Maria Sultana
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Maria Sultana has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Ariful Haque
Texas State University
4 shared publications - Pallab Kumar Sarkar
Texas State University
3 shared publications - Pujan Lamsal
Electrical Engineering, Ingram School of Engineering, Texas State University
2 shared publications Ravi Droopad
Materials Science, Engineering, and Commercialization Program, Texas State University
2 shared publications- Ravi Droopad
Department of Physics, Texas State University 2 , San Marcos, Texas 78666
2 shared publications Abdul Halim
Electrical Engineering, Ingram School of Engineering, Texas State University 1 , San Marcos, Texas 78666, USA
1 shared publication
Latest Publications
- Open Access
- 23 September 2026
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 59 (38) , 385302
Epitaxial growth and characterization of hexagonal ϵ-(In x Ga 1- x ) 2 O 3 ( x =0.05 and 0.15) on AlN
Growth parameter optimization to deposit hexagonal ϵ-(In x Ga 1-x ) 2 O 3 (x = 0.05 and 0.15) on AlN by pulsed laser deposition (PLD) was performed for the first time. The PLD heater temperature and chamber oxygen pressure were systematically tuned to fine-tune the optimum growth parameters of ϵ-(In x Ga 1-x ) 2 O 3 on AlN. A heater temperature of 550 ∘ C was the most suitable temperature to obtain the metastable hexagonal phase, avoiding polycrystallinity, suppressing the formation of cubic indium oxide, and inhibiting transformation to the monoclinic β-Ga 2 O 3 phase. A chamber pressure of 1.25 × 10 −2 Torr was necessary to uniformly incorporate indium throughout the ϵ-Ga 2 O 3 lattice and turn it into ϵ-(In x Ga 1-x ) 2 O 3 . The X-ray diffraction (XRD) phi scans confirmed the hexagonal phase, and the epitaxial relationship was determined to be (105) ϵ-(In x Ga 1- x ) 2 O 3 (103) AlN. The presence of indium in the ϵ-Ga 2 O 3 was confirmed by XRD 2θ peak position shift and X-ray photoelectron spectroscopy (XPS) via the elemental scan depth profile, with a minor presence of unoxidized gallium atoms and oxygen vacancy centers. The measured bandgaps were 4.55 eV and 4.86 eV for ϵ-(In 0.15 Ga 0.85 ) 2 O 3 and ϵ-(In 0.05 Ga 0.95 ) 2 O 3 , respectively.
- 23 September 2026
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 59 (38) , 385302
Open AccessEpitaxial growth and characterization of hexagonal ϵ-(In x Ga 1- x ) 2 O 3 ( x =0.05 and 0.15) on AlN
Growth parameter optimization to deposit hexagonal ϵ-(In x Ga 1-x ) 2 O 3 (x = 0.05 and 0.15) on AlN by pulsed laser deposition (PLD) was performed for the first time. The PLD heater temperature and chamber oxygen pressure were systematically tuned to fine-tune the optimum growth parameters of ϵ-(In x Ga 1-x ) 2 O 3 on AlN. A heater temperature of 550 ∘ C was the most suitable temperature to obtain the metastable hexagonal phase, avoiding polycrystallinity, suppressing the formation of cubic indium oxide, and inhibiting transformation to the monoclinic β-Ga 2 O 3 phase. A chamber pressure of 1.25 × 10 −2 Torr was necessary to uniformly incorporate indium throughout the ϵ-Ga 2 O 3 lattice and turn it into ϵ-(In x Ga 1-x ) 2 O 3 . The X-ray diffraction (XRD) phi scans confirmed the hexagonal phase, and the epitaxial relationship was determined to be (105) ϵ-(In x Ga 1- x ) 2 O 3 (103) AlN. The presence of indium in the ϵ-Ga 2 O 3 was confirmed by XRD 2θ peak position shift and X-ray photoelectron spectroscopy (XPS) via the elemental scan depth profile, with a minor presence of unoxidized gallium atoms and oxygen vacancy centers. The measured bandgaps were 4.55 eV and 4.86 eV for ϵ-(In 0.15 Ga 0.85 ) 2 O 3 and ϵ-(In 0.05 Ga 0.95 ) 2 O 3 , respectively.
