Katherine Betts
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Katherine Betts has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Yuhan Jiang
University of Nevada, Las Vegas
5 shared publications- Zhange Feng
Department of Chemistry and Biochemistry, University of Nevada, Las Vegas, Las Vegas, Nevada 89154, United States of America
4 shared publications Kidus Yohannes
University of Nevada, Las Vegas
3 shared publicationsMichael Frailey
University of Nevada, Las Vegas
3 shared publications- Zhange Feng
University of Nevada, Las Vegas
3 shared publications Andrew Yanagimachi
University of Nevada, Las Vegas
2 shared publications
Latest Publications
- 7 July 2026
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2026-01 (58) , 464
In situ Characterization of the Solid Electrolyte Interphase on Au Electrodes Insuperconcentrated Lifsi/EC and Lifsi/Dmc Electrolytes
Understanding the formation and properties of the solid electrolyte interphase (SEI) is critical forimproving lithium-ion battery (LIB) performance. In this study, we investigate the interfacialdynamics of gold electrodes in two superconcentrated LiFSI-based carbonateelectrolytes—ethylene carbonate (EC)/LiFSI and dimethyl carbonate (DMC)/LiFSI—using athree-electrode configuration with Li as reference and counter electrodes.We employ in situ Attenuated Total Reflection–Surface-Enhanced Infrared AbsorptionSpectroscopy (ATR-SEIRAS) to monitor potential-dependent changes in interfacial composition,and Electrochemical Quartz Crystal Microbalance with Dissipation (EQCM-D) to track mass andviscoelastic properties of the evolving interphase.Upon stepping from open-circuit potential (OCP) toward positive potentials, both EC- andDMC-based electrolytes show gradual growth of carbonyl and anionic signals, corresponding toreversible interfacial ordering without formation of distinct oxidation products. In contrast,negative potential scans reveal distinct differences: DMC/LiFSI exhibits pronounced carbonateSEI features in SEIRAS (870 and 1480–1500 cm⁻¹) accompanied by continuous massaccumulation and increasing dissipation in EQCM-D, indicating formation of a soft, growinginterphase. EC/LiFSI, however, produces weaker carbonate signals and minimal changes in massand dissipation, consistent with a self-limiting, mechanically robust SEI.These results suggest that EC/LiFSI promotes the formation of a more compact and stable SEIwith favorable ionic conductivity and mechanical properties, whereas DMC/LiFSI generates asofter, thicker layer that may limit Faradaic efficiency and Li cycling stability. This combinedATR-SEIRAS/EQCM-D approach provides a powerful framework for evaluating electrolyteinterfacial behavior and guiding the design of high-performance LIB electrolytes.
- 7 July 2026
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2026-01 (58) , 464
In situ Characterization of the Solid Electrolyte Interphase on Au Electrodes Insuperconcentrated Lifsi/EC and Lifsi/Dmc Electrolytes
Understanding the formation and properties of the solid electrolyte interphase (SEI) is critical forimproving lithium-ion battery (LIB) performance. In this study, we investigate the interfacialdynamics of gold electrodes in two superconcentrated LiFSI-based carbonateelectrolytes—ethylene carbonate (EC)/LiFSI and dimethyl carbonate (DMC)/LiFSI—using athree-electrode configuration with Li as reference and counter electrodes.We employ in situ Attenuated Total Reflection–Surface-Enhanced Infrared AbsorptionSpectroscopy (ATR-SEIRAS) to monitor potential-dependent changes in interfacial composition,and Electrochemical Quartz Crystal Microbalance with Dissipation (EQCM-D) to track mass andviscoelastic properties of the evolving interphase.Upon stepping from open-circuit potential (OCP) toward positive potentials, both EC- andDMC-based electrolytes show gradual growth of carbonyl and anionic signals, corresponding toreversible interfacial ordering without formation of distinct oxidation products. In contrast,negative potential scans reveal distinct differences: DMC/LiFSI exhibits pronounced carbonateSEI features in SEIRAS (870 and 1480–1500 cm⁻¹) accompanied by continuous massaccumulation and increasing dissipation in EQCM-D, indicating formation of a soft, growinginterphase. EC/LiFSI, however, produces weaker carbonate signals and minimal changes in massand dissipation, consistent with a self-limiting, mechanically robust SEI.These results suggest that EC/LiFSI promotes the formation of a more compact and stable SEIwith favorable ionic conductivity and mechanical properties, whereas DMC/LiFSI generates asofter, thicker layer that may limit Faradaic efficiency and Li cycling stability. This combinedATR-SEIRAS/EQCM-D approach provides a powerful framework for evaluating electrolyteinterfacial behavior and guiding the design of high-performance LIB electrolytes.
