Ming Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ming Li has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Manping Liao
The Civil Engineering Group Corporation of China Second Engineering Bureau Ltd., Beijing 101100, China
2 shared publications - Mei-Ling Zhuang
School of Transportation and Civil Engineering, Nantong University, Nantong 226019, China
2 shared publications - Xiaochuan Hu
The Civil Engineering Group Corporation of China Second Engineering Bureau Ltd., Beijing 101100, China
2 shared publications - Cun Lu
State Key Laboratory of High Performance Civil Engineering Materials, Jiangsu Research Institute of Building Science Co., Ltd., Nanjing 210008, China
1 shared publication - Fuqiang Wang
Harbin Institute of Technology
1 shared publication - Lei Liu
The Civil Engineering Group Corporation of China Second Engineering Bureau Ltd., Beijing 101100, China
1 shared publication
Latest Publications
- Open Access
Experimental Investigations on the On-Site Crack Control of Pier Concrete in High-Altitude Environments
Concrete structures in high-altitude environments face many challenges. Establishing concrete crack control methods in high-altitude environments is crucial for enhancing the service capacity of concrete structures. In this study, a multi-field (hydration-temperature–humidity-constraint) coupling model was used to quantitatively assess the cracking risk of pier bodies at high altitude. On-site crack control tests were conducted on pier bodies using a micro-expansion anti-cracking agent to demonstrate the effectiveness of deformation shrinkage compensation in crack control at high altitudes. The results indicated that there was a risk of cracking in the pier body at high-altitude conditions, especially within 0.3 m from the pile cap and ±2.5 m from the center of the pier side surface. Compared with conventional piers, the micro-expansion anti-cracking agent approximately doubled the unit expansion deflection of piers at high temperatures while reducing the unit shrinkage deflection of piers by 11% to 12% at low temperatures. The concrete in conventional pier bodies was in a tension state after long-term hardening, while the concrete treated with the micro-expansive anti-cracking agent was in compression. Therefore, the deformation compensation effect of the micro-expansive anti-cracking agent was significant and reduced the risk of concrete cracking. In addition, early freezing had a significant impact on concrete strength, underscoring the importance of effective temperature control during the early stages of concrete placement in high-altitude environments.
Open AccessExperimental Investigations on the On-Site Crack Control of Pier Concrete in High-Altitude Environments
Concrete structures in high-altitude environments face many challenges. Establishing concrete crack control methods in high-altitude environments is crucial for enhancing the service capacity of concrete structures. In this study, a multi-field (hydration-temperature–humidity-constraint) coupling model was used to quantitatively assess the cracking risk of pier bodies at high altitude. On-site crack control tests were conducted on pier bodies using a micro-expansion anti-cracking agent to demonstrate the effectiveness of deformation shrinkage compensation in crack control at high altitudes. The results indicated that there was a risk of cracking in the pier body at high-altitude conditions, especially within 0.3 m from the pile cap and ±2.5 m from the center of the pier side surface. Compared with conventional piers, the micro-expansion anti-cracking agent approximately doubled the unit expansion deflection of piers at high temperatures while reducing the unit shrinkage deflection of piers by 11% to 12% at low temperatures. The concrete in conventional pier bodies was in a tension state after long-term hardening, while the concrete treated with the micro-expansive anti-cracking agent was in compression. Therefore, the deformation compensation effect of the micro-expansive anti-cracking agent was significant and reduced the risk of concrete cracking. In addition, early freezing had a significant impact on concrete strength, underscoring the importance of effective temperature control during the early stages of concrete placement in high-altitude environments.
- Open Access
Investigations on the Environmental Characteristics and Cracking Control of Plateau Concrete
In the present study, first, the environmental challenges and cracking characteristics during the construction of plateau concrete on the Sichuan–Tibet route were revealed. Then, using a multi-field coupled shrinkage model with hydration temperature humidity constraints, the early and long-term cracking risks in the core of plateau pier bodies were investigated. Later, the effects of tensile strength, pouring interval age and adiabatic temperature rise on the cracking risk were analyzed. Finally, various control measures for high-altitude concrete cracking were proposed. The results indicated that the complex environment of the plateau led to different forms of cracks in the pier body, especially vertical cracks in the straight sections. The long-term risk of core cracking in the plateau pier body is significantly greater than the risk of early cracking. This risk was strongly influenced by factors such as the concrete tensile strength, pouring interval age and adiabatic temperature rise, which should be given more attention. Deformation compensation can significantly enhance the peak and residual deformation capacities of plateau concrete, with peak values greater than 900 με and residual deformation greater than 200 με at day 60, as well as its resistance to cracking. Strategies such as adopting radiant cooling techniques, improving construction techniques and implementing effective management measures can all play a vital role in improving the cracking resistance of highland concrete.
Open AccessInvestigations on the Environmental Characteristics and Cracking Control of Plateau Concrete
In the present study, first, the environmental challenges and cracking characteristics during the construction of plateau concrete on the Sichuan–Tibet route were revealed. Then, using a multi-field coupled shrinkage model with hydration temperature humidity constraints, the early and long-term cracking risks in the core of plateau pier bodies were investigated. Later, the effects of tensile strength, pouring interval age and adiabatic temperature rise on the cracking risk were analyzed. Finally, various control measures for high-altitude concrete cracking were proposed. The results indicated that the complex environment of the plateau led to different forms of cracks in the pier body, especially vertical cracks in the straight sections. The long-term risk of core cracking in the plateau pier body is significantly greater than the risk of early cracking. This risk was strongly influenced by factors such as the concrete tensile strength, pouring interval age and adiabatic temperature rise, which should be given more attention. Deformation compensation can significantly enhance the peak and residual deformation capacities of plateau concrete, with peak values greater than 900 με and residual deformation greater than 200 με at day 60, as well as its resistance to cracking. Strategies such as adopting radiant cooling techniques, improving construction techniques and implementing effective management measures can all play a vital role in improving the cracking resistance of highland concrete.