Kuo-Tsung Huang
Research Subjects
Kuo-Tsung Huang has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
- Shih-Hsien Chang
Department of Materials and Mineral Resources Engineering, National Taipei University of Technology, Taipei 106344, Taiwan
15 shared publications Cheng Liang
3 shared publications- Chih-Hao Yang
Department of Mechanical Engineering, National Pingtung University of Science and Technology, Pingtung 912301, Taiwan
3 shared publications - Cheng Liang
National Taipei University of Technology, Department of Materials and Miner al Resources Engineering, Taipei 10608, Taiwan, ROC
2 shared publications Shih-Hsien Chang
2 shared publications- Yun-Fang Chen
Department of Materials and Mineral Resources Engineering, National Taipei University of Technology, Taipei, 10608, Taiwan, ROC
2 shared publications
Latest Publications
- Open Access
- 13 August 2026
- Published by Elsevier in SSRN Electronic Journal
Impact of adding vanadium powders on the material characteristics, TEM structures, and mechanical performances of TiNbMoCo medium-entropy alloys via vacuum sintering
Titanium-rich NbMoCo medium-entropy alloys (MEAs) with varying vanadium contents (3, 6, 9, and 12 mass%) were fabricated via vacuum sintering at 1150°C, 1175°C, and 1200°C for 1 h. The effects of vanadium addition and sintering temperature on the microstructure and mechanical properties were investigated systematically. The results show that the TiNbMoCo MEA containing 9 mass% V and sintered at 1175°C had the most balanced overall performance, achieving a low apparent porosity of 0.57±0.27%, a high sintered density of 6.88±0.04 g·cm−3, a hardness of 75.67±0.84 HRA, a transverse rupture strength of 606.51±7.06 MPa, and a flexural modulus of 75.98±1.09 GPa. Electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM) analyses indicate the formation of a BCC-Ti solid solution by incorporating Nb, Mo, Co, and V, leading to effective solid-solution strengthening. Additionally, CoTi2 intermetallic compounds precipitated within the matrix, promoting the transformation of HCP-Ti to FCC-Ti at phase interfaces while contributing to its enhanced mechanical properties.
- 13 August 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessImpact of adding vanadium powders on the material characteristics, TEM structures, and mechanical performances of TiNbMoCo medium-entropy alloys via vacuum sintering
Titanium-rich NbMoCo medium-entropy alloys (MEAs) with varying vanadium contents (3, 6, 9, and 12 mass%) were fabricated via vacuum sintering at 1150°C, 1175°C, and 1200°C for 1 h. The effects of vanadium addition and sintering temperature on the microstructure and mechanical properties were investigated systematically. The results show that the TiNbMoCo MEA containing 9 mass% V and sintered at 1175°C had the most balanced overall performance, achieving a low apparent porosity of 0.57±0.27%, a high sintered density of 6.88±0.04 g·cm−3, a hardness of 75.67±0.84 HRA, a transverse rupture strength of 606.51±7.06 MPa, and a flexural modulus of 75.98±1.09 GPa. Electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM) analyses indicate the formation of a BCC-Ti solid solution by incorporating Nb, Mo, Co, and V, leading to effective solid-solution strengthening. Additionally, CoTi2 intermetallic compounds precipitated within the matrix, promoting the transformation of HCP-Ti to FCC-Ti at phase interfaces while contributing to its enhanced mechanical properties.
- Open Access
- 9 April 2026
- Published by Elsevier in SSRN Electronic Journal
Investigating the microstructure, mechanical properties, and TEM characteristics of CoNiVCr medium-entropy alloys processed via vacuum hot-press sintering powder metallurgy
This study synthesized CoNiVCr medium-entropy alloys (MEAs) using powder metallurgy followed by vacuum hot-press sintering (VHPS). The experiments involved various hot-press sintering temperatures (1050°C, 1100°C, 1150°C, and 1200°C) and pressures (20, 35, and 50 MPa) to identify the optimal parameters for CoNiVCr MEAs while investigating the differences in microstructures and material characteristics. The study results indicate that CoNiVCr MEAs exhibited the most optimal mechanical properties under sintering conditions of 1100°C at 50 MPa for 1 h, which achieved a sintering density of 8.07±0.01 g·cm−3, a hardness of 75.3±0.5 HRA, a transverse rupture strength (TRS) of 1985.2±18.1 MPa, and a flexural modulus of 126.3±5.1 GPa. The corresponding electrical conductivity was 6.15±0.17×104 S·cm−1. Electron backscatter diffraction (EBSD) analysis confirmed the presence of a single-phase face-centered cubic (FCC) structure with random grain orientation in this alloy. Transmission electron microscopy (TEM) observation showed that a small amount of Ni3V intermetallic compounds exists. The findings suggest that VHPS promotes densification while enhancing the mechanical properties of CoNiVCr MEAs.