- 7 July 2026
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2026-01 (3) , 464
In situ Characterization of the Solid Electrolyte Interphase on Au Electrodes Insuperconcentrated Lifsi/EC and Lifsi/Dmc Electrolytes
Understanding the formation and properties of the solid electrolyte interphase (SEI) is critical forimproving lithium-ion battery (LIB) performance. In this study, we investigate the interfacialdynamics of gold electrodes in two superconcentrated LiFSI-based carbonateelectrolytes—ethylene carbonate (EC)/LiFSI and dimethyl carbonate (DMC)/LiFSI—using athree-electrode configuration with Li as reference and counter electrodes.We employ in situ Attenuated Total Reflection–Surface-Enhanced Infrared AbsorptionSpectroscopy (ATR-SEIRAS) to monitor potential-dependent changes in interfacial composition,and Electrochemical Quartz Crystal Microbalance with Dissipation (EQCM-D) to track mass andviscoelastic properties of the evolving interphase.Upon stepping from open-circuit potential (OCP) toward positive potentials, both EC- andDMC-based electrolytes show gradual growth of carbonyl and anionic signals, corresponding toreversible interfacial ordering without formation of distinct oxidation products. In contrast,negative potential scans reveal distinct differences: DMC/LiFSI exhibits pronounced carbonateSEI features in SEIRAS (870 and 1480–1500 cm⁻¹) accompanied by continuous massaccumulation and increasing dissipation in EQCM-D, indicating formation of a soft, growinginterphase. EC/LiFSI, however, produces weaker carbonate signals and minimal changes in massand dissipation, consistent with a self-limiting, mechanically robust SEI.These results suggest that EC/LiFSI promotes the formation of a more compact and stable SEIwith favorable ionic conductivity and mechanical properties, whereas DMC/LiFSI generates asofter, thicker layer that may limit Faradaic efficiency and Li cycling stability. This combinedATR-SEIRAS/EQCM-D approach provides a powerful framework for evaluating electrolyteinterfacial behavior and guiding the design of high-performance LIB electrolytes.
- 7 July 2026
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2026-01 (3) , 464
In situ Characterization of the Solid Electrolyte Interphase on Au Electrodes Insuperconcentrated Lifsi/EC and Lifsi/Dmc Electrolytes
Understanding the formation and properties of the solid electrolyte interphase (SEI) is critical forimproving lithium-ion battery (LIB) performance. In this study, we investigate the interfacialdynamics of gold electrodes in two superconcentrated LiFSI-based carbonateelectrolytes—ethylene carbonate (EC)/LiFSI and dimethyl carbonate (DMC)/LiFSI—using athree-electrode configuration with Li as reference and counter electrodes.We employ in situ Attenuated Total Reflection–Surface-Enhanced Infrared AbsorptionSpectroscopy (ATR-SEIRAS) to monitor potential-dependent changes in interfacial composition,and Electrochemical Quartz Crystal Microbalance with Dissipation (EQCM-D) to track mass andviscoelastic properties of the evolving interphase.Upon stepping from open-circuit potential (OCP) toward positive potentials, both EC- andDMC-based electrolytes show gradual growth of carbonyl and anionic signals, corresponding toreversible interfacial ordering without formation of distinct oxidation products. In contrast,negative potential scans reveal distinct differences: DMC/LiFSI exhibits pronounced carbonateSEI features in SEIRAS (870 and 1480–1500 cm⁻¹) accompanied by continuous massaccumulation and increasing dissipation in EQCM-D, indicating formation of a soft, growinginterphase. EC/LiFSI, however, produces weaker carbonate signals and minimal changes in massand dissipation, consistent with a self-limiting, mechanically robust SEI.These results suggest that EC/LiFSI promotes the formation of a more compact and stable SEIwith favorable ionic conductivity and mechanical properties, whereas DMC/LiFSI generates asofter, thicker layer that may limit Faradaic efficiency and Li cycling stability. This combinedATR-SEIRAS/EQCM-D approach provides a powerful framework for evaluating electrolyteinterfacial behavior and guiding the design of high-performance LIB electrolytes.