- Open Access
- 27 February 2026
- Published by Elsevier in SSRN Electronic Journal
Direct Fabrication of Diamond Films on β-Ga₂O₃ Using Q-carbon
Beta gallium oxide (β-Ga₂O₃) is a promising ultrawide-bandgap (UWBG) semiconductor for high-power electronic devices. However, its low thermal conductivity critically limits device performance. While diamond integration can address thermal management, it suffers from challenges such as stress, decomposition, and surface energy mismatch. To overcome these difficulties, pulsed laser annealing is used to form a thin quenched carbon (Q-carbon) layer on β-Ga₂O₃, promoting diamond growth while preventing cracking, delamination, and oxide-layer degradation. Simulation results show a melt regrowth velocity of 12.5 m/s that enables Q-carbon/nanodiamond composite formation on β-Ga₂O₃. Using Q-carbon as a seed layer resulted in the formation of a high-quality, uniform diamond film with minimal graphitic content and a sharp T2g peak at 1332.6 cm⁻¹ with an FWHM of 9.28 cm⁻¹. Furthermore, Q-carbon helps minimize the thermal mismatch between the diamond and β-Ga₂O₃ films, thereby preventing delamination of the diamond film during post-deposition cooling. Stress in diamond/Q-carbon/β-Ga₂O₃ was reduced by ~70% compared to untreated diamond/β-Ga₂O₃ and ~75% compared to diamond/c-Al₂O₃. Additionally, Q-carbon boosts the formation of well-faceted five-fold twinned diamond crystals and accelerates the growth of columnar structure diamond film. This study successfully addresses a persistent challenge in diamond nucleation and the fabrication of high-quality, large-area diamond growth on β-Ga₂O₃.
- 27 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessDirect Fabrication of Diamond Films on β-Ga₂O₃ Using Q-carbon
Beta gallium oxide (β-Ga₂O₃) is a promising ultrawide-bandgap (UWBG) semiconductor for high-power electronic devices. However, its low thermal conductivity critically limits device performance. While diamond integration can address thermal management, it suffers from challenges such as stress, decomposition, and surface energy mismatch. To overcome these difficulties, pulsed laser annealing is used to form a thin quenched carbon (Q-carbon) layer on β-Ga₂O₃, promoting diamond growth while preventing cracking, delamination, and oxide-layer degradation. Simulation results show a melt regrowth velocity of 12.5 m/s that enables Q-carbon/nanodiamond composite formation on β-Ga₂O₃. Using Q-carbon as a seed layer resulted in the formation of a high-quality, uniform diamond film with minimal graphitic content and a sharp T2g peak at 1332.6 cm⁻¹ with an FWHM of 9.28 cm⁻¹. Furthermore, Q-carbon helps minimize the thermal mismatch between the diamond and β-Ga₂O₃ films, thereby preventing delamination of the diamond film during post-deposition cooling. Stress in diamond/Q-carbon/β-Ga₂O₃ was reduced by ~70% compared to untreated diamond/β-Ga₂O₃ and ~75% compared to diamond/c-Al₂O₃. Additionally, Q-carbon boosts the formation of well-faceted five-fold twinned diamond crystals and accelerates the growth of columnar structure diamond film. This study successfully addresses a persistent challenge in diamond nucleation and the fabrication of high-quality, large-area diamond growth on β-Ga₂O₃.
