Sheng-Tao Qiu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Sheng-Tao Qiu has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Jialong Qiao
Iron and Steel Research Institute Co., Ltd., Beijing 100081, China
2 shared publications - Chao Shi
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing
1 shared publication - Cheng Song
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing
1 shared publication Chuan-Xing Liu
WISDRI(xinyu) Cold Processing Engineering Co. Ltd, Xinyu 338029, PR China
1 shared publicationFei-Hu Guo
National Engineering Research Center of Continuous Casting Technology, China Iron & Steel Research Institute Group, Beijing 100081, PR China
1 shared publication- Jianfeng Liu
Xinyu Iron and Steel Group Co., Ltd
1 shared publication
Latest Publications
- Open Access
- 15 April 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (6) , 1000-1009
Effect of Rare Earth La–Ce on Solidification Structure of 3.2%Si-0.9%Al Non-oriented Silicon Steel
The effect of rare earth on the solidification structure of 3.2%Si-0.9%Al non-oriented silicon steel was investigated using industrial trials. The outputs demonstrated that increasing rare earth content leads to a decrease in the average size of equiaxed crystals in the casting billets. In order to further understand the rare earth on the grain refinement of δ-ferrite, the conventional inclusion detection technology, was used to investigate the distribution characteristics of inclusions, together with theoretical calculation of the equilibrium partition coefficients, pinning forces and mismatch degrees. The detection results of inclusions and the calculation results of pinning force showed that the effect of rare earth on the pinning force of inclusions was marginal. Thermodynamic calculation indicated that Ce addition had negligible effect on the equilibrium partition coefficient of Si, Al and Mn. Combined with the calculation results of GRF model, it is reasonable to consider that the contribution of rare earth element to the refinement of equiaxed crystals can be ignored. Further, the outcomes obtained from the E2EM model calculations revealed that the principal mechanism responsible for the refinement of equiaxed crystals through rare earth treatment can be attributed to the heterogeneous nucleation effect of (La, Ce)2O2S.
- 15 April 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (6) , 1000-1009
Open AccessEffect of Rare Earth La–Ce on Solidification Structure of 3.2%Si-0.9%Al Non-oriented Silicon Steel
The effect of rare earth on the solidification structure of 3.2%Si-0.9%Al non-oriented silicon steel was investigated using industrial trials. The outputs demonstrated that increasing rare earth content leads to a decrease in the average size of equiaxed crystals in the casting billets. In order to further understand the rare earth on the grain refinement of δ-ferrite, the conventional inclusion detection technology, was used to investigate the distribution characteristics of inclusions, together with theoretical calculation of the equilibrium partition coefficients, pinning forces and mismatch degrees. The detection results of inclusions and the calculation results of pinning force showed that the effect of rare earth on the pinning force of inclusions was marginal. Thermodynamic calculation indicated that Ce addition had negligible effect on the equilibrium partition coefficient of Si, Al and Mn. Combined with the calculation results of GRF model, it is reasonable to consider that the contribution of rare earth element to the refinement of equiaxed crystals can be ignored. Further, the outcomes obtained from the E2EM model calculations revealed that the principal mechanism responsible for the refinement of equiaxed crystals through rare earth treatment can be attributed to the heterogeneous nucleation effect of (La, Ce)2O2S.
- 24 February 2021
- Published by EDP Sciences in Metallurgical Research & Technology
- Vol. 118 (1) , 113
Development of thin-gauge low iron loss non-oriented silicon steel
Microstructure, texture, inclusions and precipitates in Fe-2.97wt%Si non-oriented silicon steel during manufacture were investigated using Scanning Electron Microscopy (SEM), Organic Solvent Electrolysis and Electron Backscattered Diffraction(EBSD)techniques. The P10/400, P15/50 and B50 of thin-gauge non-oriented silicon steel with 0.3 mm in thickness were 13.85 W/kg, 2.38 W/kg and 1.66 T, respectively. Due to annealing of hot rolled band, the size of precipitates increased. The precipitates are mostly located at the grain boundaries in the annealed sheet, the main and average size of the grain-boundary precipitates were in the range of 30 ∼ 500 nm and 63.2 nm, respectively. The pinning force caused by 100 ∼ 300 nm particles at the grain boundaries was the largest, 70 ∼ 100 nm was second. During annealing of hot rolled band, the α*-fiber texture significantly developed and γ-fiber dropped dramatically. The γ-fiber texture and α*-fiber texture composed the main textures of annealed sheet. The texture randomization would give rise to better magnetic properties compared to the γ-fiber.
- 24 February 2021
- Published by EDP Sciences in Metallurgical Research & Technology
- Vol. 118 (1) , 113
Development of thin-gauge low iron loss non-oriented silicon steel
Microstructure, texture, inclusions and precipitates in Fe-2.97wt%Si non-oriented silicon steel during manufacture were investigated using Scanning Electron Microscopy (SEM), Organic Solvent Electrolysis and Electron Backscattered Diffraction(EBSD)techniques. The P10/400, P15/50 and B50 of thin-gauge non-oriented silicon steel with 0.3 mm in thickness were 13.85 W/kg, 2.38 W/kg and 1.66 T, respectively. Due to annealing of hot rolled band, the size of precipitates increased. The precipitates are mostly located at the grain boundaries in the annealed sheet, the main and average size of the grain-boundary precipitates were in the range of 30 ∼ 500 nm and 63.2 nm, respectively. The pinning force caused by 100 ∼ 300 nm particles at the grain boundaries was the largest, 70 ∼ 100 nm was second. During annealing of hot rolled band, the α*-fiber texture significantly developed and γ-fiber dropped dramatically. The γ-fiber texture and α*-fiber texture composed the main textures of annealed sheet. The texture randomization would give rise to better magnetic properties compared to the γ-fiber.