Jiajia Peng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jiajia Peng has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Jianbing Wu
School of Textile Garment & Design, Changshu Institute of Technology, Changshu 215500, China
2 shared publications - Jishu Zhang
School of Textile Garment & Design, Changshu Institute of Technology, Changshu 215500, China
2 shared publications - Mengxin Zhang
School of Textile Garment & Design, Changshu Institute of Technology, Changshu 215500, China
2 shared publications - Dongsheng Li
School of Computer Science and Artificial Intelligence, Wuhan Textile University, Wuhan, China
1 shared publication - Jin Tao
Department of Textile, Garment and Design Suzhou University of Technology Suzhou China
1 shared publication - Jinxing Liang
School of Computer Science and Artificial Intelligence, Wuhan Textile University, Wuhan 430200, China
1 shared publication
Latest Publications
- Open Access
Development and Performance of Negative Ion Functional Blended Yarns and Double-Sided Knitted Fabrics Based on ZnO/TM/PET Fiber
Zinc oxide-modified tourmaline-based negative ion polyester fiber (ZnO/TM/PET), as a new functional fiber with excellent negative ion emission characteristics, is of great significance to human health, and its industrial application needs to be expanded and promoted. In this paper, using zinc oxide, tourmaline, and polyethylene terephthalate as the main raw materials, ZnO/TM/PET negative ion functional fiber with 5% ZnO/TM composites was prepared. Then, it was blended with cotton fiber and interknitted with wool yarn and spandex yarn, from which we developed five kinds of negative ion polyester/cotton-blended yarn and four different kinds of knitted double-sided fabric using different equipment and process parameters. The micromorphology of the fiber samples, the basic properties of the blended yarns, and the wearability and functional properties of the knitted fabrics were tested. The results show that the ZnO/TM negative ion additive is randomly dispersed in the polymer matrix without visible conglobation and the fiber has a good appearance. The blending ratio has an important effect on the properties of functional polyester/cotton blended yarn. The higher the ratio of negative ion polyester fiber in the blended yarn, the better the mechanical index of the blended yarn, the higher the negative ion emission, and the lower the hairiness index. The performances of fabric are influenced by the comprehensive action of fiber raw material type, yarn ratio, fabric tightness, and structure. The mechanical properties of the fabric knitted from negative ion polyester/cotton-blended yarn are lower than those made from negative ion polyester filament yarn. In the case of the same fabric structure, the negative ion emission performance, far-infrared emission performance, and antibacterial property of the fabric with a higher ratio of negative ion functional fiber is better than the lower ratio. With the same yarn composition, the negative ion emission performance and air permeability of the fabric with a loose structure are better than that of the fabric with a tight structure, but the moisture permeability, far-infrared emission properties, and antibacterial properties show little difference.
Open AccessDevelopment and Performance of Negative Ion Functional Blended Yarns and Double-Sided Knitted Fabrics Based on ZnO/TM/PET Fiber
Zinc oxide-modified tourmaline-based negative ion polyester fiber (ZnO/TM/PET), as a new functional fiber with excellent negative ion emission characteristics, is of great significance to human health, and its industrial application needs to be expanded and promoted. In this paper, using zinc oxide, tourmaline, and polyethylene terephthalate as the main raw materials, ZnO/TM/PET negative ion functional fiber with 5% ZnO/TM composites was prepared. Then, it was blended with cotton fiber and interknitted with wool yarn and spandex yarn, from which we developed five kinds of negative ion polyester/cotton-blended yarn and four different kinds of knitted double-sided fabric using different equipment and process parameters. The micromorphology of the fiber samples, the basic properties of the blended yarns, and the wearability and functional properties of the knitted fabrics were tested. The results show that the ZnO/TM negative ion additive is randomly dispersed in the polymer matrix without visible conglobation and the fiber has a good appearance. The blending ratio has an important effect on the properties of functional polyester/cotton blended yarn. The higher the ratio of negative ion polyester fiber in the blended yarn, the better the mechanical index of the blended yarn, the higher the negative ion emission, and the lower the hairiness index. The performances of fabric are influenced by the comprehensive action of fiber raw material type, yarn ratio, fabric tightness, and structure. The mechanical properties of the fabric knitted from negative ion polyester/cotton-blended yarn are lower than those made from negative ion polyester filament yarn. In the case of the same fabric structure, the negative ion emission performance, far-infrared emission performance, and antibacterial property of the fabric with a higher ratio of negative ion functional fiber is better than the lower ratio. With the same yarn composition, the negative ion emission performance and air permeability of the fabric with a loose structure are better than that of the fabric with a tight structure, but the moisture permeability, far-infrared emission properties, and antibacterial properties show little difference.
- 8 March 2025
- Published by Springer Nature in The Visual Computer
- p. 1-14
Enhancing low-frequency stitch code generation for knitted fabrics: an LFSCG-E-Net approach
- 8 March 2025
- Published by Springer Nature in The Visual Computer
- p. 1-14
Enhancing low-frequency stitch code generation for knitted fabrics: an LFSCG-E-Net approach
- Open Access
Preparation and Performance of a Novel ZnO/TM/PET Composite Negative Ion Functional Fiber
Using zinc oxide (ZnO), tourmaline (TM), and polyethylene terephthalate (PET) as main raw materials, a novel ZnO/TM/PET negative ion functional fiber was created. The rheological properties of a ZnO/TM/PET masterbatch were investigated; the morphology, XRD, and FT-IR of the fibers were observed; and the mechanical properties, thermal properties, and negative ion release properties of the new fiber were tested. The results showed that the average particle size of the ZnO/TM composite is nearly 365 nm, with an increase in negative ion emission efficiency by nearly 50% compared to the original TM. The apparent viscosity of fiber masterbatch decreases with the increase in the addition of the ZnO/TM composite, and the rheological properties of the PET fiber masterbatch are not significantly effected, still showing shear thinning characteristics when the amount of addition reaches 10%. The ZnO/TM composite disperses well in the interior and surface of the ZnO/TM/PET fiber matrix. The prepared ZnO/TM/PET fiber has excellent properties, such as fineness of 1.54 dtex, glass transition temperature of 122.4 °C, fracture strength of 3.31 cN/dtex, and negative ion release of 1640/cm3, which shows great industrialization potential.
Open AccessPreparation and Performance of a Novel ZnO/TM/PET Composite Negative Ion Functional Fiber
Using zinc oxide (ZnO), tourmaline (TM), and polyethylene terephthalate (PET) as main raw materials, a novel ZnO/TM/PET negative ion functional fiber was created. The rheological properties of a ZnO/TM/PET masterbatch were investigated; the morphology, XRD, and FT-IR of the fibers were observed; and the mechanical properties, thermal properties, and negative ion release properties of the new fiber were tested. The results showed that the average particle size of the ZnO/TM composite is nearly 365 nm, with an increase in negative ion emission efficiency by nearly 50% compared to the original TM. The apparent viscosity of fiber masterbatch decreases with the increase in the addition of the ZnO/TM composite, and the rheological properties of the PET fiber masterbatch are not significantly effected, still showing shear thinning characteristics when the amount of addition reaches 10%. The ZnO/TM composite disperses well in the interior and surface of the ZnO/TM/PET fiber matrix. The prepared ZnO/TM/PET fiber has excellent properties, such as fineness of 1.54 dtex, glass transition temperature of 122.4 °C, fracture strength of 3.31 cN/dtex, and negative ion release of 1640/cm3, which shows great industrialization potential.