Priya S. Nair
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Priya S. Nair has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
Blessen Skariah Thomas
National Institute of Technology Calicut, Kozhikode, Kerala, 673601, India
2 shared publicationsRajesh Gupta
Malaviya National Institute of Technology, Jaipur, Jaipur, Rajasthan, 302017, India
2 shared publicationsVinay Agrawal
Malaviya National Institute of Technology, Jaipur, Jaipur, Rajasthan, 302017, India
2 shared publicationsAzree Othuman Mydin
School of Housing, Building and Planning, Universiti Sains Malaysia, Penang, 11800, Malaysia
1 shared publication- Missgna Addisalem Berhe
Department of Civil Engineering, College of Engineering and Technology, Adigrat University, Adigrat, Ethiopia.
1 shared publication - Shashwati Soumya Pradhan
Department of Civil Engineering, National Institution of Technology, Agartala, India
1 shared publication
Latest Publications
- Open Access
- 14 May 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Synergistic enhancement of strength and durability in self-healing concrete using treated pineapple fibres and bacterial mineralization
Conventional cement concrete is inherently brittle and susceptible to microcracking, which compromises durability and long-term performance. In order to remediate such conditions, the current research explores the integration of bacterial wollastonite and alkali-treated natural pineapple leaf Fibres (PALFs) to enhance mechanical, durability, and self-healing performance in cement concrete composite. A consortium of microbial system comprising ureolytic Bacillus sp. and non-ureolytic Bacillus cohnii was inoculated with an optimum 10% wollastonite mineral. Treated Fibres of varying dimensions (5, 10, 15 and 20 mm) and percentages (0.25, 0.5, 0.75 and 1%) were examined for their mechanical and durability properties. The inclusion of Fibres demonstrated the highest compressive strength improvement up to 26%, while the flexural and tensile features increased by 27.80% and 35%. Water absorption remained below 10%, with final absorption under 3%, confirming reduced porosity. Longer Fibres improved interlocking, minimizing abrasion loss (< 2.5 mm). Ultrasonic Pulse Velocity (UPV) exceeding 4.5 km/s and rebound number (> 40) classified the concrete as structurally dense and durable. The consistency of material integrity was substantiated by significant correlations observed between compressive strength, rebound number, and UPV. Comprehensive analyses through XRD and SEM-EDS validated extensive calcite deposition, indicating biomineralization that can contribute to autonomous crack-healing mechanisms, although self-healing efficiency was not directly quantified. These results demonstrate the viability of consortium-reinforced concrete incorporating wollastonite Fibres as a resilient and sustainability-oriented material, particularly for infrastructure applications where enhanced durability, extended service life, and reduced maintenance demands are critical.
- 14 May 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Open AccessSynergistic enhancement of strength and durability in self-healing concrete using treated pineapple fibres and bacterial mineralization
Conventional cement concrete is inherently brittle and susceptible to microcracking, which compromises durability and long-term performance. In order to remediate such conditions, the current research explores the integration of bacterial wollastonite and alkali-treated natural pineapple leaf Fibres (PALFs) to enhance mechanical, durability, and self-healing performance in cement concrete composite. A consortium of microbial system comprising ureolytic Bacillus sp. and non-ureolytic Bacillus cohnii was inoculated with an optimum 10% wollastonite mineral. Treated Fibres of varying dimensions (5, 10, 15 and 20 mm) and percentages (0.25, 0.5, 0.75 and 1%) were examined for their mechanical and durability properties. The inclusion of Fibres demonstrated the highest compressive strength improvement up to 26%, while the flexural and tensile features increased by 27.80% and 35%. Water absorption remained below 10%, with final absorption under 3%, confirming reduced porosity. Longer Fibres improved interlocking, minimizing abrasion loss (< 2.5 mm). Ultrasonic Pulse Velocity (UPV) exceeding 4.5 km/s and rebound number (> 40) classified the concrete as structurally dense and durable. The consistency of material integrity was substantiated by significant correlations observed between compressive strength, rebound number, and UPV. Comprehensive analyses through XRD and SEM-EDS validated extensive calcite deposition, indicating biomineralization that can contribute to autonomous crack-healing mechanisms, although self-healing efficiency was not directly quantified. These results demonstrate the viability of consortium-reinforced concrete incorporating wollastonite Fibres as a resilient and sustainability-oriented material, particularly for infrastructure applications where enhanced durability, extended service life, and reduced maintenance demands are critical.
