Shoubin Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Shoubin Zhang has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Fuwei Wang
Research Institute for Frontier Science, Beihang University, Beijing 100191, China
1 shared publication - Hu Zhang
Beihang Univ, Sch Mat Sci & Engn, Beijing 100191, Peoples R China
1 shared publication - Huarui Zhang
School of Materials Science and Engineering, Beihang University, Beijing, China
1 shared publication - Kai Guan
Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing, China
1 shared publication - Rui Zhang
Ningbo Institute of Technology (NIT), Beihang University, Ningbo 315000, China
1 shared publication - Wenbo Wang
Beihang Univ, Dept Ningbo Innovat Res Inst, Ningbo 315800, Peoples R China
1 shared publication
Latest Publications
- Open Access
Study of the Microstructure Characterization and In Situ Observation of Crack Propagation in TC4/Al3Ti Metal–Intermetallic Laminated Composites
TC4/Al3Ti metal–intermetallic laminated (MIL) composites were fabricated by the vacuum hot-pressing process at 650 °C. The microstructure characteristics, i.e., grain boundary distribution, crystallographic orientation and Kernel Average Misorientation (KAM) map, were analyzed using EBSD. Meanwhile, the distribution of local strain and the fracture behavior of TC4/Al3Ti MIL composites during tensile process were determined by Digital Image Correlation (DIC) and in situ tensile experiments, respectively. Results show that the TC4/Al3Ti interfaces are well bonded and exhibit a distinct wavy morphology. The obvious Kirkendall pores and centerline are observed within the central region of the Al3Ti layer. The texture components of (10-10) and (11-20) are predominant in the TC4 layers; (100) and (110) are observed in the Al3Ti layer. Additionally, the average geometrically necessary dislocation (GNDs) density is 2.53 × 1014 m−2 in the TC4 layer, whereas it is 1.74 × 1014 m−2 in the Al3Ti layer. In the tensile test, the fracture resistance of TC4/Al3Ti MIL composites is significantly improved by the plastic deformation of the TC4 layers and the suppression of crack-tip instability. It is found that the extrinsic toughening mechanisms contain crack deflection, crack blunting, crack bridging, multiple cracking modes, and the plastic deformation of ductile TC4 layers in TC4/Al3Ti MIL composites. The real-time observation technique may provide more complete insights into the relationship between fracture behavior and enhanced toughness.
Open AccessStudy of the Microstructure Characterization and In Situ Observation of Crack Propagation in TC4/Al3Ti Metal–Intermetallic Laminated Composites
TC4/Al3Ti metal–intermetallic laminated (MIL) composites were fabricated by the vacuum hot-pressing process at 650 °C. The microstructure characteristics, i.e., grain boundary distribution, crystallographic orientation and Kernel Average Misorientation (KAM) map, were analyzed using EBSD. Meanwhile, the distribution of local strain and the fracture behavior of TC4/Al3Ti MIL composites during tensile process were determined by Digital Image Correlation (DIC) and in situ tensile experiments, respectively. Results show that the TC4/Al3Ti interfaces are well bonded and exhibit a distinct wavy morphology. The obvious Kirkendall pores and centerline are observed within the central region of the Al3Ti layer. The texture components of (10-10) and (11-20) are predominant in the TC4 layers; (100) and (110) are observed in the Al3Ti layer. Additionally, the average geometrically necessary dislocation (GNDs) density is 2.53 × 1014 m−2 in the TC4 layer, whereas it is 1.74 × 1014 m−2 in the Al3Ti layer. In the tensile test, the fracture resistance of TC4/Al3Ti MIL composites is significantly improved by the plastic deformation of the TC4 layers and the suppression of crack-tip instability. It is found that the extrinsic toughening mechanisms contain crack deflection, crack blunting, crack bridging, multiple cracking modes, and the plastic deformation of ductile TC4 layers in TC4/Al3Ti MIL composites. The real-time observation technique may provide more complete insights into the relationship between fracture behavior and enhanced toughness.
- Open Access
The Influence of Yttrium Content and Ceramic Crucible Materials on Desulfurization during Vacuum Induction Melting of DD5 Superalloys
In this study, the effect of adding different contents of yttrium (Y) during vacuum induction melting in Al2O3 and Y2O3 crucibles on the purification of DD5 alloys was investigated. The results show that the Y2O3 crucible exhibited great crucible stability and an excellent desulfurization effect when melting a Y-containing DD5 alloy. The S content of the alloy was reduced from 5.03 ppm to 1.36 ppm with the addition of 0.50 wt.% Y. Element Y combined with free S in the melt to form the YS phase, which was removed from the condensate shell and slag during the vacuum induction melting (VIM) process. Meanwhile, when the alloy was melted in the Y2O3 crucible with 0.50 wt.% Y addition, there was a reduction in S content from 2.77 ppm to 1.36 ppm compared to the Al2O3 crucible. Additionally, the loss of Y decreased from 0.12 wt.% to 0.05 wt.%.
Open AccessThe Influence of Yttrium Content and Ceramic Crucible Materials on Desulfurization during Vacuum Induction Melting of DD5 Superalloys
In this study, the effect of adding different contents of yttrium (Y) during vacuum induction melting in Al2O3 and Y2O3 crucibles on the purification of DD5 alloys was investigated. The results show that the Y2O3 crucible exhibited great crucible stability and an excellent desulfurization effect when melting a Y-containing DD5 alloy. The S content of the alloy was reduced from 5.03 ppm to 1.36 ppm with the addition of 0.50 wt.% Y. Element Y combined with free S in the melt to form the YS phase, which was removed from the condensate shell and slag during the vacuum induction melting (VIM) process. Meanwhile, when the alloy was melted in the Y2O3 crucible with 0.50 wt.% Y addition, there was a reduction in S content from 2.77 ppm to 1.36 ppm compared to the Al2O3 crucible. Additionally, the loss of Y decreased from 0.12 wt.% to 0.05 wt.%.