Xiu-Cheng Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Xiu-Cheng Zhang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Xue-Fei Chen
Department of Architecture and Civil Engineering, City University of Hong Kong, 83 Tat Chee Avenue, Kowloon Tong, Hong Kong 999077, China
16 shared publications - Ying Peng
School of Civil Engineering, Putian University, Putian 351100, China
5 shared publications - Cheng-Gong Lu
School of Civil Engineering and Transportation, Guangzhou University, Guangzhou 510006, China
3 shared publications - Guo-Hui Yan
Jinxi Holding Group Co., Ltd., Putian 351100, China
2 shared publications - Hai-Sheng Huang
School of Civil Engineering, Putian University, Putian 351100, China
2 shared publications - Jian-Sheng Zheng
Fujian Zhongyong Construction Engineering Co., Ltd., Putian 351100, China
2 shared publications
Latest Publications
- Open Access
Age-Dependent Effects of Graphene Oxide on Hydration-Gel Evolution and Strength Development of Fly Ash-Blended Cementitious Materials
Fly ash is an effective supplementary cementitious material for reducing clinker consumption and carbon emissions, but its low early reactivity often results in delayed hydration and insufficient early-age strength. This study investigated the age-dependent role of graphene oxide (GO) in fly ash-blended cementitious materials by combining compressive strength testing with X-ray diffraction (XRD), thermogravimetric analysis (TG-DTG), 29Si magic-angle spinning nuclear magnetic resonance (29Si MAS NMR), and scanning electron microscopy coupled with energy-dispersive spectroscopy (SEM-EDS). Fly ash replacement levels of 10%, 20%, and 30% were considered, and 0.07% GO was introduced to evaluate its effect at 3, 7, and 28 days. The results showed that fly ash reduced the 3-day compressive strength, whereas the strength differences became much smaller at 28 days. GO enhanced the compressive strength of all fly ash-blended mixtures. XRD and TG-DTG results showed that GO refined Ca(OH)2 crystallization and reduced the retained CH content, indicating more effective CH utilization during hydration and pozzolanic reaction. At 28 days, the incorporation of 0.07% GO increased the compressive strength of the 30% fly ash mixture from 47.38 MPa to 56.58 MPa, while reducing the total CH content from 14.20% to 12.89%, indicating enhanced CH utilization and gel development. 29Si MAS NMR further demonstrated that GO promoted a more mature and polymerized silicate gel structure, as evidenced by lower Q0 fractions, higher mean chain length, and higher proportions of more polymerized silicate species. SEM-EDS observations confirmed that GO led to a denser matrix, less dominant coarse CH, and lower Ca/Si and Ca/(Si + Al) ratios. Overall, GO improved the mechanical performance of fly ash-blended cementitious materials through coupled regulation of hydration products, silicate gel polymerization, and matrix densification.
Open AccessAge-Dependent Effects of Graphene Oxide on Hydration-Gel Evolution and Strength Development of Fly Ash-Blended Cementitious Materials
Fly ash is an effective supplementary cementitious material for reducing clinker consumption and carbon emissions, but its low early reactivity often results in delayed hydration and insufficient early-age strength. This study investigated the age-dependent role of graphene oxide (GO) in fly ash-blended cementitious materials by combining compressive strength testing with X-ray diffraction (XRD), thermogravimetric analysis (TG-DTG), 29Si magic-angle spinning nuclear magnetic resonance (29Si MAS NMR), and scanning electron microscopy coupled with energy-dispersive spectroscopy (SEM-EDS). Fly ash replacement levels of 10%, 20%, and 30% were considered, and 0.07% GO was introduced to evaluate its effect at 3, 7, and 28 days. The results showed that fly ash reduced the 3-day compressive strength, whereas the strength differences became much smaller at 28 days. GO enhanced the compressive strength of all fly ash-blended mixtures. XRD and TG-DTG results showed that GO refined Ca(OH)2 crystallization and reduced the retained CH content, indicating more effective CH utilization during hydration and pozzolanic reaction. At 28 days, the incorporation of 0.07% GO increased the compressive strength of the 30% fly ash mixture from 47.38 MPa to 56.58 MPa, while reducing the total CH content from 14.20% to 12.89%, indicating enhanced CH utilization and gel development. 29Si MAS NMR further demonstrated that GO promoted a more mature and polymerized silicate gel structure, as evidenced by lower Q0 fractions, higher mean chain length, and higher proportions of more polymerized silicate species. SEM-EDS observations confirmed that GO led to a denser matrix, less dominant coarse CH, and lower Ca/Si and Ca/(Si + Al) ratios. Overall, GO improved the mechanical performance of fly ash-blended cementitious materials through coupled regulation of hydration products, silicate gel polymerization, and matrix densification.