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (53) , 2545
Potential-Dependent Surface Enhanced Infrared Absorption Spectroscopy (SEIRAS) Study of Perfluoroalkyl Substances (PFAS)
Per- and polyfluoroalkyl substances (PFAS), often referred to as "forever chemicals," are persistent organic compounds with strong carbon-fluorine (C-F) bonds, making them highly stable and resistant to degradation. Since the 1940s, PFAS have been widely used in firefighting foam, food packaging, cookware, cosmetics, and paints. Their bioaccumulation in the environment raises significant concerns, as PFAS exposure—primarily through contaminated drinking water and food—has been linked to DNA modification, reproductive toxicity, immunotoxicity and cancer. To mitigate these risks, it is essential to develop effective methods for PFAS removal from water supplies. Perfluorooctanoic acid (PFOA) and perfluorooctane sulfonate (PFOS), are the most studied PFAS due to their wide use and bioaccumulation. These substances are being progressively eliminated worldwide, however, addressing contamination in existing water supplies remains an urgent priority. The capture and/or degradation of PFAS in water requires the development of successful separation methods and an understanding of its adsorption mechanisms. Whether for degradation, capture or detection applications, electrosorption is a key area of interest in the mitigation of PFAS in water. Understanding the mechanisms of surface adsorption and relationship with water is essential to innovation in remediation technology. Potential dependent surface-enhanced infrared absorption spectroscopy (SEIRAS) provides a powerful tool for studying PFAS adsorption at the electrode interface. PFOA and PFOS were analyzed with cyclic voltammetry and SEIRAS protocols in a NaClO 4 supporting electrolyte, across a range of pHs. Experimental observations describe PFOA adsorbing to the electrode via the hydrophobic tail, rather than the electronegative carboxylic acid head, confirmed by the large increase in C-F bond molecular vibrations at positive potentials. Potential cycling demonstrated weak adsorption hysteresis, and a disruption of surface interactions was observed in the presence of potassium bromide. For comparison, PFOS was also tested and observed to adsorb via the hydrophobic carbon-fluorine tail. Time-dependent adsorption behavior for PFOS was noted, with higher pH solution showing a higher rate of surface adsorption. These findings demonstrate the complexities involved in competition between electrostatic and hydrophobic interactions and contribute to future innovation in electrosorption methods for remediation of PFAS contamination. Figure 1
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (53) , 2545
Potential-Dependent Surface Enhanced Infrared Absorption Spectroscopy (SEIRAS) Study of Perfluoroalkyl Substances (PFAS)
Per- and polyfluoroalkyl substances (PFAS), often referred to as "forever chemicals," are persistent organic compounds with strong carbon-fluorine (C-F) bonds, making them highly stable and resistant to degradation. Since the 1940s, PFAS have been widely used in firefighting foam, food packaging, cookware, cosmetics, and paints. Their bioaccumulation in the environment raises significant concerns, as PFAS exposure—primarily through contaminated drinking water and food—has been linked to DNA modification, reproductive toxicity, immunotoxicity and cancer. To mitigate these risks, it is essential to develop effective methods for PFAS removal from water supplies. Perfluorooctanoic acid (PFOA) and perfluorooctane sulfonate (PFOS), are the most studied PFAS due to their wide use and bioaccumulation. These substances are being progressively eliminated worldwide, however, addressing contamination in existing water supplies remains an urgent priority. The capture and/or degradation of PFAS in water requires the development of successful separation methods and an understanding of its adsorption mechanisms. Whether for degradation, capture or detection applications, electrosorption is a key area of interest in the mitigation of PFAS in water. Understanding the mechanisms of surface adsorption