- Open Access
- 22 October 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1) , 1-32
Bacterial wollastonite concrete for sustainable high performance construction
This study explores the mechanical, microstructural, and non-destructive properties of concrete incorporating microbial consortia, specifically ureolytic and non-ureolytic variants, at concentrations of 10⁹ and 10⁵ cells/ml across water-to-binder (w/b) ratios of 0.45, 0.4, and 0.35. Wollastonite was introduced as a mineral additive at substitution levels of 5%, 10%, and 15%, with performance declining beyond the optimal substitution threshold. After 28 days of curing, specimens with a higher consortium concentration (10⁹ cells/ml) exhibited compressive strength enhancements of 27.20%, 23%, and 22.31% for 5%, 10%, and 15% wollastonite incorporation, respectively, compared to the control. In contrast, the lower consortium concentration (10⁵ cells/ml) resulted in compressive strength improvements of 41.45%, 39.35%, and 31.07% for the corresponding substitution levels, indicating the efficacy of the lower consortium to develop strength properties at a younger age. Flexural strength followed a similar trend, with increases of 25%, 16.15%, and 25%, respectively. Notably, the lower consortium concentration (10⁵ cells/ml) provided superior mechanical performance compared to the higher concentration (10⁹ cells/ml) due to the lower cell density and biofilm formation. Non-destructive evaluations, including Ultrasonic Pulse Velocity (UPV > 4.5 km/sec) and rebound number above 40, confirmed the enhanced quality of the concrete. Regression analysis exhibited strong correlations (R² values) between compressive strength, flexural strength, split tensile strength, UPV, and rebound number. Microstructural analyses employing SEM-EDS, XRD, and FTIR spectroscopy remarked significant calcite deposition, leading to matrix densification and improved durability. The embodied energy evaluation significantly underscores the inclusion of wollastonite, a low-energy and low-emission calcium silicate mineral, significantly enhancing eco-efficiency by partially replacing cement. At the same time, the bacterial consortium promotes self-healing and durability with minimal environmental impact. These findings highlight the potential of microbial-wollastonite-based concrete as a sustainable and high-performance material for modern construction applications.
- 22 October 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1) , 1-32
Open AccessBacterial wollastonite concrete for sustainable high performance construction
This study explores the mechanical, microstructural, and non-destructive properties of concrete incorporating microbial consortia, specifically ureolytic and non-ureolytic variants, at concentrations of 10⁹ and 10⁵ cells/ml across water-to-binder (w/b) ratios of 0.45, 0.4, and 0.35. Wollastonite was introduced as a mineral additive at substitution levels of 5%, 10%, and 15%, with performance declining beyond the optimal substitution threshold. After 28 days of curing, specimens with a higher consortium concentration (10⁹ cells/ml) exhibited compressive strength enhancements of 27.20%, 23%, and 22.31% for 5%, 10%, and 15% wollastonite incorporation, respectively, compared to the control. In contrast, the lower consortium concentration (10⁵ cells/ml) resulted in compressive strength improvements of 41.45%, 39.35%, and 31.07% for the corresponding substitution levels, indicating the efficacy of the lower consortium to develop strength properties at a younger age. Flexural strength followed a similar trend, with increases of 25%, 16.15%, and 25%, respectively. Notably, the lower consortium concentration (10⁵ cells/ml) provided superior mechanical performance compared to the higher concentration (10⁹ cells/ml) due to the lower cell density and biofilm formation. Non-destructive evaluations, including Ultrasonic Pulse Velocity (UPV > 4.5 km/sec) and rebound number above 40, confirmed the enhanced quality of the concrete. Regression analysis exhibited strong correlations (R² values) between compressive strength, flexural strength, split tensile strength, UPV, and rebound number. Microstructural analyses employing SEM-EDS, XRD, and FTIR spectroscopy remarked significant calcite deposition, leading to matrix densification and improved durability. The embodied energy evaluation significantly underscores the inclusion of wollastonite, a low-energy and low-emission calcium silicate mineral, significantly enhancing eco-efficiency by partially replacing cement. At the same time, the bacterial consortium promotes self-healing and durability with minimal environmental impact. These findings highlight the potential of microbial-wollastonite-based concrete as a sustainable and high-performance material for modern construction applications.