Jingjing Liao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Jingjing Liao has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
Jun Wu
State Key Laboratory of Advanced Nuclear Energy Technology, Nuclear Power Institute of China, Chengdu, 610213, PR China
2 shared publicationsShaoyu Qiu
State Key Laboratory of Advanced Nuclear Energy Technology, Nuclear Power Institute of China, Chengdu, 610213, PR China
2 shared publicationsWei Zhang
State Key Laboratory of Advanced Nuclear Energy Technology, Nuclear Power Institute of China, Chengdu, 610213, PR China
2 shared publicationsFei Xu
1 shared publicationHongying Sun
Anyang Institute of Technology
1 shared publicationHui Wang
Chengdu University
1 shared publication
Latest Publications
- Open Access
- 9 September 2026
- Published by Elsevier in SSRN Electronic Journal
A Distinct Slip-Oxidation Mechanism for Stress Corrosion Cracking in a Zr–Sn–Nb Alloy in PWR Primary Water: The Decoupled Roles of Oxidation Kinetics and Hydrogen Uptake
The stress corrosion cracking (SCC) behavior of a Zr–Sn–Nb alloy in simulated PWR primary water was systematically investigated as a function of dissolved oxygen (DO, ~10–500 ppb), dissolved hydrogen (DH, 0–50 cc STP H2/kg H2O), and pre-hydrogenation (~640 ppm H). Crack growth rates, crack-tip oxide thickness, hydride fraction, and local plasticity were characterized by DCPD, TEM, and TKD. The SCC propagation rate is largely insensitive to DO, whereas DH exerts a clear retarding effect, reducing the rate by a factor of 2 to 5. Pre-hydrogenation slightly accelerates cracking, an effect attributed not to altered oxidation kinetics, since oxide thickness and hydride fraction remain essentially unchanged, but to enhanced oxide film rupture promoted by solute hydrogen via the HELP mechanism. This hydrogen-induced effect primarily lowers the threshold stress intensity factor for crack propagation, while its influence on the subsequent growth rate is marginal. Crack-tip oxidation is governed predominantly by the direct Zr–H2O reaction, with DO/DH-mediated cathodic reactions playing only a subordinate role. These findings reveal that oxidation kinetics and hydrogen uptake are decoupled in governing SCC propagation: oxidation kinetics control the rate of film regrowth, whereas hydrogen uptake modulates the plasticity-dependent film rupture process through the competing effects of solute hydrogen and hydrides. A distinct slip-oxidation mechanism is thus established for zirconium alloys in high-temperature water, fundamentally different from the water-chemistry-controlled behavior of stainless steels. This mechanistic distinction provides a new basis for evaluating SCC susceptibility in zirconium-based fuel cladding under extended service conditions.
- 9 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessA Distinct Slip-Oxidation Mechanism for Stress Corrosion Cracking in a Zr–Sn–Nb Alloy in PWR Primary Water: The Decoupled Roles of Oxidation Kinetics and Hydrogen Uptake
The stress corrosion cracking (SCC) behavior of a Zr–Sn–Nb alloy in simulated PWR primary water was systematically investigated as a function of dissolved oxygen (DO, ~10–500 ppb), dissolved hydrogen (DH, 0–50 cc STP H2/kg H2O), and pre-hydrogenation (~640 ppm H). Crack growth rates, crack-tip oxide thickness, hydride fraction, and local plasticity were characterized by DCPD, TEM, and TKD. The SCC propagation rate is largely insensitive to DO, whereas DH exerts a clear retarding effect, reducing the rate by a factor of 2 to 5. Pre-hydrogenation slightly accelerates cracking, an effect attributed not to altered oxidation kinetics, since oxide thickness and hydride fraction remain essentially unchanged, but to enhanced oxide film rupture promoted by solute hydrogen via the HELP mechanism. This hydrogen-induced effect primarily lowers the threshold stress intensity factor for crack propagation, while its influence on the subsequent growth rate is marginal. Crack-tip oxidation is governed predominantly by the direct Zr–H2O reaction, with DO/DH-mediated cathodic reactions playing only a subordinate role. These findings reveal that oxidation kinetics and hydrogen uptake are decoupled in governing SCC propagation: oxidation kinetics control the rate of film regrowth, whereas hydrogen uptake modulates the plasticity-dependent film rupture process through the competing effects of solute hydrogen and hydrides. A distinct slip-oxidation mechanism is thus established for zirconium alloys in high-temperature water, fundamentally different from the water-chemistry-controlled behavior of stainless steels. This mechanistic distinction provides a new basis for evaluating SCC susceptibility in zirconium-based fuel cladding under extended service conditions.
