Byung‐Koog Jang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Byung‐Koog Jang has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
Nobuo Nagashima
Research Center for Structural Materials, National Institute for Materials Science
2 shared publications- Byung-Nam Kim
Research Center for Functional Materials National Institute for Materials Science Tsukuba Ibaraki Japan
1 shared publication Byung‐Nam Kim
Research Center for Functional Materials National Institute for Materials Science Tsukuba Ibaraki Japan
1 shared publication- Ji-Hwoan Lee
Interdisciplinary Graduate School of Engineering Sciences Kyushu University Kasuga Fukuoka Japan
1 shared publication Kee-Sung Lee
School of Mechanical Engineering, Kookmin University
1 shared publicationSeung-Hyeon Kim
Research Center for Structural Materials, National Institute for Materials Science
1 shared publication
Latest Publications
- Open Access
- 1 May 2024
- Published by Ceramic Society of Japan in Journal of the Ceramic Society of Japan
- Vol. 132 (5) , 205-213
Corrosion behavior of calcium-magnesium-alumino-silicate on (La,Gd)2Zr2O7/YSZ multilayer for thermal barrier coatings
In this study, the high-temperature corrosion behavior was evaluated for (La,Gd)2Zr2O7 (LGZ) used as a promising thermal barrier coatings (TBCs) material. (La,Gd)2Zr2O7 + YSZ multilayer prepared from atmospheric plasma spray (APS) were exposed to calcium-magnesium-alumino-silicate (CMAS) melt at 1300 °C for 2, 12, 48, and 100 h. Molten CMAS and (La,Gd)2Zr2O7 reacted to form reaction layer Ca2Gd8(SiO4)6O2 (apatite) at 1300 °C. The thickness of the reaction layer increased with increasing heat-treatment time. A correlation between the hardness and Young’s modulus relationship for the reaction layer of the coating was observed for the microstructure using nanoindentation. It was confirmed that the pores of the coating were reduced through the infiltration of molten CMAS in the initial stage of the corrosion reaction, and the hardness and Young’s modulus were increased due to densification. Fracture toughness increased with heat treatment time in both directions (in-plane and through-thickness). The fracture toughness in the in-plane direction is 0.19–0.23 MPa√m. On the other hand, the fracture resistance in the thickness direction was 0.87–1.26 MPa√m, which was higher than that in the in-plane direction. These results show that the crack propagates in the in-plane direction and causes TBC delamination.
- 1 May 2024
- Published by Ceramic Society of Japan in Journal of the Ceramic Society of Japan
- Vol. 132 (5) , 205-213
Open AccessCorrosion behavior of calcium-magnesium-alumino-silicate on (La,Gd)2Zr2O7/YSZ multilayer for thermal barrier coatings
In this study, the high-temperature corrosion behavior was evaluated for (La,Gd)2Zr2O7 (LGZ) used as a promising thermal barrier coatings (TBCs) material. (La,Gd)2Zr2O7 + YSZ multilayer prepared from atmospheric plasma spray (APS) were exposed to calcium-magnesium-alumino-silicate (CMAS) melt at 1300 °C for 2, 12, 48, and 100 h. Molten CMAS and (La,Gd)2Zr2O7 reacted to form reaction layer Ca2Gd8(SiO4)6O2 (apatite) at 1300 °C. The thickness of the reaction layer increased with increasing heat-treatment time. A correlation between the hardness and Young’s modulus relationship for the reaction layer of the coating was observed for the microstructure using nanoindentation. It was confirmed that the pores of the coating were reduced through the infiltration of molten CMAS in the initial stage of the corrosion reaction, and the hardness and Young’s modulus were increased due to densification. Fracture toughness increased with heat treatment time in both directions (in-plane and through-thickness). The fracture toughness in the in-plane direction is 0.19–0.23 MPa√m. On the other hand, the fracture resistance in the thickness direction was 0.87–1.26 MPa√m, which was higher than that in the in-plane direction. These results show that the crack propagates in the in-plane direction and causes TBC delamination.