- Open Access
- 26 March 2026
- Published by MDPI AG in Fractal and Fractional
- Vol. 10 (4) , 219
Time-Dependent Porosity–Fractal Coupling and Brittleness Evolution in Cementitious Materials with Slag Dosage Variation: From Pore Geometry to Strength
Understanding how pore-system geometry governs mechanical performance remains essential for designing slag-blended cementitious materials. This study investigates the time-dependent coupling between porosity P and fractal dimension D and its implications for strength development and brittleness evolution in cementitious materials with slag dosage variation (0–40%). Compressive strength (f_c), flexural strength (f_f), the compressive-to-flexural strength ratio (f_c/f_f, used as a practical brittleness proxy), porosity (%), fractal dimension, and low-field nuclear magnetic resonance (LF-NMR) permeability (k, mD) were evaluated at 3, 7, and 28 days. Results reveal a pronounced age dependence in microstructure–property relationships. At 28 days, increasing slag dosage led to monotonic pore refinement and geometric reorganization, evidenced by reduced porosity (4.84% → 3.88%), increased fractal dimension (2.754 → 2.820), and decreased permeability (0.00025 → 0.00011 mD), accompanied by enhanced mechanical performance (47.73 → 49.33 MPa in f_c; 6.34 → 7.11 MPa in f_f) and reduced brittleness (f_c/f_f: 7.53 → 6.94). In contrast, a critical 7-day decoupling was observed: slag mixtures exhibited substantially lower porosity (≈5.42–5.69% vs. 7.07% for the reference) yet lower compressive strength (≈34.81–35.29 MPa vs. 38.65 MPa), indicating that porosity alone is insufficient to interpret early-age compressive capacity. Across ages, permeability and fractal trends highlight the role of pore-network connectivity and geometric complexity in governing transport resistance and fracture-related behavior. Overall, the findings demonstrate that a time-dependent porosity–fractal coupling framework provides a coherent pathway “from pore geometry to strength,” particularly for brittleness-relevant indices where geometric effects are amplified.
- 26 March 2026
- Published by MDPI AG in Fractal and Fractional
- Vol. 10 (4) , 219
Open AccessTime-Dependent Porosity–Fractal Coupling and Brittleness Evolution in Cementitious Materials with Slag Dosage Variation: From Pore Geometry to Strength
Understanding how pore-system geometry governs mechanical performance remains essential for designing slag-blended cementitious materials. This study investigates the time-dependent coupling between porosity P and fractal dimension D and its implications for strength development and brittleness evolution in cementitious materials with slag dosage variation (0–40%). Compressive strength (f_c), flexural strength (f_f), the compressive-to-flexural strength ratio (f_c/f_f, used as a practical brittleness proxy), porosity (%), fractal dimension, and low-field nuclear magnetic resonance (LF-NMR) permeability (k, mD) were evaluated at 3, 7, and 28 days. Results reveal a pronounced age dependence in microstructure–property relationships. At 28 days, increasing slag dosage led to monotonic pore refinement and geometric reorganization, evidenced by reduced porosity (4.84% → 3.88%), increased fractal dimension (2.754 → 2.820), and decreased permeability (0.00025 → 0.00011 mD), accompanied by enhanced mechanical performance (47.73 → 49.33 MPa in f_c; 6.34 → 7.11 MPa in f_f) and reduced brittleness (f_c/f_f: 7.53 → 6.94). In contrast, a critical 7-day decoupling was observed: slag mixtures exhibited substantially lower porosity (≈5.42–5.69% vs. 7.07% for the reference) yet lower compressive strength (≈34.81–35.29 MPa vs. 38.65 MPa), indicating that porosity alone is insufficient to interpret early-age compressive capacity. Across ages, permeability and fractal trends highlight the role of pore-network connectivity and geometric complexity in governing transport resistance and fracture-related behavior. Overall, the findings demonstrate that a time-dependent porosity–fractal coupling framework provides a coherent pathway “from pore geometry to strength,” particularly for brittleness-relevant indices where geometric effects are amplified.