- 9 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessInvestigating the microstructure, mechanical properties, and TEM characteristics of CoNiVCr medium-entropy alloys processed via vacuum hot-press sintering powder metallurgy
This study synthesized CoNiVCr medium-entropy alloys (MEAs) using powder metallurgy followed by vacuum hot-press sintering (VHPS). The experiments involved various hot-press sintering temperatures (1050°C, 1100°C, 1150°C, and 1200°C) and pressures (20, 35, and 50 MPa) to identify the optimal parameters for CoNiVCr MEAs while investigating the differences in microstructures and material characteristics. The study results indicate that CoNiVCr MEAs exhibited the most optimal mechanical properties under sintering conditions of 1100°C at 50 MPa for 1 h, which achieved a sintering density of 8.07±0.01 g·cm−3, a hardness of 75.3±0.5 HRA, a transverse rupture strength (TRS) of 1985.2±18.1 MPa, and a flexural modulus of 126.3±5.1 GPa. The corresponding electrical conductivity was 6.15±0.17×104 S·cm−1. Electron backscatter diffraction (EBSD) analysis confirmed the presence of a single-phase face-centered cubic (FCC) structure with random grain orientation in this alloy. Transmission electron microscopy (TEM) observation showed that a small amount of Ni3V intermetallic compounds exists. The findings suggest that VHPS promotes densification while enhancing the mechanical properties of CoNiVCr MEAs.
- Open Access
- 15 February 2026
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 66 (2) , 274-283
Enhancement of Wear and Corrosion Properties of OPTI N+ High-Nitrogen Stainless Steel via DC Magnetron Sputtered CrSiN and Ion Nitriding Duplex Treatments
This study investigates the enhancement of surface properties of OPTI N+ high-nitrogen stainless steel through a duplex treatment combining ion nitriding and CrSiN coating deposition via DC magnetron sputtering. Ion nitriding produced a hardened layer approximately 50 μm thick with a surface hardness of 1037.1 HV0.05, primarily composed of Fe₂N, Fe₃N and Fe₄N phases. CrSiN coatings deposited at various temperatures showed that the sample coated at 300°C exhibited the highest hardness (13.07 GPa), optimal H/E ratio (0.055), and superior tribological performance, including the lowest friction coefficient (0.5773), wear loss volume (7.67 × 10⁻⁴ mm³), and specific wear rate (3.23 × 10⁻⁷ mm³·m⁻¹·N⁻¹) under a 5 N load. Electrochemical tests confirmed enhanced corrosion resistance, with the lowest corrosion current density (1.38 × 10⁻⁶ A·cm⁻²) and highest polarization resistance (339.98 Ω·cm²). HRTEM analysis revealed a nanocomposite microstructure consisting of crystalline CrN and amorphous SiN. These results demonstrate that the CrSiN/ion nitriding duplex treatment significantly improves the mechanical, tribological, and corrosion resistance of high-nitrogen stainless steel.
- 15 February 2026
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 66 (2) , 274-283
Open AccessEnhancement of Wear and Corrosion Properties of OPTI N+ High-Nitrogen Stainless Steel via DC Magnetron Sputtered CrSiN and Ion Nitriding Duplex Treatments
This study investigates the enhancement of surface properties of OPTI N+ high-nitrogen stainless steel through a duplex treatment combining ion nitriding and CrSiN coating deposition via DC magnetron sputtering. Ion nitriding produced a hardened layer approximately 50 μm thick with a surface hardness of 1037.1 HV0.05, primarily composed of Fe₂N, Fe₃N and Fe₄N phases. CrSiN coatings deposited at various temperatures showed that the sample coated at 300°C exhibited the highest hardness (13.07 GPa), optimal H/E ratio (0.055), and superior tribological performance, including the lowest friction coefficient (0.5773), wear loss volume (7.67 × 10⁻⁴ mm³), and specific wear rate (3.23 × 10⁻⁷ mm³·m⁻¹·N⁻¹) under a 5 N load. Electrochemical tests confirmed enhanced corrosion resistance, with the lowest corrosion current density (1.38 × 10⁻⁶ A·cm⁻²) and highest polarization resistance (339.98 Ω·cm²). HRTEM analysis revealed a nanocomposite microstructure consisting of crystalline CrN and amorphous SiN. These results demonstrate that the CrSiN/ion nitriding duplex treatment significantly improves the mechanical, tribological, and corrosion resistance of high-nitrogen stainless steel.