- 9 June 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (11) , 5501-5508
Fabrication of transparent Y 2 O 3 ceramics by two‐step spark plasma sintering
Transparent Y 2 O 3 ceramics were successfully fabricated by spark plasma sintering applying a two‐step pressure and heating profile. Through the shrinkage curve of the single‐step SPS profile, it was confirmed that shrinkage occurred at 800°C–1250°C, and it was selected as the two‐step pressure profile. After the first‐step SPS stage at 1250°C, the second‐step SPS stage, which had the highest real in‐line transmittance, was completed at 1500°C. The two‐step SPS profile improved the shrinkage behavior and was able to achieve sufficient densification without excessive coarsening. As a result, the normalized real in‐line transmittance to 1 mm was 80.6% at 1100 nm, which is close to the theoretical transmittance of 81.6%. The two‐step pressure and heating profile in the SPS process was a significant advantage in manufacturing ceramics that were transparent and had sufficient densification.
- 9 June 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (11) , 5501-5508
Fabrication of transparent Y 2 O 3 ceramics by two‐step spark plasma sintering
Transparent Y 2 O 3 ceramics were successfully fabricated by spark plasma sintering applying a two‐step pressure and heating profile. Through the shrinkage curve of the single‐step SPS profile, it was confirmed that shrinkage occurred at 800°C–1250°C, and it was selected as the two‐step pressure profile. After the first‐step SPS stage at 1250°C, the second‐step SPS stage, which had the highest real in‐line transmittance, was completed at 1500°C. The two‐step SPS profile improved the shrinkage behavior and was able to achieve sufficient densification without excessive coarsening. As a result, the normalized real in‐line transmittance to 1 mm was 80.6% at 1100 nm, which is close to the theoretical transmittance of 81.6%. The two‐step pressure and heating profile in the SPS process was a significant advantage in manufacturing ceramics that were transparent and had sufficient densification.
- 29 January 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (7) , 3119-3129
Corrosion behavior of calcium–magnesium–aluminosilicate (CMAS) on sintered Gd 2 SiO 5 for environmental barrier coatings
The Gd 2 SiO 5 performed high‐temperature corrosion behavior on calcium–magnesium– aluminosilicate (CMAS) for environmental barrier coatings (EBCs). The synthesized Gd 2 O 3 ‐SiO 2 powder was prepared to fabricate a sintered Gd 2 SiO 5 by spark plasma sintering (SPS) at 1400°C for 20 min. CMAS was sprinkled on the sintered Gd 2 SiO 5 surface and exposed for 2, 12, and 48 h at 1400°C by isothermal heat treatment. The main corrosion factor is Ca, and Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase is formed by reacting with Gd 2 SiO 5 . Extended morphology of Ca 2 Gd 8 (SiO 4 ) 6 O 2 particles observed in the reaction area become thicker as the heat treatment time increases as the CMAS is dissolved. According to the results of high‐temperature X‐ray diffraction (HT‐XRD) and differential scanning calorimetry (DSC), CMAS melted at 1243°C or a higher temperature formed the reaction area. The Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase was recrystallized and grown due to the reaction of Gd 2 SiO 5 and Ca of the CMAS components.
- 29 January 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (7) , 3119-3129
Corrosion behavior of calcium–magnesium–aluminosilicate (CMAS) on sintered Gd 2 SiO 5 for environmental barrier coatings
The Gd 2 SiO 5 performed high‐temperature corrosion behavior on calcium–magnesium– aluminosilicate (CMAS) for environmental barrier coatings (EBCs). The synthesized Gd 2 O 3 ‐SiO 2 powder was prepared to fabricate a sintered Gd 2 SiO 5 by spark plasma sintering (SPS) at 1400°C for 20 min. CMAS was sprinkled on the sintered Gd 2 SiO 5 surface and exposed for 2, 12, and 48 h at 1400°C by isothermal heat treatment. The main corrosion factor is Ca, and Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase is formed by reacting with Gd 2 SiO 5 . Extended morphology of Ca 2 Gd 8 (SiO 4 ) 6 O 2 particles observed in the reaction area become thicker as the heat treatment time increases as the CMAS is dissolved. According to the results of high‐temperature X‐ray diffraction (HT‐XRD) and differential scanning calorimetry (DSC), CMAS melted at 1243°C or a higher temperature formed the reaction area. The Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase was recrystallized and grown due to the reaction of Gd 2 SiO 5 and Ca of the CMAS components.