Arai Abdimutalip
Arai Abdimutalip has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Sherzod Kurbanbekov
Center of Excellence “VERITAS”, NJSC D. Serikbayev East Kazakhstan Technical University, Ust-Kamenogorsk 070004, Kazakhstan
2 shared publications - Alibek Tazhibayev
LLP “ALCOR”, Almaty 050043, Kazakhstan
1 shared publication - Berik Kaldar
Research Institute of Natural Sciences, Nanotechnology and New Materials, Khoja Akhmet Yassawi International Kazakh-Turkish University, Turkestan 161200, Kazakhstan
1 shared publication - Dilnoza Baltabayeva
The Research Institute “Natural Sciences, Nanotechnology and New Materials”, Khoja Akhmet Yassawi International Kazakh-Turkish University, Turkestan 161200, Kazakhstan
1 shared publication - Diyar Patchakhanov
The Research Institute “Natural Sciences, Nanotechnology and New Materials”, Khoja Akhmet Yassawi International Kazakh-Turkish University, Turkestan 161200, Kazakhstan
1 shared publication - Lyaila Bayatanova
International School of Engineering, D. Serikbayev East Kazakhstan Technical University, Ust-Kamenogorsk 070000, Kazakhstan
1 shared publication
Latest Publications
- Open Access
Structural-Phase Evolution and Morphology of Cobalt-Free WC Hard Alloys Produced by SPS
This study examines the effect of spark plasma sintering (SPS) temperature on the phase composition, microstructure, densification, and microhardness of cobalt-free WC–Fe and WC–Fe–Ni hard alloys. Increasing the sintering temperature from 1250 °C to 1300 °C improved densification in both alloy systems. Residual porosity decreased from 13.2% to 12.7% in the WC–Fe–Ni alloy and from 13.8% to 12.0% in the WC–Fe alloy, while the density increased from 12.39 g/cm3 to 12.46 g/cm3 and from 12.15 g/cm3 to 12.40 g/cm3, respectively. The WC–Fe -Ni alloy exhibited a more homogeneous microstructure and higher microhardness, increasing from 708 10 HV0.2 to 823 ± 15 HV0.2, whereas the WC–Fe alloy showed an increase from 630 ± 15 HV0.2 to 770 ± 5 HV0.2. X-ray diffraction analyses identified Fe3W3C, FeNi3, and (Fe, Ni) solid-solution phases formed during SPS. The results indicate that both the sintering temperature and binder composition influence densification, phase evolution, and mechanical performance. Among the investigated materials, the WC–Fe–Ni alloy showed better microstructural stability and hardness than the WC–Fe alloy. These findings suggest that Fe–Ni binders are promising candidates for cobalt-free cemented carbides, although additional studies on fracture toughness and wear resistance are required before practical cutting-tool applications can be fully assessed.Open AccessStructural-Phase Evolution and Morphology of Cobalt-Free WC Hard Alloys Produced by SPS
This study examines the effect of spark plasma sintering (SPS) temperature on the phase composition, microstructure, densification, and microhardness of cobalt-free WC–Fe and WC–Fe–Ni hard alloys. Increasing the sintering temperature from 1250 °C to 1300 °C improved densification in both alloy systems. Residual porosity decreased from 13.2% to 12.7% in the WC–Fe–Ni alloy and from 13.8% to 12.0% in the WC–Fe alloy, while the density increased from 12.39 g/cm3 to 12.46 g/cm3 and from 12.15 g/cm3 to 12.40 g/cm3, respectively. The WC–Fe -Ni alloy exhibited a more homogeneous microstructure and higher microhardness, increasing from 708 10 HV0.2 to 823 ± 15 HV0.2, whereas the WC–Fe alloy showed an increase from 630 ± 15 HV0.2 to 770 ± 5 HV0.2. X-ray diffraction analyses identified Fe3W3C, FeNi3, and (Fe, Ni) solid-solution phases formed during SPS. The results indicate that both the sintering temperature and binder composition influence densification, phase evolution, and mechanical performance. Among the investigated materials, the WC–Fe–Ni alloy showed better microstructural stability and hardness than the WC–Fe alloy. These findings suggest that Fe–Ni binders are promising candidates for cobalt-free cemented carbides, although additional studies on fracture toughness and wear resistance are required before practical cutting-tool applications can be fully assessed. - Open Access
- 6 July 2025
- Published by MDPI AG in Lubricants
- Vol. 13 (7) , 297
Microstructure, Phase Components, and Tribological Properties of Al65Cu20Fe15 Quasicrystal Coatings Deposited by HVOF
Quasicrystalline coatings based on Al65Cu20Fe15 are of increasing interest as potential alternatives to conventional wear-resistant materials due to their unique structural and tribological properties. This study explores the influence of air pressure during high-velocity oxy-fuel (HVOF) spraying on the phase composition, morphology, and wear behavior of Al65Cu20Fe15 coatings deposited on U8G tool steel. Coatings were applied at a fixed spraying distance of 350 mm using three air pressures (1.9, 2.1, and 2.3 bar), with constant propane (2.0 bar) and oxygen (2.1 bar) supply. X-ray diffraction analysis identified the formation of Al78Cu48Fe14 and Al0.5Fe1.5 phases, while scanning electron microscopy revealed a dense, uniform microstructure with low porosity and homogeneous element distribution across all samples. Tribological testing using the ball-on-disk method showed wear track widths ranging from 853.47 to 952.50 µm, depending on the air pressure applied. These findings demonstrate that fine-tuning the air pressure during HVOF spraying significantly influences the structural characteristics and wear resistance of the resulting quasicrystalline coatings, highlighting their promise for advanced surface engineering applications.
- 6 July 2025
- Published by MDPI AG in Lubricants
- Vol. 13 (7) , 297
Open AccessMicrostructure, Phase Components, and Tribological Properties of Al65Cu20Fe15 Quasicrystal Coatings Deposited by HVOF
Quasicrystalline coatings based on Al65Cu20Fe15 are of increasing interest as potential alternatives to conventional wear-resistant materials due to their unique structural and tribological properties. This study explores the influence of air pressure during high-velocity oxy-fuel (HVOF) spraying on the phase composition, morphology, and wear behavior of Al65Cu20Fe15 coatings deposited on U8G tool steel. Coatings were applied at a fixed spraying distance of 350 mm using three air pressures (1.9, 2.1, and 2.3 bar), with constant propane (2.0 bar) and oxygen (2.1 bar) supply. X-ray diffraction analysis identified the formation of Al78Cu48Fe14 and Al0.5Fe1.5 phases, while scanning electron microscopy revealed a dense, uniform microstructure with low porosity and homogeneous element distribution across all samples. Tribological testing using the ball-on-disk method showed wear track widths ranging from 853.47 to 952.50 µm, depending on the air pressure applied. These findings demonstrate that fine-tuning the air pressure during HVOF spraying significantly influences the structural characteristics and wear resistance of the resulting quasicrystalline coatings, highlighting their promise for advanced surface engineering applications.