.9 μC/cm 2 even after 10 10 cycles (△2Pr/2Pr pristine ≈ 7% from pristine to 10 10 cycles). With a maximum process temperature of 400°C, our approach thereby meets the stringent requirement of Back-End-of-Line (BEOL) integration.
- 28 November 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 45 (1) , 60-63
Suppressing Threshold Voltage Drift in Sub-2 nm In2O3 Transistors With Improved Thermal Stability
Ultrathin In 2 O 3 films with a thickness of less than 2 nm have emerged as highly intriguing semiconductor channels owing to their exceptional electronic properties. However, their process reliability, particularly the challenge of threshold voltage (VT) drift during gate-stack processing, hinders their potential applications in back-end-of-line (BEOL). This study explores the VT shift induced by stacked HfO2, showing both thermal atomic layer deposition (T-ALD) and plasma-enhanced atomic layer deposition (PE-ALD) cause significant VT shift in ultrathin In 2 O 3 . To mitigate VT shift, we introduce a pre-dielectric stacking, solution-based treatment, which can effectively passivate oxygen-related defects in ultrathin In 2 O 3 , maintaining VT without adversely affecting electrical properties. Utilizing this technique, we have successfully demonstrated the first top-gate In 2 O 3 transistor without the requirement of post-fabrication annealing to uphold the on/off ratio. The developed top-gate device also exhibits superior thermal stability, suggesting its potential for future monolithic 3D integration applications.
- 28 November 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 45 (1) , 60-63
Suppressing Threshold Voltage Drift in Sub-2 nm In2O3 Transistors With Improved Thermal Stability
Ultrathin In 2 O 3 films with a thickness of less than 2 nm have emerged as highly intriguing semiconductor channels owing to their exceptional electronic properties. However, their process reliability, particularly the challenge of threshold voltage (VT) drift during gate-stack processing, hinders their potential applications in back-end-of-line (BEOL). This study explores the VT shift induced by stacked HfO2, showing both thermal atomic layer deposition (T-ALD) and plasma-enhanced atomic layer deposition (PE-ALD) cause significant VT shift in ultrathin In 2 O 3 . To mitigate VT shift, we introduce a pre-dielectric stacking, solution-based treatment, which can effectively passivate oxygen-related defects in ultrathin In 2 O 3 , maintaining VT without adversely affecting electrical properties. Utilizing this technique, we have successfully demonstrated the first top-gate In 2 O 3 transistor without the requirement of post-fabrication annealing to uphold the on/off ratio. The developed top-gate device also exhibits superior thermal stability, suggesting its potential for future monolithic 3D integration applications.