  • Open Access

    Experimental Study on Mechanical Properties of Silica Fume Foam Concrete After Exposure to High Temperatures

    by Shiyi Zhao, Xiaolong Li, Alipujiang Jierula, Hushitaer Niyazi, Bin Yang

    To investigate how the content of silica fume (SF) influences the performance of foam concrete (FC) after high-temperature exposure and the underlying mechanisms, this study prepared standard FC cube specimens with SF contents of 0%, 0.15%, 0.2%, 0.25%, and 0.3%. The working properties of the material at room temperature were systematically tested, and the mass loss, residual compressive strength, failure mode, microstructure and acoustic emission (AE) data at different temperatures (100 °C, 200 °C, 300 °C and 400 °C) were analyzed. The test results indicate that increasing the SF content reduces the fluidity of the fresh paste yet significantly enhances the compressive strength and lowers the water absorption of FC at room temperature. After high-temperature exposure, the effect of SF exhibits a dual character: at 200 °C and below, SF effectively mitigates the performance degradation of FC. However, when the temperature reaches 300–400 °C, specimens with an excessively high SF content (e.g., 0.3%) experience rapidly built-up internal steam pressure that cannot escape in time, which triggers the formation and propagation of a microcrack network and leads to a sharp drop in strength. Based on AE detection and scanning electron microscopy (SEM) image analysis, the failure process of silica fume foam concrete (SFFC) proceeds through three stages: free water evaporation at low temperatures, dehydration shrinkage of the C-S-H gel at medium temperatures, and finally, structural failure marked by the collapse of the C-S-H gel network at high temperatures. This study indicates that an SF content of 0.25% allows FC to achieve an optimal balance between mechanical properties and high-temperature stability. The findings provide a theoretical basis for optimizing FC mix proportions and enhancing fire prevention design.

  • Open Access

    Axial Performance of GFRP-Confined High-Fly-Ash Coal-Gangue Self-Compacting Concrete: Strength Enhancement and Damage Evolution

    by Baiyun Yu, Abudusaimaiti Kali, Hushitaer Niyazi, Hongchao Zhao

    As infrastructure construction expands, the massive consumption of traditional concrete materials has led to resource shortages and environmental pollution. Utilizing industrial wastes such as coal gangue and fly ash to produce high-performance concrete is an important pathway toward a greener construction industry. However, concrete incorporating high volumes of fly ash and coal gangue (i.e., high-volume fly-ash coal-gangue self-compacting concrete, CGSC) suffers from low strength and high brittleness due to the inherent deficiencies of its constituents. This study proposes using glass fiber-reinforced polymer (GFRP) tubes for external confinement to improve the axial compressive capacity and deformability of CGSC. A total of 27 concrete cylinders were prepared and tested under axial compression, with real-time acoustic emission (AE) monitoring. The variables examined include the coarse aggregate type (coal-gangue and natural gravel), GFRP tube thickness (5 mm and 8 mm), and fly-ash content (80%, 85%, 90%). The stress–strain response of each specimen and the failure evolution of internal cracks were recorded throughout the loading process. The results show that GFRP tube confinement markedly increases the axial strength and ductility of CGSC. AE features exhibited staged behavior that closely mirrored the stress–strain curves. This correspondence reveals the progression of internal cracks under confinement and indicates that AE is an effective tool for damage monitoring in such composites. The findings provide a new technical approach for the efficient reuse of solid waste in concrete and offer a theoretical and practical basis for applying FRP composite structures in underground support engineering.