ARA. V. Razinkin

A. V. Razinkin

*This is an algorithmically generated author record based on publicly available information.

A. V. Razinkin has a total of 13 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Deformation behavior of 1441 aluminum-lithium alloy in the hot rolling temperature range

    by A. M. Pesin, A. V. Razinkin, V. A. Zamaraev, D. O. Pustovoytov

    The hot torsion method using the Gleeble 3800 thermomechanical process simulator and the Torsion module was used to experimentally study the deformation resistance of 1441 aluminum-lithium alloy of the Al – Cu – Mg – Li system in a wide range of equivalent (true) strains (in the interval of 0.01–1.0), temperatures (250–450 оC) and strain rates (0.01–50) corresponding to the hot rolling conditions on a two-stand mill of the DANIELI company at Kamensk-Uralsky Metallurgical Works. To approximate the experimental curves of deformation resistance, a tabular dependence (by points) was used, which can be applied in specialized engineering programs for computer modeling based on the finite element method, for example, in the QForm program. The accuracy of the approximation of the experimental curves was assessed by comparing the calculated and experimental values of the torsion moment depending on the twist angle at different temperatures (250–450 оC) and deformation rates (0.01–50). The relative approximation error was within ±5%. For different temperature-rate conditions, the values of equivalent deformations corresponding to the onset of destruction of the sample material were determined experimentally. It is shown that at a low strain rate (0.01) and high temperatures (450–400 оC), the equivalent strain to failure has a high value. With an increase in the strain rate to 50 and a decrease in temperature to 250–300 оC, the equivalent strain to failure significantly decreases to 0. The research results can be used to improve and optimize the process modes of hot rolling of sheets and strips made of 1441 aluminum-lithium alloy under the conditions of a two-stand mill of the DANIELI company at Kamensk-Uralsky Metallurgical Works.The research was carried out at the expense of a grant from the Russian Science Foundation (agreement No. 23-79-30015) and a co-financing agreement №KK0987F-2023.

  • Aluminum alloy extrusion scheme and model with reduction of basis metal waste

    by Yu. E. Loginov, A. V. Razinkin, G. V. Shimov, N. I. Bushueva

    This paper considers the process of extrusion of aluminium alloy 6061 bars aimed at finding a way to minimize the in-process metal loss due to the use of an additional work piece (in the form of back plug) made of cheaper material. Numerical modelling of the extrusion process was carried out for three different heating modes applied to both the tooling and the work pieces. The authors analyzed the mutual flow of the ingot and plug material at the final stage of extrusion in order to determine the moment when the back end defect starts to form and how it forms. The stress-strain state for three process options was investigated. Thus, the authors looked at the colour gradient pictures showing the distribution of strain and strain rate longitudinally along the extrusion centerline. It was found that when a pre-heated additional work piece is used, the butt-end should be made larger because of the early formed back end defect. When a cold plug and a hot dummy block are used, the back end defect forms early as well, as the back plug heats up at the final process stage reaching almost the same temperatures as the main work piece. It was established that the optimum option would be not heating the back work piece or the dummy block. The modelling helped reveal that the size of the buttend in this case is smaller. The obtained modelling data can be used for conducting pilot studies aimed at reducing the size of the butt-end when producing extruded aluminium bars. This will help improve the metal utilization factor.This research was carried out as part of Project No. 22-29-00931 dated 20/12/2021 by the Russian Science Foundation.


  • Open Access

    Structure and strain state of aluminum bars at the initial phase of extrusion

    by Yu. N. Loginov, A. V. Razinkin, G. V. Shimov, T. V. Maltseva, N. I. Bushueva, E. G. Dymshakova, N. A. Kalinina

    The structure of insufficiently deformed areas at the non-steady phase of extrusion was studied. The tests at Kamensk Uralsky Metallurgical Works using a 120 MN press and 800 mm dia. container, in order to extrude a 355.6 mm dia. Bar was performed. The bar material is the Al–Mg–Si AD33 aluminum alloy (GOST 4784), similar to ASTM 6061. The percentage reduction was 80 %, and the reduction ratio was 5.06. After that, the macrostructure, microstructure, and average grain size along the radius, mechanical properties at room and elevated temperatures were investigated. It was found that the extruded bar macrostructure is fine-grained, homogeneous, and dense, with no nonmetallic or intermetallic inclusions. The cross-section contained several structures. The central part is weakly deformed preserving the dendritic cell structure inherited from the casting. At the circumference, a streaked structure is formed. Its components are crushed and uniformly distributed. We measured the strength at elevated temperatures and compared the results to the data available in the literature. The tested material strength almost doubled, thus indicating its incomplete softening. The ductility was also performed. The DEFORM-2D software, in order to simulate the low reduction of extrusion was used. The metal at the circumference is exposed to a greater strain from the extrusion beginning. A step-by-step analysis indicated that at the first step, the strain is localized near the die hole. In the second step, a rigid area is formed in the vicinity of the die/container liner interface. The circumference layer of metal with a 1.75–2.00 reduction of area is formed. At the bar center, this range is 0.75–1.00 (half of the circumference value). In the third step, the circumference layer with an elevated strain has a wedge-like shape. In the fourth step, the circumference layer (with elevated strain) has an equal thickness along the extrusion axis. This indicates the steady phase. The plastic strain at the bar front end is higher at the circumference than in the center. This confirms the structural analysis results. They show that the central part of the bar may retain its cast structure, while the circumference is deformed. If the bar central part is required to have some specific properties, the bar has to undergo another manufacturing operation to increase the accumulated strain. Re-extrusion processes the areas insufficiently deformed during the first extrusion.