- Open Access
- 28 February 2026
- Published by MDPI AG in Fractal and Fractional
- Vol. 10 (3) , 160
Fractal Geometry–Porosity-Coupled Mathematical Modeling of Mechanical Degradation in Low-Carbon Marine Concrete with High-Volume SCMs Under Sulfate–Chloride–Carbonate–Magnesium Attack
Marine concrete is often exposed to multiple aggressive ions, so mechanical deterioration cannot be reliably interpreted using single-ion durability concepts. This study investigates ocean-oriented concretes incorporating high contents of mineral admixtures under coupled sulfate/chloride/carbonate/magnesium actions and develops a pore-structure-based D–P dual-parameter framework linking microstructural descriptors to macroscopic peak stress and peak strain. Three binder systems were designed: ordinary Portland cement concrete (OPC), cement–silica fume concrete (CSC, 20% silica fume), and cement–silica fume–fly ash concrete (CSFC, 20% silica fume + 50% fly ash). Specimens were immersed for 12 and 24 months in four representative binary-salt solutions. Porosity evolution and pore-size-class distributions were quantified by low-field NMR, while pore complexity was characterized using multi-scale fractal dimensions. The results show that mineral admixtures generally refine the pore system and improve the integrity of fine pores; CSFC exhibits the most robust microstructural stability across the tested environments, whereas CSC shows a pronounced degradation of fine-pore structure under CE4. A second-order response surface model built on Z-score normalized fractal dimension (D) and porosity (P) achieves reliable predictability for peak strain (R2 = 0.85) and peak stress (R2 = 0.79). Global Sobol sensitivity analysis reveals distinct controlling mechanisms: peak strain is predominantly governed by porosity (S_P = 85.9%), whereas peak stress is controlled by the combined effects of porosity, pore complexity, and their interaction (S_P = 42.4%, S_D = 19.8%, S_{D × P} = 37.8%). Local sensitivity mapping further identifies high-sensitivity regimes at extreme pore states, providing mechanistic guidance for mixture optimization. Overall, the proposed D–P framework quantitatively bridges pore volume/geometry evolution and mechanical degradation, offering a practical predictive tool for durability-oriented design of marine concretes under multi-ionic attack.
- 28 February 2026
- Published by MDPI AG in Fractal and Fractional
- Vol. 10 (3) , 160
Open AccessFractal Geometry–Porosity-Coupled Mathematical Modeling of Mechanical Degradation in Low-Carbon Marine Concrete with High-Volume SCMs Under Sulfate–Chloride–Carbonate–Magnesium Attack
Marine concrete is often exposed to multiple aggressive ions, so mechanical deterioration cannot be reliably interpreted using single-ion durability concepts. This study investigates ocean-oriented concretes incorporating high contents of mineral admixtures under coupled sulfate/chloride/carbonate/magnesium actions and develops a pore-structure-based D–P dual-parameter framework linking microstructural descriptors to macroscopic peak stress and peak strain. Three binder systems were designed: ordinary Portland cement concrete (OPC), cement–silica fume concrete (CSC, 20% silica fume), and cement–silica fume–fly ash concrete (CSFC, 20% silica fume + 50% fly ash). Specimens were immersed for 12 and 24 months in four representative binary-salt solutions. Porosity evolution and pore-size-class distributions were quantified by low-field NMR, while pore complexity was characterized using multi-scale fractal dimensions. The results show that mineral admixtures generally refine the pore system and improve the integrity of fine pores; CSFC exhibits the most robust microstructural stability across the tested environments, whereas CSC shows a pronounced degradation of fine-pore structure under CE4. A second-order response surface model built on Z-score normalized fractal dimension (D) and porosity (P) achieves reliable predictability for peak strain (R2 = 0.85) and peak stress (R2 = 0.79). Global Sobol sensitivity analysis reveals distinct controlling mechanisms: peak strain is predominantly governed by porosity (S_P = 85.9%), whereas peak stress is controlled by the combined effects of porosity, pore complexity, and their interaction (S_P = 42.4%, S_D = 19.8%, S_{D × P} = 37.8%). Local sensitivity mapping further identifies high-sensitivity regimes at extreme pore states, providing mechanistic guidance for mixture optimization. Overall, the proposed D–P framework quantitatively bridges pore volume/geometry evolution and mechanical degradation, offering a practical predictive tool for durability-oriented design of marine concretes under multi-ionic attack.
- Open Access
- 29 August 2025
- Published by MDPI AG in Fractal and Fractional
- Vol. 9 (9) , 568
Fractal-Based Non-Linear Assessment of Crack Propagation in Recycled Aggregate Concrete Using 3D Response Surface Methodology
This study investigates the fracture behavior of recycled aggregate concrete by integrating fractal theory and empirical modeling to quantify how recycled coarse aggregates (RCAs) and recycled fine aggregates (RFAs) influence crack complexity and maximum crack width under varying content and loads. The results reveal distinct scale-dependent behaviors between RCA and RFA. For RCA, moderate dosages enhance fractal complexity (a measure of surface roughness) by promoting micro-crack proliferation, while excessive RCA reduces complexity due to matrix homogenization. In contrast, RFA significantly increases both fractal complexity and crack width under equivalent loads, reflecting its susceptibility to micro-scale interfacial transition zone (ITZ) degradation. Non-linear thresholds are identified: RCA’s fractal complexity plateaus at high loads as cracks coalesce into fewer dominant paths, while RFA’s crack width growth decelerates at extreme dosages due to balancing effects like particle packing. Empirical models link aggregate dosage and load to fractal dimension and crack width with high predictive accuracy (R2 > 0.85), capturing interaction effects such as RCA’s load-induced complexity reduction and RFA’s load-driven crack width amplification. Secondary analyses further demonstrate that fractal dimension correlates with crack width through non-linear relationships, emphasizing the coupled nature of micro- and macro-scale damage. These findings challenge conventional design assumptions by differentiating the impacts of RCA (macro-crack coalescence) and RFA (micro-crack proliferation), providing actionable thresholds for optimizing mix designs. The study also advances sustainable material design by offering a scientific basis for updating standards to accommodate higher recycled aggregate percentages, supporting circular economy goals through reduced carbon emissions and waste diversion, and laying the groundwork for resilient, low-carbon infrastructure.