and relationship with water is essential to innovation in remediation technology. Potential dependent surface-enhanced infrared absorption spectroscopy (SEIRAS) provides a powerful tool for studying PFAS adsorption at the electrode interface. PFOA and PFOS were analyzed with cyclic voltammetry and SEIRAS protocols in a NaClO 4 supporting electrolyte, across a range of pHs. Experimental observations describe PFOA adsorbing to the electrode via the hydrophobic tail, rather than the electronegative carboxylic acid head, confirmed by the large increase in C-F bond molecular vibrations at positive potentials. Potential cycling demonstrated weak adsorption hysteresis, and a disruption of surface interactions was observed in the presence of potassium bromide. For comparison, PFOS was also tested and observed to adsorb via the hydrophobic carbon-fluorine tail. Time-dependent adsorption behavior for PFOS was noted, with higher pH solution showing a higher rate of surface adsorption. These findings demonstrate the complexities involved in competition between electrostatic and hydrophobic interactions and contribute to future innovation in electrosorption methods for remediation of PFAS contamination. Figure 1
- 18 July 2025
- Published by American Chemical Society (ACS) in Analytical Chemistry
- Vol. 97 (29) , 15762-15770
Potential-Dependent SEIRAS Study of PFAS Surface Adsorption
Per- and polyfluoroalkyl substances (PFAS) and their bioaccumulation are growing priorities for water remediation efforts. Using surface-enhanced infrared absorption spectroscopy (SEIRAS), our measurements allowed observations of PFAS adsorption in response to surface charge. Increased adsorption of perfluorooctanoic acid (PFOA) was observed at positive potentials via the molecule's hydrophobic long-chain carbon-fluorine tail, despite the electronegativity of the carboxylic acid head. This behavior was observed at pH 2, 3, and 4, with a continued lay-flat orientation of the surface molecules due to the dominance of the hydrophobic interaction versus electrostatic interaction. Potential cycling demonstrated weak adsorption hysteresis, and a disruption of surface interactions was observed in the presence of potassium bromide. For comparison, perfluorooctanesulfonate (PFOS) was also tested and observed to adsorb via the hydrophobic carbon-fluorine tail. Time-dependent adsorption behavior for PFOS was noted, with a higher pH solution showing a higher rate of surface adsorption. These findings demonstrate the complexities involved in the competition between electrostatic and hydrophobic interactions and contribute to future innovation in electrosorption methods for remediation of PFAS contamination.
- 18 July 2025
- Published by American Chemical Society (ACS) in Analytical Chemistry
- Vol. 97 (29) , 15762-15770
Potential-Dependent SEIRAS Study of PFAS Surface Adsorption
Per- and polyfluoroalkyl substances (PFAS) and their bioaccumulation are growing priorities for water remediation efforts. Using surface-enhanced infrared absorption spectroscopy (SEIRAS), our measurements allowed observations of PFAS adsorption in response to surface charge. Increased adsorption of perfluorooctanoic acid (PFOA) was observed at positive potentials via the molecule's hydrophobic long-chain carbon-fluorine tail, despite the electronegativity of the carboxylic acid head. This behavior was observed at pH 2, 3, and 4, with a continued lay-flat orientation of the surface molecules due to the dominance of the hydrophobic interaction versus electrostatic interaction. Potential cycling demonstrated weak adsorption hysteresis, and a disruption of surface interactions was observed in the presence of potassium bromide. For comparison, perfluorooctanesulfonate (PFOS) was also tested and observed to adsorb via the hydrophobic carbon-fluorine tail. Time-dependent adsorption behavior for PFOS was noted, with a higher pH solution showing a higher rate of surface adsorption. These findings demonstrate the complexities involved in the competition between electrostatic and hydrophobic interactions and contribute to future innovation in electrosorption methods for remediation of PFAS contamination.
