Wenlin Tu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Wenlin Tu has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Shengqian Ruan
College of Civil Engineering and Architecture, Zhejiang University, Hangzhou 310058, China
3 shared publications Chi Sun Poon
Department of Civil and Environmental Engineering and Research Centre for Resources Engineering Towards Carbon Neutrality The Hong Kong Polytechnic University Hong Kong China
2 shared publications- Dingqiang Fan
Department of Civil and Environmental Engineering & Research Centre for Resources Engineering Toward Carbon Neutrality The Hong Kong Polytechnic University Hung Hom, Kowloon Hong Kong China
1 shared publication Dongming Yan
1 shared publication- Dongming Yan
College of Civil Engineering and Architecture, Zhejiang University, Hangzhou 310058, China
1 shared publication Gen Li
1 shared publication
Latest Publications
- 7 November 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (11)
Sulfuric Acid Degradation of Alkali‐Activated Fly Ash–Slag Binders: Multiscale Evolution and Paradoxical Role of Ca
Alkali‐activated fly ash–slag (AAFS) binders have attracted interest as alternative cementitious materials for applications exposed to sulfuric acid, for example, in sewer environments. However, how binder chemistry governs degradation behavior and resistance remains insufficiently understood, particularly regarding structural evolution and damage mechanisms. This study investigated AAFS binders with different precursor compositions (slag content: 10%–75%) and activator chemistries (dosage: 15% and 20%; Ms: 1 and 2) under sulfuric acid exposure, with weekly solution renewal at an initial pH of 1.0 (rising to 1.5–1.9 before renewal). Decreasing slag content generally reduced the 90‐day compressive strength before exposure. Higher activator dosage and Ms also resulted in slight reductions in strength. After a 90‐day exposure, the spatially continuous evolution of the residual gel skeleton across the degraded zone was tracked using multiscale imaging techniques and microhardness testing. The results revealed a paradoxical role of Ca. High‐Ca, slag‐rich AAFS formed denser matrices with greater acid–neutralization capacity, resulting in a 90‐day degradation depth up to 64.8% lower than that of low‐Ca AAFS. However, high‐Ca AAFS developed network cracking and a spalling‐prone weak layer due to decalcification, dealumination, and gypsum‐induced stress, retaining only 15.0%–29.7% of the unaffected‐matrix microhardness. In contrast, low‐Ca AAFS showed faster acid penetration but retained a more continuous, Al‐rich skeleton, with 36.4%–53.3% microhardness retention. These findings distinguish resistance to acid ingress from the preservation of residual‐skeleton integrity and provide new insights into degradation modes, gel‐skeleton evolution, and composition‐informed design of AAFS binders.
- 7 November 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (11)
Sulfuric Acid Degradation of Alkali‐Activated Fly Ash–Slag Binders: Multiscale Evolution and Paradoxical Role of Ca
Alkali‐activated fly ash–slag (AAFS) binders have attracted interest as alternative cementitious materials for applications exposed to sulfuric acid, for example, in sewer environments. However, how binder chemistry governs degradation behavior and resistance remains insufficiently understood, particularly regarding structural evolution and damage mechanisms. This study investigated AAFS binders with different precursor compositions (slag content: 10%–75%) and activator chemistries (dosage: 15% and 20%; Ms: 1 and 2) under sulfuric acid exposure, with weekly solution renewal at an initial pH of 1.0 (rising to 1.5–1.9 before renewal). Decreasing slag content generally reduced the 90‐day compressive strength before exposure. Higher activator dosage and Ms also resulted in slight reductions in strength. After a 90‐day exposure, the spatially continuous evolution of the residual gel skeleton across the degraded zone was tracked using multiscale imaging techniques and microhardness testing. The results revealed a paradoxical role of Ca. High‐Ca, slag‐rich AAFS formed denser matrices with greater acid–neutralization capacity, resulting in a 90‐day degradation depth up to 64.8% lower than that of low‐Ca AAFS. However, high‐Ca AAFS developed network cracking and a spalling‐prone weak layer due to decalcification, dealumination, and gypsum‐induced stress, retaining only 15.0%–29.7% of the unaffected‐matrix microhardness. In contrast, low‐Ca AAFS showed faster acid penetration but retained a more continuous, Al‐rich skeleton, with 36.4%–53.3% microhardness retention. These findings distinguish resistance to acid ingress from the preservation of residual‐skeleton integrity and provide new insights into degradation modes, gel‐skeleton evolution, and composition‐informed design of AAFS binders.