- 29 August 2025
- Published by MDPI AG in Fractal and Fractional
- Vol. 9 (9) , 568
Open AccessFractal-Based Non-Linear Assessment of Crack Propagation in Recycled Aggregate Concrete Using 3D Response Surface Methodology
This study investigates the fracture behavior of recycled aggregate concrete by integrating fractal theory and empirical modeling to quantify how recycled coarse aggregates (RCAs) and recycled fine aggregates (RFAs) influence crack complexity and maximum crack width under varying content and loads. The results reveal distinct scale-dependent behaviors between RCA and RFA. For RCA, moderate dosages enhance fractal complexity (a measure of surface roughness) by promoting micro-crack proliferation, while excessive RCA reduces complexity due to matrix homogenization. In contrast, RFA significantly increases both fractal complexity and crack width under equivalent loads, reflecting its susceptibility to micro-scale interfacial transition zone (ITZ) degradation. Non-linear thresholds are identified: RCA’s fractal complexity plateaus at high loads as cracks coalesce into fewer dominant paths, while RFA’s crack width growth decelerates at extreme dosages due to balancing effects like particle packing. Empirical models link aggregate dosage and load to fractal dimension and crack width with high predictive accuracy (R2 > 0.85), capturing interaction effects such as RCA’s load-induced complexity reduction and RFA’s load-driven crack width amplification. Secondary analyses further demonstrate that fractal dimension correlates with crack width through non-linear relationships, emphasizing the coupled nature of micro- and macro-scale damage. These findings challenge conventional design assumptions by differentiating the impacts of RCA (macro-crack coalescence) and RFA (micro-crack proliferation), providing actionable thresholds for optimizing mix designs. The study also advances sustainable material design by offering a scientific basis for updating standards to accommodate higher recycled aggregate percentages, supporting circular economy goals through reduced carbon emissions and waste diversion, and laying the groundwork for resilient, low-carbon infrastructure.
- Open Access
- 11 July 2025
- Published by MDPI AG in Fractal and Fractional
- Vol. 9 (7) , 454
Quantitative Fractal Analysis of Fracture Mechanics and Damage Evolution in Recycled Aggregate Concrete Beams: Investigation of Dosage-Dependent Mechanical Response Under Incremental Load
This study investigated the fracture behavior of concrete beams with recycled coarse aggregate (RCA) and recycled fine aggregate (RFA) using the box-counting method to measure crack fractal dimensions under load. Beams with RCA showed higher fractal dimensions due to RCA’s lower elastic moduli and compressive strengths, resulting in reduced deformation resistance, ductility, and more late-stage crack propagation. A direct proportional relationship existed between RCA/RFA replacement ratios and crack fractal dimensions. Second-order and third-order polynomial trend surface-fitting techniques were applied to examine the complex relationships among RFA/RCA dosage, applied load, and crack fractal dimension. The results indicated that the RFA dosage had a negative quadratic influence, while load had a positive linear effect, with dosage impact increasing with load. A second-order functional relationship was found between mid-span deflection and crack fractal dimension, reflecting nonlinear behavior consistent with concrete mechanics. This study enhances the understanding of recycled aggregate concrete beam fracture behavior, with the crack fractal dimension serving as a valuable quantitative indicator for damage state and crack complexity assessment. These findings are crucial for engineering design and application, enabling better evaluation of structural performance under various conditions.