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01 (9) , 3143
In Situ Double Probe Beam Deflection Estimating Concentration Profiles of Battery Electrolytes
A deeper understanding of battery concentration gradients within the diffusion layer offers crucial information to address the limitations in innovative new electrochemical systems. An in situ double probe beam deflection (PBD) technique has been developed using two laser beams to map the concentration profile of the diffusion layer in an electrochemical cell. This approach features a microscale moving upper probe paired with a stationary secondary beam, enabling the real-time assessment of concentration gradients throughout the depth of the diffusion layer. Utilizing the double PBD method, concentration profiles for 0.1 mol/kg CuSO4 and ZnSO4 were plotted across a range of applied currents, showing increased magnitudes of gradients for higher currents. Both single and double beam PBD techniques were analyzed, demonstrating the distance and time dependence of the developing concentration gradient. While CuSO4 showed a systematic trend of increased response delay and decreased deflection with increased distance from the electrode, ZnSO4 experienced some additional phenomena affecting the refractive index within the diffusion layer. The in situ double probe beam deflection method has proven to be exceptionally sensitive, paving the way for future investigations into charge migration within this vital region of the electrochemical cell.
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01 (9) , 3143
In Situ Double Probe Beam Deflection Estimating Concentration Profiles of Battery Electrolytes
A deeper understanding of battery concentration gradients within the diffusion layer offers crucial information to address the limitations in innovative new electrochemical systems. An in situ double probe beam deflection (PBD) technique has been developed using two laser beams to map the concentration profile of the diffusion layer in an electrochemical cell. This approach features a microscale moving upper probe paired with a stationary secondary beam, enabling the real-time assessment of concentration gradients throughout the depth of the diffusion layer. Utilizing the double PBD method, concentration profiles for 0.1 mol/kg CuSO4 and ZnSO4 were plotted across a range of applied currents, showing increased magnitudes of gradients for higher currents. Both single and double beam PBD techniques were analyzed, demonstrating the distance and time dependence of the developing concentration gradient. While CuSO4 showed a systematic trend of increased response delay and decreased deflection with increased distance from the electrode, ZnSO4 experienced some additional phenomena affecting the refractive index within the diffusion layer. The in situ double probe beam deflection method has proven to be exceptionally sensitive, paving the way for future investigations into charge migration within this vital region of the electrochemical cell.
- Open Access
- 1 April 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (4) , 040521
In Situ Double Probe Beam Deflection Estimating Concentration Profiles of Battery Electrolytes
An in situ double probe beam deflection (PBD) technique has been developed using two laser beams to map the concentration profile of the diffusion layer in an electrochemical cell. A microscale moving upper probe and a fixed position secondary beam offer real-time concentration gradients to be profiled throughout the depth of the diffusion layer. The double PBD technique was used to plot concentration profiles for 0.1 mol kg−1 CuSO4 and ZnSO4 within a range of applied currents, showing increased magnitudes of gradients for higher currents. Both single and double beam PBD were explored, demonstrating the distance and time dependence of the developing concentration gradient. While CuSO4 showed a systematic trend of increased response delay and decreased deflection with increased distance from the electrode, ZnSO4 experienced some additional phenomena affecting the refractive index within the diffusion layer. The in situ double probe beam deflection was shown to be highly sensitive and offers future work in quantifying charge migration within this important region of the electrochemical cell.
- 1 April 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (4) , 040521
Open AccessIn Situ Double Probe Beam Deflection Estimating Concentration Profiles of Battery Electrolytes
An in situ double probe beam deflection (PBD) technique has been developed using two laser beams to map the concentration profile of the diffusion layer in an electrochemical cell. A microscale moving upper probe and a fixed position secondary beam offer real-time concentration gradients to be profiled throughout the depth of the diffusion layer. The double PBD technique was used to plot concentration profiles for 0.1 mol kg−1 CuSO4 and ZnSO4 within a range of applied currents, showing increased magnitudes of gradients for higher currents. Both single and double beam PBD were explored, demonstrating the distance and time dependence of the developing concentration gradient. While CuSO4 showed a systematic trend of increased response delay and decreased deflection with increased distance from the electrode, ZnSO4 experienced some additional phenomena affecting the refractive index within the diffusion layer. The in situ double probe beam deflection was shown to be highly sensitive and offers future work in quantifying charge migration within this important region of the electrochemical cell.
