Haojian Tang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Haojian Tang has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Dejin Xing
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications - Dunlei Su
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications - Jiahui Wang
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications - Mingxin Yang
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications - Weiyi Kong
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications - Xin Liu
School of Civil Engineering, Shandong Jiaotong University, Jinan 250357, China
2 shared publications
Latest Publications
- Open Access
Study on the High-Temperature Reaction Kinetics of Solid Waste-Based High Belite Sulphoaluminate Cement Containing Residual Gypsum in Clinker
In order to elucidate the high-temperature reaction process of solid waste-based high belite sulphoaluminate cement containing residual gypsum in clinker (NHBSAC) and obtain the formation laws of each mineral in clinker, this article studied its high-temperature reaction kinetics. Through QXRD analysis and numerical fitting methods, the formation of C4A3, β-C2S, and CaSO4 in clinker under different calcination systems was quantitatively characterized, the corresponding high-temperature reaction kinetics models were established, and the reaction activation energies of each mineral were obtained. The results indicate that the content of C4A3 and β-C2S increases with the prolongation of holding time and the increase in calcination temperature, while CaSO4 is continuously consumed. Under the control mechanism of solid-state reaction, the formation and consumption of minerals follow the kinetic equation. C4A3 and β-C2S satisfy the D4 equation under diffusion mechanism control, and CaSO4 satisfies the R3 equation under interface chemical reaction mechanism control. The activation energy required for mineral formation varies with different temperature ranges. The activation energies required to form C4A3 at 1200–1225 °C, 1225–1275 °C, and 1275–1300 °C are 166.28 kJ/mol, 83.14 kJ/mol, and 36.58 kJ/mol, respectively. The activation energies required to form β-C2S at 1200–1225 °C and 1225–1300 °C are 374.13 kJ/mol and 66.51 kJ/mol, respectively. This study is beneficial for achieving flexible control of the mineral composition of NHBSAC clinker, providing a theoretical basis and practical experience for the preparation of low-carbon cement and the optimization design of its mineral composition.Open AccessStudy on the High-Temperature Reaction Kinetics of Solid Waste-Based High Belite Sulphoaluminate Cement Containing Residual Gypsum in Clinker
In order to elucidate the high-temperature reaction process of solid waste-based high belite sulphoaluminate cement containing residual gypsum in clinker (NHBSAC) and obtain the formation laws of each mineral in clinker, this article studied its high-temperature reaction kinetics. Through QXRD analysis and numerical fitting methods, the formation of C4A3, β-C2S, and CaSO4 in clinker under different calcination systems was quantitatively characterized, the corresponding high-temperature reaction kinetics models were established, and the reaction activation energies of each mineral were obtained. The results indicate that the content of C4A3 and β-C2S increases with the prolongation of holding time and the increase in calcination temperature, while CaSO4 is continuously consumed. Under the control mechanism of solid-state reaction, the formation and consumption of minerals follow the kinetic equation. C4A3 and β-C2S satisfy the D4 equation under diffusion mechanism control, and CaSO4 satisfies the R3 equation under interface chemical reaction mechanism control. The activation energy required for mineral formation varies with different temperature ranges. The activation energies required to form C4A3 at 1200–1225 °C, 1225–1275 °C, and 1275–1300 °C are 166.28 kJ/mol, 83.14 kJ/mol, and 36.58 kJ/mol, respectively. The activation energies required to form β-C2S at 1200–1225 °C and 1225–1300 °C are 374.13 kJ/mol and 66.51 kJ/mol, respectively. This study is beneficial for achieving flexible control of the mineral composition of NHBSAC clinker, providing a theoretical basis and practical experience for the preparation of low-carbon cement and the optimization design of its mineral composition. - Open Access
Analysis of Influencing Factors in the Preparation Process of Solid Waste-Based Ternesite Sulphoaluminate Cement
Based on a novel ternesite sulphoaluminate cement (NTSAC), the effects of various influencing factors on the calcination of clinker were studied, including mineral composition of clinker, grinding fineness of raw materials, molding technology of samples, and cooling methods of clinker. The research was carried out by taking the calcination system and mineral content of clinker as evaluation indexes, and using RSM and QXRD as analytical means. The results indicate that the optimal calcination temperature of clinker varies with the design mineral composition, while the holding time remains basically unchanged. Clinker with high CaSO4 content has a relatively lower calcination temperature. The use of a calcination system of 1175 °C-49 min can control the mineral content error of the cement below 15%. Moreover, the molding pressure, molding methods, grinding fineness of raw materials, and cooling methods of clinker have significant effects on the clinker preparation to varying degrees, with the order of influence from high to low being molding methods, grinding fineness of raw materials, molding pressure, and cooling methods of clinker. Within the range of experimental parameters, the better preparation conditions are compression molding (molding method), 15 MPa (molding pressure), and 20 μm (grinding fineness). The above research conclusions provide reference data for cement preparation in the laboratory, offering useful guidance for developing novel types of cement.
Open AccessAnalysis of Influencing Factors in the Preparation Process of Solid Waste-Based Ternesite Sulphoaluminate Cement
Based on a novel ternesite sulphoaluminate cement (NTSAC), the effects of various influencing factors on the calcination of clinker were studied, including mineral composition of clinker, grinding fineness of raw materials, molding technology of samples, and cooling methods of clinker. The research was carried out by taking the calcination system and mineral content of clinker as evaluation indexes, and using RSM and QXRD as analytical means. The results indicate that the optimal calcination temperature of clinker varies with the design mineral composition, while the holding time remains basically unchanged. Clinker with high CaSO4 content has a relatively lower calcination temperature. The use of a calcination system of 1175 °C-49 min can control the mineral content error of the cement below 15%. Moreover, the molding pressure, molding methods, grinding fineness of raw materials, and cooling methods of clinker have significant effects on the clinker preparation to varying degrees, with the order of influence from high to low being molding methods, grinding fineness of raw materials, molding pressure, and cooling methods of clinker. Within the range of experimental parameters, the better preparation conditions are compression molding (molding method), 15 MPa (molding pressure), and 20 μm (grinding fineness). The above research conclusions provide reference data for cement preparation in the laboratory, offering useful guidance for developing novel types of cement.