- Open Access
Early-Age Properties and Reaction of Hydrophobic Portland Cement and Alkali-Activated Fly Ash–Slag Pastes with Alkyl Silanes
Cementitious materials are susceptible to water ingress due to their hydrophilicity and porous microstructure, which can cause premature destruction and compromise long-term durability. Integral hydrophobic modification using alkyl silanes is an effective strategy for enhancing water resistance, while the influence of different silanes on early-age properties (within the first 7 d) of various binder systems remains unclear. This study investigates the rheology, flowability, setting behavior, reaction kinetics, compressive strength, and hydrophobicity of ordinary Portland cement (OPC) and alkali-activated fly ash–slag (AAFS) pastes incorporating alkyl silanes of varying alkyl chain lengths, i.e., methyl-(C1TMS), butyl-(C4TMS), octyl-(C8TMS), and dodecyl-trimethoxysilane (C12TMS). In OPC, C1TMS reduced yield stress and plastic viscosity by 33.6% and 21.0%, respectively, and improved flowability by 27.6%, whereas C4TMS, C8TMS, and C12TMS showed the opposite effects. In contrast, the effect of alkyl silanes on rheology and flowability of AAFS was less pronounced. Silanes delayed setting of OPC and AAFS by 5.6–164.4%, with shorter alkyl chains causing greater retardation. C1TMS and C4TMS inhibited early-age heat release and decreased the 1-day compressive strength by 14.8–35.7% in OPC and 82.0–84.5% in AAFS, whereas longer-chain silanes had comparatively minor effects. The hydrophobic performance in both binder systems was strongly correlated with alkyl chain length. C8TMS exhibited the best hydrophobicity in OPC, achieving a water contact angle of 145° and a 75.7% reduction in water sorptivity, while C4TMS demonstrated the highest hydrophobicity in AAFS. This study provides fundamental guidance for the rational selection of alkyl silanes in OPC and AAFS systems, offering insights into the design of multifunctional water-resistant cementitious composites for marine structures, building facades, and other applications with waterproofing requirements.
Open AccessEarly-Age Properties and Reaction of Hydrophobic Portland Cement and Alkali-Activated Fly Ash–Slag Pastes with Alkyl Silanes
Cementitious materials are susceptible to water ingress due to their hydrophilicity and porous microstructure, which can cause premature destruction and compromise long-term durability. Integral hydrophobic modification using alkyl silanes is an effective strategy for enhancing water resistance, while the influence of different silanes on early-age properties (within the first 7 d) of various binder systems remains unclear. This study investigates the rheology, flowability, setting behavior, reaction kinetics, compressive strength, and hydrophobicity of ordinary Portland cement (OPC) and alkali-activated fly ash–slag (AAFS) pastes incorporating alkyl silanes of varying alkyl chain lengths, i.e., methyl-(C1TMS), butyl-(C4TMS), octyl-(C8TMS), and dodecyl-trimethoxysilane (C12TMS). In OPC, C1TMS reduced yield stress and plastic viscosity by 33.6% and 21.0%, respectively, and improved flowability by 27.6%, whereas C4TMS, C8TMS, and C12TMS showed the opposite effects. In contrast, the effect of alkyl silanes on rheology and flowability of AAFS was less pronounced. Silanes delayed setting of OPC and AAFS by 5.6–164.4%, with shorter alkyl chains causing greater retardation. C1TMS and C4TMS inhibited early-age heat release and decreased the 1-day compressive strength by 14.8–35.7% in OPC and 82.0–84.5% in AAFS, whereas longer-chain silanes had comparatively minor effects. The hydrophobic performance in both binder systems was strongly correlated with alkyl chain length. C8TMS exhibited the best hydrophobicity in OPC, achieving a water contact angle of 145° and a 75.7% reduction in water sorptivity, while C4TMS demonstrated the highest hydrophobicity in AAFS. This study provides fundamental guidance for the rational selection of alkyl silanes in OPC and AAFS systems, offering insights into the design of multifunctional water-resistant cementitious composites for marine structures, building facades, and other applications with waterproofing requirements.
- 26 June 2025
- Published by Elsevier in Cement and Concrete Composites
- Vol. 163
Hydration products and hybridisation mechanisms of hydrophobic cement pastes with alkyl-organosilanes
- 26 June 2025
- Published by Elsevier in Cement and Concrete Composites
- Vol. 163
Hydration products and hybridisation mechanisms of hydrophobic cement pastes with alkyl-organosilanes