- 14 April 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (14) , 20914-20922
Oxidation behaviour of interlocking SiC–Si coating for graphite prepared by preoxidation and gaseous silicon infiltration process
- 14 April 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (14) , 20914-20922
Oxidation behaviour of interlocking SiC–Si coating for graphite prepared by preoxidation and gaseous silicon infiltration process
- Open Access
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Addition of Niobium in Fe-13cr-4.5al-2mo Alloy Used as Atf Cladding: Effect on High Temperature Water Corrosion and In-Situ Electrochemistry
Niobium addition in candidate accident tolerant fuel (ATF) cladding FeCrAl alloy has received much attention, but its effect on high temperature water corrosion behavior has not been revealed. Four alloys with different Nb content (0wt%, 0.5wt%, 1.0wt% and 1.5wt%) based on Fe-13Cr-4.5Al-2Mo model alloy were designed, and the corrosion behavior was investigated by in-situ electrochemistry and microscopy. The in-situ electrochemistry analyses were carried out in 360℃/19.0MPa lithiated and borated water connected with a loop system to monitor the water chemistry. Detailed studies on the oxide film formed after exposure for 85 days were conducted by focused ion bombarding and transmission electron microscopy. FeCrAl alloys have satisfactory corrosion resistance because of small corrosion currents and thin oxide films. Only monolayer multicrystal spinel oxide forms on alloy surface. Slight Nb addition (0.5% and 1.0wt%) benefits the corrosion resistance due to relatively large impedance of oxide and delayed oxidation of Fe 2 Nb particles. Porosities with Fe depletion are spotted in oxide and especially severe in 1.5wt%-Nb alloy. Cathodic Tafel kinetics and corrosion mechanisms of FeCrAl are further discussed.
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessAddition of Niobium in Fe-13cr-4.5al-2mo Alloy Used as Atf Cladding: Effect on High Temperature Water Corrosion and In-Situ Electrochemistry
Niobium addition in candidate accident tolerant fuel (ATF) cladding FeCrAl alloy has received much attention, but its effect on high temperature water corrosion behavior has not been revealed. Four alloys with different Nb content (0wt%, 0.5wt%, 1.0wt% and 1.5wt%) based on Fe-13Cr-4.5Al-2Mo model alloy were designed, and the corrosion behavior was investigated by in-situ electrochemistry and microscopy. The in-situ electrochemistry analyses were carried out in 360℃/19.0MPa lithiated and borated water connected with a loop system to monitor the water chemistry. Detailed studies on the oxide film formed after exposure for 85 days were conducted by focused ion bombarding and transmission electron microscopy. FeCrAl alloys have satisfactory corrosion resistance because of small corrosion currents and thin oxide films. Only monolayer multicrystal spinel oxide forms on alloy surface. Slight Nb addition (0.5% and 1.0wt%) benefits the corrosion resistance due to relatively large impedance of oxide and delayed oxidation of Fe 2 Nb particles. Porosities with Fe depletion are spotted in oxide and especially severe in 1.5wt%-Nb alloy. Cathodic Tafel kinetics and corrosion mechanisms of FeCrAl are further discussed.
- Open Access
- 1 September 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (9) , 096515
Microstructure and twin behavior of Ti-2Al-2.5Zr during cold pilgering
The microstructure and twin behavior of Ti-2Al-2.5Zr tube during cold pilgering were investigated. During the deformation, the intragranular deformation is not uniform, and the microstructure characteristics are similar to low-cycle shear fatigue. Under alternating stress, the rotation tendency of grain is mainly related to the ratio of circumferential to radial strain. As the mainly primary twin, tensile {10–12}〈10–11〉 is activated in large number, which selection of twinning variant conforms to the Schmidt factor law. However, the selection of the secondary twinning variant is related to the slip system activated by the adjacent grains to accommodate the shear strain caused by the twins. The Schmidt factor of the secondary twin is determined by the slip system opened by the adjacent grains.
- 1 September 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (9) , 096515
Open AccessMicrostructure and twin behavior of Ti-2Al-2.5Zr during cold pilgering
The microstructure and twin behavior of Ti-2Al-2.5Zr tube during cold pilgering were investigated. During the deformation, the intragranular deformation is not uniform, and the microstructure characteristics are similar to low-cycle shear fatigue. Under alternating stress, the rotation tendency of grain is mainly related to the ratio of circumferential to radial strain. As the mainly primary twin, tensile {10–12}〈10–11〉 is activated in large number, which selection of twinning variant conforms to the Schmidt factor law. However, the selection of the secondary twinning variant is related to the slip system activated by the adjacent grains to accommodate the shear strain caused by the twins. The Schmidt factor of the secondary twin is determined by the slip system opened by the adjacent grains.