- 4 November 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (45) , 63026-63038
Potential-Dependent ATR-SEIRAS and EQCM-D Analysis of Interphase Formation in Zinc Battery Electrolytes
With the heightening interest in bivalent battery technology, there arises a necessity for a thorough investigation into zinc-ion battery (ZIB) electrolytes, accommodating their chemical attributes and potential-dependent structural dynamics. While the phenomenon of in situ solid electrolyte interphase formation is extensively documented in lithium-ion batteries, its analogous occurrences in ZIBs remain limited. Herein is a comparative study of three zinc electrolytes of interest: ZnSO4, ZnOTF, and Zn(TFSI)2/LiTFSI hybrid water-in-salt electrolyte. Additionally, the impact of an acetonitrile additive is scrutinized, with a comparative assessment of the interfacial behavior in aqueous solutions. Utilizing ATR-SEIRAS, potential-dependent alterations in the composition of the electrolyte/electrode interface were monitored, while EQCM-D facilitated a comprehensive understanding of variations in the mass and structural properties of the adsorbed layer. Aqueous ZnSO4 demonstrated the accumulation of porous Zn4SO4(OH)6·xH2O at negative potentials, leading to a mass of 1.47 μg cm-2 after five cycles. Bisulfate formation was observed at positive potentials. SEIRAS measurements for ZnOTF demonstrated reorientation and surface adsorption of CF3SO3- to favor CF3 at the surface for positive potentials, and acetonitrile showed increased stability for the electrode at negative potentials. The additive was also reported to lead to the accumulation of a substantial passivation layer with viscoelastic properties. The zinc water-in-salt showed exceptional surface stability at negative potentials and a widened potential window. A thin rigid zinc SEI layer is reported with a mass of 0.7 μg cm-2. The compositional intricacies of these surface structures are discussed in relation to their solvent conditions. This investigation not only sheds light on the initial charge/discharge cycles in ZIBs but also underscores their pivotal role in instigating enduring transformations that can significantly influence their long-term cycling performance.
- 4 November 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (45) , 63026-63038
Potential-Dependent ATR-SEIRAS and EQCM-D Analysis of Interphase Formation in Zinc Battery Electrolytes
With the heightening interest in bivalent battery technology, there arises a necessity for a thorough investigation into zinc-ion battery (ZIB) electrolytes, accommodating their chemical attributes and potential-dependent structural dynamics. While the phenomenon of in situ solid electrolyte interphase formation is extensively documented in lithium-ion batteries, its analogous occurrences in ZIBs remain limited. Herein is a comparative study of three zinc electrolytes of interest: ZnSO4, ZnOTF, and Zn(TFSI)2/LiTFSI hybrid water-in-salt electrolyte. Additionally, the impact of an acetonitrile additive is scrutinized, with a comparative assessment of the interfacial behavior in aqueous solutions. Utilizing ATR-SEIRAS, potential-dependent alterations in the composition of the electrolyte/electrode interface were monitored, while EQCM-D facilitated a comprehensive understanding of variations in the mass and structural properties of the adsorbed layer. Aqueous ZnSO4 demonstrated the accumulation of porous Zn4SO4(OH)6·xH2O at negative potentials, leading to a mass of 1.47 μg cm-2 after five cycles. Bisulfate formation was observed at positive potentials. SEIRAS measurements for ZnOTF demonstrated reorientation and surface adsorption of CF3SO3- to favor CF3 at the surface for positive potentials, and acetonitrile showed increased stability for the electrode at negative potentials. The additive was also reported to lead to the accumulation of a substantial passivation layer with viscoelastic properties. The zinc water-in-salt showed exceptional surface stability at negative potentials and a widened potential window. A thin rigid zinc SEI layer is reported with a mass of 0.7 μg cm-2. The compositional intricacies of these surface structures are discussed in relation to their solvent conditions. This investigation not only sheds light on the initial charge/discharge cycles in ZIBs but also underscores their pivotal role in instigating enduring transformations that can significantly influence their long-term cycling performance.
