Narjes Mohsen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Narjes Mohsen has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Fatima Abusua
Department of Prosthodontics, Faculty of Dentistry, University of Tripoli, Tripoli, Libya
2 shared publications - Mohamed Elmaroush
Department of Prosthodontics, Faculty of Dentistry, University of Tripoli, Libya
2 shared publications - Sarra Ben Hamida
Department of Prosthodontics, Faculty of Dentistry, University of Tripoli, Tripoli, Libya
2 shared publications - Zieneb Elgarboae
Department of Prosthodontics, Faculty of Dentistry, University of Tripoli, Tripoli, Libya
1 shared publication
Latest Publications
- Open Access
- 22 September 2025
- Published by Attahadi Medical University
- p. 334-338
Comparative Analysis of Flexural Strength between Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM (PEEK) Denture Base Materials: An In-Vitro Study
This study aimed to compare the flexural strength of Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM Polyether Ether Ketone (PEEK) denture base materials. A total of 36 rectangular samples with dimensions of (64mm x 10 mm x 3.3mm) were fabricated from Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM (PEEK). These samples were divided into three groups of 12 samples. The three-point flexural strength test was carried out using a universal testing machine. A one-way analysis of variance (ANOVA) test was used for statistical analysis. Statistical significance was set at P ≤ 0.05. The flexural strength of CAD/CAM (PEEK) (137.92 ± 8.92555 MPa) was the highest, followed by Heat Polymerized Acrylic Resin (75.162 ± 9.40870 MPa), and the lowest was for Injectable Flexible Nylon-Based Resin (54.01 ± 20.29325 MPa). Considering the study’s limitations, CAD/CAM PEEK showed the highest flexural strength, followed by heat-polymerized PMMA, while injectable flexible nylon-based resin exhibited the lowest strength. These findings suggest that PEEK may provide more durable and reliable denture bases, potentially improving prosthesis longevity and patient satisfaction
- 22 September 2025
- Published by Attahadi Medical University
- p. 334-338
Open AccessComparative Analysis of Flexural Strength between Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM (PEEK) Denture Base Materials: An In-Vitro Study
This study aimed to compare the flexural strength of Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM Polyether Ether Ketone (PEEK) denture base materials. A total of 36 rectangular samples with dimensions of (64mm x 10 mm x 3.3mm) were fabricated from Heat Polymerized PMMA, Injectable Flexible Nylon-Based Resin, and CAD/CAM (PEEK). These samples were divided into three groups of 12 samples. The three-point flexural strength test was carried out using a universal testing machine. A one-way analysis of variance (ANOVA) test was used for statistical analysis. Statistical significance was set at P ≤ 0.05. The flexural strength of CAD/CAM (PEEK) (137.92 ± 8.92555 MPa) was the highest, followed by Heat Polymerized Acrylic Resin (75.162 ± 9.40870 MPa), and the lowest was for Injectable Flexible Nylon-Based Resin (54.01 ± 20.29325 MPa). Considering the study’s limitations, CAD/CAM PEEK showed the highest flexural strength, followed by heat-polymerized PMMA, while injectable flexible nylon-based resin exhibited the lowest strength. These findings suggest that PEEK may provide more durable and reliable denture bases, potentially improving prosthesis longevity and patient satisfaction
- Open Access
- 7 February 2025
- Published by Medical Research Center in AlQalam Journal of Medical and Applied Sciences
- p. 230-235
In Vitro Evaluation of the Fracture Strength among Three Different Denture Base Materials
Failure in the form of denture fracture is commonly encountered by both removable prosthodontics wearers and dentists, it is mainly attributed to material properties, technical features, stresses while in function or due to impact as a consequence of dropping the dentures. Traditionally, Heat-Polymerized Polymethylmethacrylate (PMMA) has been the gold standard for denture bases due to its ease of processing and acceptable mechanical properties. However, newer materials, injectable flexible nylon-based resin and CAD/CAM Polyether ether Ketone (PEEK) denture bases are being introduced with claims of superior strength and durability. The aim of this study was to investigate the fracture strength of three commonly used denture base materials in Libya, which may aid in selecting the best material for a given application and predicting potential material behavior under load when holding the durability of the material in mind. A total of 36 samples were tested. These samples were divided into three groups, with 12 samples each: Group I heat polymerized acrylic resin PMMA, group II Injectable flexible nylon-based resin and group III CAD/CAM (PEEK). The fracture strength test was carried out on a universal testing machine at a crosshead speed of 5 mm/min. The results were analyzed using ANOVA, and multiple comparisons were undertaken using Tukey’s HSD test. Statistical significance was set at P ≤ 0.001. The result of this study shows there were significant differences in the fracture strength among the three groups (P< 0.001). Moreover, CAD/CAM (PEEK) denture base material exhibited significantly the highest fracture strength (234.17N ± 13.5) whereas the least fracture strength value was measured with Injectable flexible nylon-based resin denture base material (75.25N±10.5). The study concluded that, within the limitations of this study, the results demonstrate that CAD/CAM (PEEK) outperforms Injectable flexible nylon-based resin and heat polymerized acrylic denture base materials in terms of the fracture strength, supporting its potential as an advanced material for denture construction. However, further clinical studies are recommended.
- 7 February 2025
- Published by Medical Research Center in AlQalam Journal of Medical and Applied Sciences
- p. 230-235
Open AccessIn Vitro Evaluation of the Fracture Strength among Three Different Denture Base Materials
Failure in the form of denture fracture is commonly encountered by both removable prosthodontics wearers and dentists, it is mainly attributed to material properties, technical features, stresses while in function or due to impact as a consequence of dropping the dentures. Traditionally, Heat-Polymerized Polymethylmethacrylate (PMMA) has been the gold standard for denture bases due to its ease of processing and acceptable mechanical properties. However, newer materials, injectable flexible nylon-based resin and CAD/CAM Polyether ether Ketone (PEEK) denture bases are being introduced with claims of superior strength and durability. The aim of this study was to investigate the fracture strength of three commonly used denture base materials in Libya, which may aid in selecting the best material for a given application and predicting potential material behavior under load when holding the durability of the material in mind. A total of 36 samples were tested. These samples were divided into three groups, with 12 samples each: Group I heat polymerized acrylic resin PMMA, group II Injectable flexible nylon-based resin and group III CAD/CAM (PEEK). The fracture strength test was carried out on a universal testing machine at a crosshead speed of 5 mm/min. The results were analyzed using ANOVA, and multiple comparisons were undertaken using Tukey’s HSD test. Statistical significance was set at P ≤ 0.001. The result of this study shows there were significant differences in the fracture strength among the three groups (P< 0.001). Moreover, CAD/CAM (PEEK) denture base material exhibited significantly the highest fracture strength (234.17N ± 13.5) whereas the least fracture strength value was measured with Injectable flexible nylon-based resin denture base material (75.25N±10.5). The study concluded that, within the limitations of this study, the results demonstrate that CAD/CAM (PEEK) outperforms Injectable flexible nylon-based resin and heat polymerized acrylic denture base materials in terms of the fracture strength, supporting its potential as an advanced material for denture construction. However, further clinical studies are recommended.