    Hydrogen uptake of Ti64 and surface–nitrided Ti64 in flowing pressurized water at 300 °C

    by Cyriac Christophe, Quentin Auzoux, Frantz Martin, Frédéric Datcharry, Estelle Loire, Laurence Latu–Romain, Yves Wouters

  • Impurity analysis of synthetic diamond for electronics and quantum physics

    by Estelle Loire, Rémi Gillet, Mohamed Elhachmi Bouras, François Jomard, Marie-Amandine Pinault-Thaury

    Diamond is an ultrawide bandgap semiconductor with exceptional physical properties, making it highly suitable for various advanced applications. However, precise doping control remains a challenge, particularly for n-type conductivity due to doping asymmetry. Additionally, in quantum applications, phosphorus donors enhance nitrogen-vacancy center coherence times, requiring precise impurity level control. This work presents a secondary ion mass spectrometry (SIMS) study on impurities analysis in diamond, focusing on hydrogen, boron, carbon isotope, nitrogen, and phosphorus. Using four implanted standards and two lab-grown samples, we optimized SIMS conditions to improve the detection limits and isotopic ratio measurements. We measured a 13C/12C isotopic ratio of ∼0.004% in a 13C-depleted diamond layer. At low mass resolution, we showed detection limits of up to 1.5 × 1016 and 3.0 × 1015 at/cm3 for boron and phosphorus, respectively. For hydrogen, the increase in the sputtering rate enabled us to move from 4.7 × 1018 to 6.3 × 1017 at/cm3. High mass resolution settings enabled phosphorus detection limits to reach above 3.0 × 1014 at/cm3. Concerning nitrogen, we use an ultrapure lab-grown layer to achieve the measurement of a detection limit of 2.3 × 1016 at/cm3, thanks to the raster size reduction. These results provide crucial insights into impurities’ characterization in diamond, supporting advancements in diamond-based electronic and quantum applications.

  • Compositionally graded Ba1−xSrxTiO3 thin film for SIMS applications

    by J. Scola, J. Garcia, F. Jomard, E. Loire, J. Wolfman, B. Negulescu, G. Z. Liu, M.-A. Pinault-Thaury

    A heterostructure of Ba1−xSrxTiO3/La1.1Sr0.9NiO3/SrTiO3 has been analyzed by magnetic sector secondary ion mass spectrometry (SIMS). The stoichiometry parameter x of the top layer was made varying continuously from 0 to 1 along the width of the sample by combinatorial pulsed laser deposition. Prior to SIMS analysis, the composition gradient of Ba1−xSrxTiO3 was quantitatively characterized by chemical characterizations including wavelength and energy dispersive x-ray spectroscopies. Even if the Ti content is constant into Ba1−xSrxTiO3, its ionic yield exhibits an increasing trend as Ba is substituted by Sr. Such a phenomenon can be explained by the variation of the neighboring atoms chemistry, which affects the ionization probability of titanium during the sputtering process. In addition to the continuously varying composition, the oxide multilayer sample features sharp interfaces hence the in-depth resolution under our analyzing conditions has been investigated too. The modeling of the interface crossing profiles reveals that the instrumental contribution to the profile broadening is as low as 5 nm.

  • Secondary ion mass spectrometry as a tool to analyze semiconductor opening switch diodes

    by Marie-Amandine Pinault-Thaury, Estelle Loire, François Jomard, Anton Gusev, Mawuena Rémi Degnon, Antoine Silvestre de Ferron, Laurent Pecastaing

    This paper presents a secondary ion mass spectrometry (SIMS) method for the analysis of semiconductor opening switch (SOS) diodes, which are crucial in nanosecond pulsed power systems. The study addresses the gap in experimental measurements of doping concentration in SOS diodes, as the current literature contains mainly theoretical doping profiles. The development of a reliable method for measuring doping concentration is expected to advance SOS technology, given the limited number of manufacturers. The SIMS technique is used to determine the depth distribution and concentration of dopants. The method is adapted to study boron, aluminum, and phosphorus in silicon, with emphasis on detection over several hundred micrometers to clarify the doping profile of SOS diodes. The experimental procedure includes (i) preparation of the SOS diode sample by cutting, polishing, and gold plating; (ii) performing dynamic SIMS analysis using specific conditions for boron/aluminum (O2+/M+) and phosphorus (Cs+/M−) detection; and (iii) using a line scan mode to measure element intensities across the sample, with quantification based on reference samples. The developed SIMS conditions enabled the measurement of the depth distribution of the dopants over a range of 1150 μm with a 2 μm step and providing sufficient lateral resolution. The quantified profiles of boron, aluminum, and phosphorus in the SOS diode are presented. The experimental impurity profiles were in partial agreement with the theoretical doping profiles. This method provides access to the analysis of semiconductor devices with thick structures, which are commonly used in power electronics and solid-state pulsed power.