- 11 July 2025
- Published by MDPI AG in Fractal and Fractional
- Vol. 9 (7) , 454
Open AccessQuantitative Fractal Analysis of Fracture Mechanics and Damage Evolution in Recycled Aggregate Concrete Beams: Investigation of Dosage-Dependent Mechanical Response Under Incremental Load
This study investigated the fracture behavior of concrete beams with recycled coarse aggregate (RCA) and recycled fine aggregate (RFA) using the box-counting method to measure crack fractal dimensions under load. Beams with RCA showed higher fractal dimensions due to RCA’s lower elastic moduli and compressive strengths, resulting in reduced deformation resistance, ductility, and more late-stage crack propagation. A direct proportional relationship existed between RCA/RFA replacement ratios and crack fractal dimensions. Second-order and third-order polynomial trend surface-fitting techniques were applied to examine the complex relationships among RFA/RCA dosage, applied load, and crack fractal dimension. The results indicated that the RFA dosage had a negative quadratic influence, while load had a positive linear effect, with dosage impact increasing with load. A second-order functional relationship was found between mid-span deflection and crack fractal dimension, reflecting nonlinear behavior consistent with concrete mechanics. This study enhances the understanding of recycled aggregate concrete beam fracture behavior, with the crack fractal dimension serving as a valuable quantitative indicator for damage state and crack complexity assessment. These findings are crucial for engineering design and application, enabling better evaluation of structural performance under various conditions.
- Open Access
Eco-Efficient Mortars with High-Content Construction, Waste-Derived Aggregates Functionalized via Nano-TiO2 for NOx Abatement
This study elucidates the photocatalytic NOx abatement efficacy of eco-efficient mortars incorporating construction waste-derived aggregates functionalized with nano-TiO2. The research findings demonstrate a positive correlation between NOx abatement efficiency and nano-TiO2 substitution ratio, with recycled glass sand (RG)-based panels exhibiting superior performance compared to standard sand and recycled clay brick sand (RCBS)-based counterparts. The employment of ultrasonic dispersion as a nano-TiO2 incorporation method yields enhanced abatement efficiency relative to direct mixing, attributable to improved photocatalyst dispersion and surface area accessibility. The loading capacity of nano-TiO2 on recycled aggregates is observed to be positively influenced by the concentration of nano-TiO2 solution, with recycled clay brick sand demonstrating the highest loading capacity. RG-RCBS panels are shown to exhibit higher NOx abatement efficiency than standard sand (SS)-RCBS panels, with an optimal substitution ratio of 40% glass sand identified for maximizing abatement efficacy in RG-RCBS systems. A decline in NOx abatement efficiency is observed with increasing NOx flow rate and concentration, attributable to reduced pollutant residence time and excess pollutant load exceeding the panels’ processing capacity. Prolonged curing time also results in diminished abatement efficiency, due to microstructural alterations within the mortar matrix and the accumulation of photocatalytic reaction byproducts. Collectively, these findings underscore the potential of recycled aggregate-based mortars, in conjunction with nano-TiO2, as a viable eco-efficient strategy for NOx abatement, highlighting the critical influence of material selection, photocatalyst loading, and operational parameters on system performance.
Open AccessEco-Efficient Mortars with High-Content Construction, Waste-Derived Aggregates Functionalized via Nano-TiO2 for NOx Abatement
This study elucidates the photocatalytic NOx abatement efficacy of eco-efficient mortars incorporating construction waste-derived aggregates functionalized with nano-TiO2. The research findings demonstrate a positive correlation between NOx abatement efficiency and nano-TiO2 substitution ratio, with recycled glass sand (RG)-based panels exhibiting superior performance compared to standard sand and recycled clay brick sand (RCBS)-based counterparts. The employment of ultrasonic dispersion as a nano-TiO2 incorporation method yields enhanced abatement efficiency relative to direct mixing, attributable to improved photocatalyst dispersion and surface area accessibility. The loading capacity of nano-TiO2 on recycled aggregates is observed to be positively influenced by the concentration of nano-TiO2 solution, with recycled clay brick sand demonstrating the highest loading capacity. RG-RCBS panels are shown to exhibit higher NOx abatement efficiency than standard sand (SS)-RCBS panels, with an optimal substitution ratio of 40% glass sand identified for maximizing abatement efficacy in RG-RCBS systems. A decline in NOx abatement efficiency is observed with increasing NOx flow rate and concentration, attributable to reduced pollutant residence time and excess pollutant load exceeding the panels’ processing capacity. Prolonged curing time also results in diminished abatement efficiency, due to microstructural alterations within the mortar matrix and the accumulation of photocatalytic reaction byproducts. Collectively, these findings underscore the potential of recycled aggregate-based mortars, in conjunction with nano-TiO2, as a viable eco-efficient strategy for NOx abatement, highlighting the critical influence of material selection, photocatalyst loading, and operational parameters on system performance.