- 9 August 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-01 (1) , 65
Refractive Laser Beam Measuring Diffusion Coefficient of Concentrated Battery Electrolytes
A thorough understanding of electrolyte transport properties is crucial in the development of alternative battery technology. As a key parameter, the diffusion coefficient offers important insights into the behavior of electrolytes, especially for fast charge of high-energy batteries. Existing methods of measurement are often limited by redox species or offer questionable accuracy due to side reactions and/or disruption of the diffusion profile. A highly sensitive optical method was developed using a refractive laser beam through triangular diffusion column to measure the diffusion coefficient of concentrated battery electrolytes. The method based on Snell’s law can be applied to all liquid phase electrolytes since the refractive index is concentration dependent for all liquid electrolytes. This universal method relies on the deflection of a refractive laser beam passing through an electrolyte of a minor concentration gradient in a triangular diffusion column (Figure 1). A polarized HeNe laser was arranged to pass the beam through a right-angled triangular quartz precision cell, slightly rotated to the normal. The exact position of the refracted beam was located by a silicon photodiode-based position detector. Deflection calibration curves made simple conversion of beam position to concentration, and during the diffusion of two layered solutions, data points were collected every minute to produce a concentration profile descriptive of the 48-hour diffusion. Diffusion coefficients were calculated using a model based on OSM theory, accounting for multi-component concentrated systems in a restricted diffusion column.1 The measured diffusion coefficients are between 4.12x10-10 m2/s for 0.15 mol/kg ZnSO4 and 0.681x10-10 m2/s for 2.5 mol/kg ZnSO4 at 22.4 °C. The profile of concentration-dependent diffusion coefficients follows a non-linear inverse relationship described by the function D=4.943(1+m)-1.564 (Figure 2). Several other physicochemical properties of the same electrolytes were studied to correlate to the concentration-dependent diffusion coefficients, including refractive index, viscosity, conductivity, and microstructure analysis based on vibrational spectroscopy (Infrared and Raman). High concentration electrolytes with more ion pairs show increased viscosity which ultimately leads to smaller diffusion coefficients. A QCM-I instrument standard flow cell were used to determine the viscosity of ZnSO4 electrolyte and the concentration-dependent viscosity was fitted to the function η=1.06-0.476m+2.13m2-1.01m3+0.204m4. Interionic interactions also led to reduced conductivity at concentrations beyond 1.5mol/kg, despite the increased charge density of concentrated solutions. FT-IR spectrums allowed analyzation of increased charge density, which increased intensity of the O-H stretching peak in concentrated electrolytes, despite the decrease in the ratio of water. Competition between charge density and viscosity continues to challenge the efficiency of concentrated electrolytes. Lastly, we demonstrate the prototype in situ triangular cell to characterize the electrolyte in working batteries. The cell responds to short, low-voltage pulses with beam deflection and relaxation, and offers an opportunity as a novel in situ spectroscopic tool to characterize the battery electrolyte. Acknowledgments This work is supported by a grant from NSF (CBET-2243098). References [1] 13. J. Newman and T. W. Chapman, AIChE J., 19, 343–348 (1973). Figure 1
- 9 August 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-01 (1) , 65
Refractive Laser Beam Measuring Diffusion Coefficient of Concentrated Battery Electrolytes
A thorough understanding of electrolyte transport properties is crucial in the development of alternative battery technology. As a key parameter, the diffusion coefficient offers important insights into the behavior of electrolytes, especially for fast charge of high-energy batteries. Existing methods of measurement are often limited by redox species or offer questionable accuracy due to side reactions and/or disruption of the diffusion profile. A highly sensitive optical method was developed using a refractive laser beam through triangular diffusion column to measure the diffusion coefficient of concentrated battery electrolytes. The method based on Snell’s law can be applied to all liquid phase electrolytes since the refractive index is concentration dependent for all liquid electrolytes. This universal method relies on the deflection of a refractive laser beam passing through an electrolyte of a minor concentration gradient in a triangular diffusion column (Figure 1). A polarized HeNe laser was arranged to pass the beam through a right-angled triangular quartz precision cell, slightly rotated to the normal. The exact position of the refracted beam was located by a silicon photodiode-based position detector. Deflection calibration curves made simple conversion of beam position to concentration, and during