- 8 December 2025
- Published by SAGE Publications in Powder Metallurgy
- Vol. 69 (2) , 181-195
Effects of the microstructure and mechanical properties of Cr 3 C 2 powders added to Ti-25Nb-25Mo-15Ni medium entropy alloys
This study fabricated Ti-25Nb-25Mo-15Ni-xCr 3 C 2 composites and added differing proportions of Cr 3 C 2 powder (where x represents 1, 3, and 5 mass%, respectively) using the vacuum sintering process-a powder metallurgy technique. The composites were simultaneously vacuum sintered at 1150, 1175, 1200, and 1225°C for 1 h, respectively. The experimental results indicate that the specimens exhibited optimal properties when the Ti-25Nb-25Mo-15Ni-1Cr 3 C 2 composites were sintered at 1225°C for 1 h. The sintered density increased to 7.29 ± 0.15 g·cm −3 , while the TRS improved to 684.23 ± 24.65 MPa, the flexural modulus increased to 69.64 ± 0.21 GPa, and the hardness rose to 75.88 ± 1.19 HRA. The EBSD and TEM results show that niobium, molybdenum, and chromium can form a strong solid solution with titanium, contributing to the solid solution strengthening effect. Moreover, nickel forms TiNi and Ti 2 Ni intermetallic compounds with titanium, which are dispersed in the titanium matrix and effectively enhance its mechanical properties.
- 8 December 2025
- Published by SAGE Publications in Powder Metallurgy
- Vol. 69 (2) , 181-195
Effects of the microstructure and mechanical properties of Cr 3 C 2 powders added to Ti-25Nb-25Mo-15Ni medium entropy alloys
This study fabricated Ti-25Nb-25Mo-15Ni-xCr 3 C 2 composites and added differing proportions of Cr 3 C 2 powder (where x represents 1, 3, and 5 mass%, respectively) using the vacuum sintering process-a powder metallurgy technique. The composites were simultaneously vacuum sintered at 1150, 1175, 1200, and 1225°C for 1 h, respectively. The experimental results indicate that the specimens exhibited optimal properties when the Ti-25Nb-25Mo-15Ni-1Cr 3 C 2 composites were sintered at 1225°C for 1 h. The sintered density increased to 7.29 ± 0.15 g·cm −3 , while the TRS improved to 684.23 ± 24.65 MPa, the flexural modulus increased to 69.64 ± 0.21 GPa, and the hardness rose to 75.88 ± 1.19 HRA. The EBSD and TEM results show that niobium, molybdenum, and chromium can form a strong solid solution with titanium, contributing to the solid solution strengthening effect. Moreover, nickel forms TiNi and Ti 2 Ni intermetallic compounds with titanium, which are dispersed in the titanium matrix and effectively enhance its mechanical properties.
- 1 March 2024
- Published by SAGE Publications in Powder Metallurgy
- Vol. 67 (2-3) , 154-168
Microstructure, material characteristics and mechanical properties of CoMoNiTa3 medium-entropy alloys through the vacuum hot pressing process
This work fabricated CoMoNiTa3 medium-entropy alloys using the vacuum hot pressing process of powder metallurgy technology. Micron-grade cobalt (6.3 μm), molybdenum (13.2 μm), nickel (2.4 μm) and tantalum powders (25.0 μm) were combined using ball milling. The experiments utilised various hot pressing temperatures (1000, 1050, 1100, and 1150 °C) and hot pressing pressures (20, 35, and 50 MPa) to identify the optimal parameters for CoMoNiTa3 alloys, while simultaneously investigating the differences in microstructures. The experimental results reveal that the optimal hot pressing parameters of this alloy were 1100 °C at 50 MPa for 1 h. The sintering density was enhanced to 9.65 ± 0.01 g cm−3, while the hardness, transverse rupture strength, and flexural modulus reached 85.5 ± 0.1 HRA, 1370.3 ± 90.1 MPa and 168.6 ± 12.7 GPa, respectively. Moreover, the electrical conductivity was 6.53 ± 0.13 × 104 S cm−1. Furthermore, the electron probe microanalyser, electron backscatter diffraction, and transmission electron microscopy results confirmed the face-centred cubic solid solution, Ni3Ta, and μ phases of the CoMoNiTa3 structure, and no preferred grain orientation was found.