- Open Access
Recycled Clay Brick Powder as a Dual-Function Additive: Mitigating the Alkali–Silica Reaction (ASR) and Enhancing Strength in Eco-Friendly Mortar with Hybrid Waste Glass and Clay Brick Aggregates
The construction industry’s escalating environmental footprint, coupled with the underutilization of construction waste streams, necessitates innovative approaches to sustainable material design. This study investigates the dual functionality of recycled clay brick powder (RCBP) as both a supplementary cementitious material (SCM) and an alkali–silica reaction (ASR) inhibitor in hybrid mortar systems incorporating recycled glass (RG) and recycled clay brick (RCB) aggregates. Leveraging the pozzolanic activity of RCBP’s residual aluminosilicate phases, the research quantifies its influence on mortar durability and mechanical performance under varying substitution scenarios. Experimental findings reveal a nonlinear relationship between RCBP dosage and mortar properties. A 30% cement replacement with RCBP yields a 28-day activity index of 96.95%, confirming significant pozzolanic contributions. Critically, RCBP substitution ≥20% effectively mitigates ASRs induced by RG aggregates, with optimal suppression observed at 25% replacement. This threshold aligns with microstructural analyses showing RCBP’s Al3+ ions preferentially reacting with alkali hydroxides to form non-expansive gels, reducing pore solution pH and silica dissolution rates. Mechanical characterization reveals trade-offs between workability and strength development. Increasing RCBP substitution decreases mortar consistency and fluidity, which is more pronounced in RG-RCBS blends due to glass aggregates’ smooth texture. Compressively, both SS-RCBS and RG-RCBS mortars exhibit strength reduction with higher RCBP content, yet all specimens show accelerated compressive strength gain relative to flexural strength over curing time. Notably, 28-day water absorption increases with RCBP substitution, correlating with microstructural porosity modifications. These findings position recycled construction wastes and glass as valuable resources in circular economy frameworks, offering municipalities a pathway to meet recycled content mandates without sacrificing structural integrity. The study underscores the importance of waste synergy in advancing sustainable mortar technology, with implications for net-zero building practices and industrial waste valorization.
Open AccessRecycled Clay Brick Powder as a Dual-Function Additive: Mitigating the Alkali–Silica Reaction (ASR) and Enhancing Strength in Eco-Friendly Mortar with Hybrid Waste Glass and Clay Brick Aggregates
The construction industry’s escalating environmental footprint, coupled with the underutilization of construction waste streams, necessitates innovative approaches to sustainable material design. This study investigates the dual functionality of recycled clay brick powder (RCBP) as both a supplementary cementitious material (SCM) and an alkali–silica reaction (ASR) inhibitor in hybrid mortar systems incorporating recycled glass (RG) and recycled clay brick (RCB) aggregates. Leveraging the pozzolanic activity of RCBP’s residual aluminosilicate phases, the research quantifies its influence on mortar durability and mechanical performance under varying substitution scenarios. Experimental findings reveal a nonlinear relationship between RCBP dosage and mortar properties. A 30% cement replacement with RCBP yields a 28-day activity index of 96.95%, confirming significant pozzolanic contributions. Critically, RCBP substitution ≥20% effectively mitigates ASRs induced by RG aggregates, with optimal suppression observed at 25% replacement. This threshold aligns with microstructural analyses showing RCBP’s Al3+ ions preferentially reacting with alkali hydroxides to form non-expansive gels, reducing pore solution pH and silica dissolution rates. Mechanical characterization reveals trade-offs between workability and strength development. Increasing RCBP substitution decreases mortar consistency and fluidity, which is more pronounced in RG-RCBS blends due to glass aggregates’ smooth texture. Compressively, both SS-RCBS and RG-RCBS mortars exhibit strength reduction with higher RCBP content, yet all specimens show accelerated compressive strength gain relative to flexural strength over curing time. Notably, 28-day water absorption increases with RCBP substitution, correlating with microstructural porosity modifications. These findings position recycled construction wastes and glass as valuable resources in circular economy frameworks, offering municipalities a pathway to meet recycled content mandates without sacrificing structural integrity. The study underscores the importance of waste synergy in advancing sustainable mortar technology, with implications for net-zero building practices and industrial waste valorization.
- Open Access
Synergistic Enhancement of Physicomechanical Performance and Microstructural Integrity in Hydrothermally Synthesized Autoclaved Lightweight Aggregates Through Quicklime–Fly Ash Blends
Herein, fly ash aggregates (FAAs) were synthesized through a hydrothermal process, utilizing fly ash (FA) and quicklime at a temperature of 180 °C under saturated steam conditions. The study focused on analyzing the ramifications of varying quicklime content on the physicomechanical attributes of the resultant FAAs. A comprehensive examination of mineralogical composition, microstructure, insoluble matter content, and loss on ignition was conducted to elucidate the mechanisms through which quicklime influences the cylinder compressive strength of the FAAs. An observed trend indicated that as the quicklime content increased, the water requirement during the granulation process also increased. Consequently, there was a gradual augmentation in the water absorption capacity of the FAAs, accompanied by a progressive decrement in their apparent density. The augmentation in the filling effect, attributed to the hydration products, led to a steady rise in cylinder compressive strength as the quicklime content escalated from 5 wt.% to 25 wt.%. However, beyond this threshold, between 25 wt.% and 45 wt.%, a decrement in cylinder compressive strength was noted due to the deterioration of the micro-aggregate effect. The interplay between the filling effect and the micro-aggregate effect resulted in the cylinder compressive strength of the FAAs peaking at 13 MPa at a quicklime content of 25 wt.%. The overarching objective of this research is to propose an efficacious approach for mitigating solid waste, with a particular emphasis on reducing the burden of FA. This study provides insights into optimizing FAAs through the modulation of quicklime content, thereby fostering advancements in waste management and resource recovery.