- Open Access
- 15 March 2024
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 135 (11)
Growth optimization, optical, and dielectric properties of heteroepitaxially grown ultrawide-bandgap ZnGa2O4 (111) thin film
Ultrawide bandgap ZnGa2O4 (ZGO) thin films were grown on sapphire (0001) substrates at various growth temperatures with a perspective to investigate the electrical and optical characteristics required for high-power electronic applications. Due to the variation in the vapor pressure of Zn and Ga, severe loss of Zn was observed during pulsed laser deposition, which was solved by using a zinc-rich Zn0.98Ga0.02O target. A pure phase single-crystalline ZGO thin film was obtained at a deposition temperature of 750 °C and an oxygen pressure of 1 × 10−2 Torr. The out-of-plane epitaxial relationship between the sapphire and ZGO thin film was obtained from φ-scan. The x-ray rocking curve of the ZGO thin film grown at 750 °C exhibits a full width at half maximum of ∼0.098°, which indicates a good crystalline phase and quality of the thin film. Core-level x-ray photoelectron spectroscopy of ZGO grown at 750 °C indicated that Zn and Ga were in the 2+ and 3+ oxidation states, respectively, and the atomic ratio of Zn/Ga was estimated to be ∼0.48 from the fitted values of Zn-2p3/2 and Ga-2p3/2. The high-resolution transmission electron microscopy images revealed a sharp interface with the thickness of the ZGO film of ∼265 nm, and the signature of minor secondary phases was observed. The bandgap of the ZGO film at different growth temperatures was calculated from the ultraviolet-diffuse reflectance spectroscopy spectra, and its value was obtained to be ∼5.08 eV for the 750 °C grown sample. The refractive index (n) and the extinction coefficient (k) were determined to be ∼1.94 and 0.023 from the ellipsometric data, respectively, and the real dielectric function (ɛr) was estimated to be ∼6.8 at energy 5 eV. The ultrawide bandgap and dielectric function of ZGO recommend its possible potential applications in deep-ultraviolet optoelectronic devices and high-power electronics.
- 15 March 2024
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 135 (11)
Open AccessGrowth optimization, optical, and dielectric properties of heteroepitaxially grown ultrawide-bandgap ZnGa2O4 (111) thin film
Ultrawide bandgap ZnGa2O4 (ZGO) thin films were grown on sapphire (0001) substrates at various growth temperatures with a perspective to investigate the electrical and optical characteristics required for high-power electronic applications. Due to the variation in the vapor pressure of Zn and Ga, severe loss of Zn was observed during pulsed laser deposition, which was solved by using a zinc-rich Zn0.98Ga0.02O target. A pure phase single-crystalline ZGO thin film was obtained at a deposition temperature of 750 °C and an oxygen pressure of 1 × 10−2 Torr. The out-of-plane epitaxial relationship between the sapphire and ZGO thin film was obtained from φ-scan. The x-ray rocking curve of the ZGO thin film grown at 750 °C exhibits a full width at half maximum of ∼0.098°, which indicates a good crystalline phase and quality of the thin film. Core-level x-ray photoelectron spectroscopy of ZGO grown at 750 °C indicated that Zn and Ga were in the 2+ and 3+ oxidation states, respectively, and the atomic ratio of Zn/Ga was estimated to be ∼0.48 from the fitted values of Zn-2p3/2 and Ga-2p3/2. The high-resolution transmission electron microscopy images revealed a sharp interface with the thickness of the ZGO film of ∼265 nm, and the signature of minor secondary phases was observed. The bandgap of the ZGO film at different growth temperatures was calculated from the ultraviolet-diffuse reflectance spectroscopy spectra, and its value was obtained to be ∼5.08 eV for the 750 °C grown sample. The refractive index (n) and the extinction coefficient (k) were determined to be ∼1.94 and 0.023 from the ellipsometric data, respectively, and the real dielectric function (ɛr) was estimated to be ∼6.8 at energy 5 eV. The ultrawide bandgap and dielectric function of ZGO recommend its possible potential applications in deep-ultraviolet optoelectronic devices and high-power electronics.