the diffusion of two layered solutions, data points were collected every minute to produce a concentration profile descriptive of the 48-hour diffusion. Diffusion coefficients were calculated using a model based on OSM theory, accounting for multi-component concentrated systems in a restricted diffusion column.1 The measured diffusion coefficients are between 4.12x10-10 m2/s for 0.15 mol/kg ZnSO4 and 0.681x10-10 m2/s for 2.5 mol/kg ZnSO4 at 22.4 °C. The profile of concentration-dependent diffusion coefficients follows a non-linear inverse relationship described by the function D=4.943(1+m)-1.564 (Figure 2). Several other physicochemical properties of the same electrolytes were studied to correlate to the concentration-dependent diffusion coefficients, including refractive index, viscosity, conductivity, and microstructure analysis based on vibrational spectroscopy (Infrared and Raman). High concentration electrolytes with more ion pairs show increased viscosity which ultimately leads to smaller diffusion coefficients. A QCM-I instrument standard flow cell were used to determine the viscosity of ZnSO4 electrolyte and the concentration-dependent viscosity was fitted to the function η=1.06-0.476m+2.13m2-1.01m3+0.204m4. Interionic interactions also led to reduced conductivity at concentrations beyond 1.5mol/kg, despite the increased charge density of concentrated solutions. FT-IR spectrums allowed analyzation of increased charge density, which increased intensity of the O-H stretching peak in concentrated electrolytes, despite the decrease in the ratio of water. Competition between charge density and viscosity continues to challenge the efficiency of concentrated electrolytes. Lastly, we demonstrate the prototype in situ triangular cell to characterize the electrolyte in working batteries. The cell responds to short, low-voltage pulses with beam deflection and relaxation, and offers an opportunity as a novel in situ spectroscopic tool to characterize the battery electrolyte. Acknowledgments This work is supported by a grant from NSF (CBET-2243098). References [1] 13. J. Newman and T. W. Chapman, AIChE J., 19, 343–348 (1973). Figure 1
- Open Access
- 1 February 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (2) , 020551
Refractive Laser Beam Measuring Diffusion Coefficient of Concentrated Battery Electrolytes
A thorough understanding of electrolyte transport properties is crucial in the development of alternative battery technology. As a key parameter, the diffusion coefficient offers important insights into the behavior of electrolytes, especially for fast charge of high-energy batteries. Existing methods of measurement are often limited by redox species or offer questionable accuracy due to side reactions and/or disruption of the diffusion profile. This work provides a novel optical method for measuring diffusion coefficients of liquid-phase concentrated battery electrolytes without electrochemical reactions. The method relies on the deflection of a refractive laser beam passing through an electrolyte of a minor concentration gradient in a triangular diffusion column. The diffusion coefficient, D, for a range of zinc sulfate electrolytes was successfully extracted by correlating the position of the laser beam to its concentration. Several other physicochemical properties of the same electrolytes are studied to correlate to the concentration-dependent diffusion coefficients, including viscosity, conductivity, and microstructure analysis based on vibrational spectroscopy (Infrared and Raman). Also included is the future application of the triangular column for in situ electrochemical measurements.
- 1 February 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (2) , 020551
Open AccessRefractive Laser Beam Measuring Diffusion Coefficient of Concentrated Battery Electrolytes
A thorough understanding of electrolyte transport properties is crucial in the development of alternative battery technology. As a key parameter, the diffusion coefficient offers important insights into the behavior of electrolytes, especially for fast charge of high-energy batteries. Existing methods of measurement are often limited by redox species or offer questionable accuracy due to side reactions and/or disruption of the diffusion profile. This work provides a novel optical method for measuring diffusion coefficients of liquid-phase concentrated battery electrolytes without electrochemical reactions. The method relies on the deflection of a refractive laser beam passing through an electrolyte of a minor concentration gradient in a triangular diffusion column. The diffusion coefficient, D, for a range of zinc sulfate electrolytes was successfully extracted by correlating the position of the laser beam to its concentration. Several other physicochemical properties of the same electrolytes are studied to correlate to the concentration-dependent diffusion coefficients, including viscosity, conductivity, and microstructure analysis based on vibrational spectroscopy (Infrared and Raman). Also included is the future application of the triangular column for in situ electrochemical measurements.