Open AccessSynergistic Enhancement of Physicomechanical Performance and Microstructural Integrity in Hydrothermally Synthesized Autoclaved Lightweight Aggregates Through Quicklime–Fly Ash Blends
Herein, fly ash aggregates (FAAs) were synthesized through a hydrothermal process, utilizing fly ash (FA) and quicklime at a temperature of 180 °C under saturated steam conditions. The study focused on analyzing the ramifications of varying quicklime content on the physicomechanical attributes of the resultant FAAs. A comprehensive examination of mineralogical composition, microstructure, insoluble matter content, and loss on ignition was conducted to elucidate the mechanisms through which quicklime influences the cylinder compressive strength of the FAAs. An observed trend indicated that as the quicklime content increased, the water requirement during the granulation process also increased. Consequently, there was a gradual augmentation in the water absorption capacity of the FAAs, accompanied by a progressive decrement in their apparent density. The augmentation in the filling effect, attributed to the hydration products, led to a steady rise in cylinder compressive strength as the quicklime content escalated from 5 wt.% to 25 wt.%. However, beyond this threshold, between 25 wt.% and 45 wt.%, a decrement in cylinder compressive strength was noted due to the deterioration of the micro-aggregate effect. The interplay between the filling effect and the micro-aggregate effect resulted in the cylinder compressive strength of the FAAs peaking at 13 MPa at a quicklime content of 25 wt.%. The overarching objective of this research is to propose an efficacious approach for mitigating solid waste, with a particular emphasis on reducing the burden of FA. This study provides insights into optimizing FAAs through the modulation of quicklime content, thereby fostering advancements in waste management and resource recovery.
- Open Access
Multi-Scale Investigation of Fly Ash Aggregates (FAAs) in Concrete: From Macroscopic Physical–Mechanical Properties to Microscopic Structure of Hydration Products
Fly ash aggregates (FAAs) were synthesized via a hydrothermal process, involving the reaction of fly ash and cement at 180 °C under saturated steam conditions. A thorough examination was carried out to evaluate the impact of cement content on the physico-mechanical properties of the resulting FAAs. A comprehensive exploration was undertaken to decipher the mechanisms by which cement modulates the cylinder compressive strength of FAAs, encompassing mineralogical composition, microstructure, insoluble residue content, and loss on ignition. As the cement proportion increased, a concomitant rise in the amount of hydration products was observed, leading to an enhanced filling effect. This, subsequently, resulted in reduced water absorption and increased apparent density of the FAAs. The augmented filling effect of hydration products contributed to a gradual elevation in the cylinder compressive strength of FAAs as cement content escalated from 5 to 35 wt%. However, a significant transition occurred when cement content surpassed 35%, reaching 35–45 wt%. Within this range, the micro-aggregate effect was diminished, causing a decrease in cylinder compressive strength. The optimal equilibrium between the filling effect and micro-aggregate effect was attained at 35 wt% cement content, where the cylinder compressive strength of FAAs reached its peak value of 18.5 MPa. This research is expected to provide a feasible approach for solid waste reduction, with a particular emphasis on the utilization of fly ash.
Open AccessMulti-Scale Investigation of Fly Ash Aggregates (FAAs) in Concrete: From Macroscopic Physical–Mechanical Properties to Microscopic Structure of Hydration Products
Fly ash aggregates (FAAs) were synthesized via a hydrothermal process, involving the reaction of fly ash and cement at 180 °C under saturated steam conditions. A thorough examination was carried out to evaluate the impact of cement content on the physico-mechanical properties of the resulting FAAs. A comprehensive exploration was undertaken to decipher the mechanisms by which cement modulates the cylinder compressive strength of FAAs, encompassing mineralogical composition, microstructure, insoluble residue content, and loss on ignition. As the cement proportion increased, a concomitant rise in the amount of hydration products was observed, leading to an enhanced filling effect. This, subsequently, resulted in reduced water absorption and increased apparent density of the FAAs. The augmented filling effect of hydration products contributed to a gradual elevation in the cylinder compressive strength of FAAs as cement content escalated from 5 to 35 wt%. However, a significant transition occurred when cement content surpassed 35%, reaching 35–45 wt%. Within this range, the micro-aggregate effect was diminished, causing a decrease in cylinder compressive strength. The optimal equilibrium between the filling effect and micro-aggregate effect was attained at 35 wt% cement content, where the cylinder compressive strength of FAAs reached its peak value of 18.5 MPa. This research is expected to provide a feasible approach for solid waste reduction, with a particular emphasis on the utilization of fly ash.