- 1 March 2024
- Published by SAGE Publications in Powder Metallurgy
- Vol. 67 (2-3) , 154-168
Microstructure, material characteristics and mechanical properties of CoMoNiTa3 medium-entropy alloys through the vacuum hot pressing process
This work fabricated CoMoNiTa3 medium-entropy alloys using the vacuum hot pressing process of powder metallurgy technology. Micron-grade cobalt (6.3 μm), molybdenum (13.2 μm), nickel (2.4 μm) and tantalum powders (25.0 μm) were combined using ball milling. The experiments utilised various hot pressing temperatures (1000, 1050, 1100, and 1150 °C) and hot pressing pressures (20, 35, and 50 MPa) to identify the optimal parameters for CoMoNiTa3 alloys, while simultaneously investigating the differences in microstructures. The experimental results reveal that the optimal hot pressing parameters of this alloy were 1100 °C at 50 MPa for 1 h. The sintering density was enhanced to 9.65 ± 0.01 g cm−3, while the hardness, transverse rupture strength, and flexural modulus reached 85.5 ± 0.1 HRA, 1370.3 ± 90.1 MPa and 168.6 ± 12.7 GPa, respectively. Moreover, the electrical conductivity was 6.53 ± 0.13 × 104 S cm−1. Furthermore, the electron probe microanalyser, electron backscatter diffraction, and transmission electron microscopy results confirmed the face-centred cubic solid solution, Ni3Ta, and μ phases of the CoMoNiTa3 structure, and no preferred grain orientation was found.
- Open Access
- 15 January 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (1) , 154-164
Microstructure, Strengthening Mechanism and Mechanical Properties of Vanadis 60-Ta0.5Nb0.5C-B4C High-speed Steel Composite via Vacuum Sintering, Sub-zero, and Heat Treatments
This research added different ratios of Ta50Nb50C and B4C powders to Vanadis 60 high-speed steel powders, and then, sintered the Vanadis 60 composite from 1205 to 1225°C by vacuum sintering for 1 hour. Subsequently, a series of heat treatments were conducted, including quenching, sub-zero, and tempering processes. The study results show that the optimal sintering temperature and the additive ratio for Vanadis 60 composites were 1205°C and 0.975 mass% Ta50Nb50C-0.025 mass% B4C powders, respectively. Simultaneously, the transverse rupture strength (TRS) value was 2328.2±0.90.7 MPa and the hardness value was 81.3±0.1 HRA, respectively. In particular, when the optimally sintered Vanadis 60 composite underwent sub-zero plus heat treatments, the TRS and hardness values obviously increased to 2456.6±76.3 MPa and 85.7±0.3 HRA, respectively. Finally, the TEM and EBSD study results also revealed that various MC and M6C-type carbides significantly appeared in the Vanadis 60 composite after vacuum sintering and sub-zero plus heat treatments.
- 15 January 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (1) , 154-164
Open AccessMicrostructure, Strengthening Mechanism and Mechanical Properties of Vanadis 60-Ta0.5Nb0.5C-B4C High-speed Steel Composite via Vacuum Sintering, Sub-zero, and Heat Treatments
This research added different ratios of Ta50Nb50C and B4C powders to Vanadis 60 high-speed steel powders, and then, sintered the Vanadis 60 composite from 1205 to 1225°C by vacuum sintering for 1 hour. Subsequently, a series of heat treatments were conducted, including quenching, sub-zero, and tempering processes. The study results show that the optimal sintering temperature and the additive ratio for Vanadis 60 composites were 1205°C and 0.975 mass% Ta50Nb50C-0.025 mass% B4C powders, respectively. Simultaneously, the transverse rupture strength (TRS) value was 2328.2±0.90.7 MPa and the hardness value was 81.3±0.1 HRA, respectively. In particular, when the optimally sintered Vanadis 60 composite underwent sub-zero plus heat treatments, the TRS and hardness values obviously increased to 2456.6±76.3 MPa and 85.7±0.3 HRA, respectively. Finally, the TEM and EBSD study results also revealed that various MC and M6C-type carbides significantly appeared in the Vanadis 60 composite after vacuum sintering and sub-zero plus heat treatments.