Ziqiang Yin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ziqiang Yin has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Gang Yu
School of Materials Science and Engineering, Shijiazhuang Tiedao University, Shijiazhuang 050043, China
1 shared publication - Haifeng Nie
College of Materials Science and Engineering, China Jiliang University, Hangzhou 310018, China
1 shared publication - Junshuai Chen
School of Materials Science and Engineering , Hebei Provincial Key Laboratory of Traffic Engineering Materials, Shijiazhuang Tiedao University, Shijiazhuang 050043, China
1 shared publication - Ping-Zhan Si
China Jiliang University
1 shared publication - Qing Huang
YongJiang Laboratory
1 shared publication - Quanxing Ren
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
1 shared publication
Latest Publications
- Open Access
Effects of Preformed Composition and Pore Size on Microstructure and Properties of SiCf/SiC Composites via Reactive Melt Infiltration
This study investigated the influence of preformed composition and pore size on the microstructure and properties of SiCf/SiC composites fabricated via reactive melt infiltration (RMI). The process began with the impregnation of SiC fiber cloth with phenolic resin, followed by lamination and pyrolysis. Subsequent steps included further impregnations with phenolic resin, SiC slurry, and carbon black slurry, each followed by additional pyrolysis. This process resulted in three types of preforms, designated as PP, PS, and PC. These preforms exhibited a multimodal distribution of pore size, with peak pore diameters around 5 μm for PP, ranging from 200 nm to 4 μm for PS, and approximately 150 nm for PC. The preforms were then subjected to molten silicon infiltration at 1600 °C under vacuum for 1 h to create SiCf/SiC composites. The PP preform contained only pyrolytic carbon, leading to a composite with high closed porosity and unreacted carbon, resulting in poor mechanical properties. The PS preform, which was impregnated with SiC particles, displayed an optimized pore size distribution but retained significant amounts of residual silicon and carbon in the final composite. In contrast, the PC preform featured both an ideal pore size distribution and an adequate amount of carbon, achieving high density and low porosity with reduced residual phases in the final composite. This optimization led to a flexural strength of 152.4 ± 15.4 MPa, an elastic modulus of about 181.1 ± 0.1 GPa, and a thermal conductivity of 27.7 W/mK in the SiCf/SiC composites product. These findings underscore the importance of preform optimization in enhancing the performance of SiCf/SiC composites, potentially paving the way for more reliable nuclear fuel cladding solutions.
Open AccessEffects of Preformed Composition and Pore Size on Microstructure and Properties of SiCf/SiC Composites via Reactive Melt Infiltration
This study investigated the influence of preformed composition and pore size on the microstructure and properties of SiCf/SiC composites fabricated via reactive melt infiltration (RMI). The process began with the impregnation of SiC fiber cloth with phenolic resin, followed by lamination and pyrolysis. Subsequent steps included further impregnations with phenolic resin, SiC slurry, and carbon black slurry, each followed by additional pyrolysis. This process resulted in three types of preforms, designated as PP, PS, and PC. These preforms exhibited a multimodal distribution of pore size, with peak pore diameters around 5 μm for PP, ranging from 200 nm to 4 μm for PS, and approximately 150 nm for PC. The preforms were then subjected to molten silicon infiltration at 1600 °C under vacuum for 1 h to create SiCf/SiC composites. The PP preform contained only pyrolytic carbon, leading to a composite with high closed porosity and unreacted carbon, resulting in poor mechanical properties. The PS preform, which was impregnated with SiC particles, displayed an optimized pore size distribution but retained significant amounts of residual silicon and carbon in the final composite. In contrast, the PC preform featured both an ideal pore size distribution and an adequate amount of carbon, achieving high density and low porosity with reduced residual phases in the final composite. This optimization led to a flexural strength of 152.4 ± 15.4 MPa, an elastic modulus of about 181.1 ± 0.1 GPa, and a thermal conductivity of 27.7 W/mK in the SiCf/SiC composites product. These findings underscore the importance of preform optimization in enhancing the performance of SiCf/SiC composites, potentially paving the way for more reliable nuclear fuel cladding solutions.
- Open Access
- 3 April 2024
- Published by LIDSEN Publishing Inc in Recent Progress in Materials
- Vol. 06 (02) , 1-48
Review on the Development of Titanium Diboride Ceramics
Titanium diboride (TiB2) materials have garnered significant attention due to their remarkable comprehensive properties. They offer potential applications in high-temperature structural materials, cutting tools, armor, electrodes for metal smelting, and wear-resistant parts. However, due to the low self-diffusion coefficient, the TiB2 exhibits poor sinterability, excessive grain growth at elevated temperatures, and inadequate oxidation resistance, limiting its wide application. Therefore, many research works are devoted to processing TiB2 at a lower sintering temperature and improving the properties through various sintering additives and more advanced techniques. This article comprehensively reviews the multiple synthesis methods and sintering technologies of TiB2, and at the same time, critically discusses the impacts of sintering additives and reinforcing agents on densification, microstructure, and various properties, including those at high temperatures, and finally predicts the future development of TiB2 composite materials.
- 3 April 2024
- Published by LIDSEN Publishing Inc in Recent Progress in Materials
- Vol. 06 (02) , 1-48
Open AccessReview on the Development of Titanium Diboride Ceramics
Titanium diboride (TiB2) materials have garnered significant attention due to their remarkable comprehensive properties. They offer potential applications in high-temperature structural materials, cutting tools, armor, electrodes for metal smelting, and wear-resistant parts. However, due to the low self-diffusion coefficient, the TiB2 exhibits poor sinterability, excessive grain growth at elevated temperatures, and inadequate oxidation resistance, limiting its wide application. Therefore, many research works are devoted to processing TiB2 at a lower sintering temperature and improving the properties through various sintering additives and more advanced techniques. This article comprehensively reviews the multiple synthesis methods and sintering technologies of TiB2, and at the same time, critically discusses the impacts of sintering additives and reinforcing agents on densification, microstructure, and various properties, including those at high temperatures, and finally predicts the future development of TiB2 composite materials.