- Open Access
Multiscale Investigation of Modified Recycled Aggregate Concrete on Sulfate Attack Resistance
This study investigated the sulfate resistance of modified recycled aggregate concrete (RAC) by applying carbonation and nano-silica soaking methodologies. Recycled concrete aggregates (RCA) derived from concretes of C30 and C60 strength grades were subjected to these modification techniques and subsequently utilized in the fabrication of RAC specimens. The results show notable porosity and crack density within the interfacial transition zone (ITZ) interfacing recycled aggregate and cement paste in recycled aggregate concrete (RAC). Specifically, the porosity within the ITZ of RAC is observed to be up to 30% higher than that of virgin aggregate concrete. These pathways facilitate the penetration of sulfate ions, subsequently inducing deterioration and resulting in a compression strength reduction of up to 40%. While carbonation treatment exhibits a moderate enhancement in sulfate resistance, decreasing the sulfate penetration depth by 15%, the incorporation of 2% nano-silica by weight of cement proves significantly more effective. This addition reduces the sulfate penetration depth by over 30% and lowers the sulfate concentration by 25%. Furthermore, the compressive strength of RAC modified with nano-silica increases by 15% following 28 days of sulfate exposure. Additionally, a 30% reduction in the sulfate ion mass equilibrium depth is observed in nano-silica-modified RAC, accompanied by a markedly lower sulfate concentration in the pore solution. After 56 days of sulfate attack, the compressive strength of nano-silica-modified RAC retains 85% of its initial value, whereas unmodified RAC decreases to 70%. Notably, the quality of recycled aggregate significantly impacts sulfate resistance, with high-strength RCA (exceeding 40 MPa) demonstrating superior resistance compared to low-strength RCA (below 20 MPa). Consequently, RAC produced with high-strength RCA experiences only a 20% loss in compressive strength under sulfate attack, whereas RAC containing low-strength RCA suffers a 40% loss. The novelty of this study is the effective use of nano-silica soaking and carbonation to enhance the sulfate resistance and compressive strength of recycled aggregate concrete originated from both normal and high-strength reference concrete.
Open AccessMultiscale Investigation of Modified Recycled Aggregate Concrete on Sulfate Attack Resistance
This study investigated the sulfate resistance of modified recycled aggregate concrete (RAC) by applying carbonation and nano-silica soaking methodologies. Recycled concrete aggregates (RCA) derived from concretes of C30 and C60 strength grades were subjected to these modification techniques and subsequently utilized in the fabrication of RAC specimens. The results show notable porosity and crack density within the interfacial transition zone (ITZ) interfacing recycled aggregate and cement paste in recycled aggregate concrete (RAC). Specifically, the porosity within the ITZ of RAC is observed to be up to 30% higher than that of virgin aggregate concrete. These pathways facilitate the penetration of sulfate ions, subsequently inducing deterioration and resulting in a compression strength reduction of up to 40%. While carbonation treatment exhibits a moderate enhancement in sulfate resistance, decreasing the sulfate penetration depth by 15%, the incorporation of 2% nano-silica by weight of cement proves significantly more effective. This addition reduces the sulfate penetration depth by over 30% and lowers the sulfate concentration by 25%. Furthermore, the compressive strength of RAC modified with nano-silica increases by 15% following 28 days of sulfate exposure. Additionally, a 30% reduction in the sulfate ion mass equilibrium depth is observed in nano-silica-modified RAC, accompanied by a markedly lower sulfate concentration in the pore solution. After 56 days of sulfate attack, the compressive strength of nano-silica-modified RAC retains 85% of its initial value, whereas unmodified RAC decreases to 70%. Notably, the quality of recycled aggregate significantly impacts sulfate resistance, with high-strength RCA (exceeding 40 MPa) demonstrating superior resistance compared to low-strength RCA (below 20 MPa). Consequently, RAC produced with high-strength RCA experiences only a 20% loss in compressive strength under sulfate attack, whereas RAC containing low-strength RCA suffers a 40% loss. The novelty of this study is the effective use of nano-silica soaking and carbonation to enhance the sulfate resistance and compressive strength of recycled aggregate concrete originated from both normal and high-strength reference concrete.