Margita Kabátová
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Margita Kabátová has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Róbert Bidulský
Bodva Industry and Innovation Cluster, Budulov 174, 04501 Moldava nad Bodvou, Slovakia
2 shared publications - Andrew S. Wronski
University of Bradford
1 shared publication - Dudrova
Slovak Academy of Sciences, Institute of Materials Research, Watsonova 47, Košice 040 01, Slovak Republic
1 shared publication E. Dudrová
Slovak Academy of Sciences in Kosice
1 shared publication- Eduard Hryha
Chalmers University of Technology
1 shared publication Eva Dudrová
Slovak Academy of Sciences
1 shared publication
Latest Publications
- 19 March 2021
- Published by EDP Sciences in Metallurgical Research & Technology
- Vol. 118 (2) , 210
Structural and mechanical properties of W-C: H coatings prepared by HiTUS
The structure and mechanical properties of hydrogenated tungsten-carbon (W-C: H) coatings have been studied as a function of the composition and structure. These coatings were prepared by the High Target Utilization Sputtering (HiTUS), the first time used for this type of coatings. W-C: H coatings were deposited from tungsten–carbide target in argon, argon–acetylene (C2H2), and argon–methane (CH4) atmosphere on bearing steel 100Cr6 substrate, Al substrate, Si wafer a, and WC-Co substrate. W-C: H coatings obtained at different acetylene and methane flow were characterized by Elastic Recoil Detection Analysis (ERDA) and Rutherford Backscattering (RBS), X-ray diffraction, Transmission electron microscopy (TEM), and nanoindentation. Mechanical properties of these coatings are controlled within a range through a change in mutual concentration of crystalline phase and amorphous hydrogenated carbon matrix. The higher hardness (Hit = 29.5 ± 4.5 GPa) was measured for coating with 3 sccm methane addition. W-C: H coatings with more than 4 sccm of C2H2 and CH4 addition had fully amorphous structure and worse off mechanical properties.
- 19 March 2021
- Published by EDP Sciences in Metallurgical Research & Technology
- Vol. 118 (2) , 210
Structural and mechanical properties of W-C: H coatings prepared by HiTUS
The structure and mechanical properties of hydrogenated tungsten-carbon (W-C: H) coatings have been studied as a function of the composition and structure. These coatings were prepared by the High Target Utilization Sputtering (HiTUS), the first time used for this type of coatings. W-C: H coatings were deposited from tungsten–carbide target in argon, argon–acetylene (C2H2), and argon–methane (CH4) atmosphere on bearing steel 100Cr6 substrate, Al substrate, Si wafer a, and WC-Co substrate. W-C: H coatings obtained at different acetylene and methane flow were characterized by Elastic Recoil Detection Analysis (ERDA) and Rutherford Backscattering (RBS), X-ray diffraction, Transmission electron microscopy (TEM), and nanoindentation. Mechanical properties of these coatings are controlled within a range through a change in mutual concentration of crystalline phase and amorphous hydrogenated carbon matrix. The higher hardness (Hit = 29.5 ± 4.5 GPa) was measured for coating with 3 sccm methane addition. W-C: H coatings with more than 4 sccm of C2H2 and CH4 addition had fully amorphous structure and worse off mechanical properties.
- 14 March 2016
- Published by SAGE Publications in Powder Metallurgy
- Vol. 59 (2) , 148-167
A review of failure of sintered steels: fractography of static and dynamic crack nucleation, coalescence, growth and propagation
The failure of sintered steels differs from the behaviour of wrought steels because of factors such as porosity, remnants of previous particle surfaces and generally more complex microstructures. All these factors influence initiation, growth and propagation of microcracks when the sintered microstructure is mechanically loaded. Fracture paths and fracture resistance are shown to be related to details of the microstructures comprising ferrite, austenite, bainite, martensite, pores and weak interfaces. All these have characteristic fracture resistance properties resulting in, frequently combinations of, dimple rupture, cleavage, intergranular and interparticle failure micromechanisms. Results are presented of systematic studies, enabling identification of relevant stresses, in static and dynamic three-point loading, as the cracking process progresses. In static loading, microcracking has been detected in some steels below the macroscopic yield stress and in the first 100 cycles in fatigue. Microcracks nucleate, grow and coalesce, in a step-wise manner, before achieving a catastrophic size – for which conventional fracture mechanics holds. Thus, application of Paris-type analysis to Stage II fatigue is therefore inappropriate. The review focuses on failure micromechanisms and interpretation of fracture surface composition of sintered steels, particularly of those based on Distaloy AE and Astaloy CrL powders. The relationships between microstructure and mechanical properties are discussed.
- 14 March 2016
- Published by SAGE Publications in Powder Metallurgy
- Vol. 59 (2) , 148-167
A review of failure of sintered steels: fractography of static and dynamic crack nucleation, coalescence, growth and propagation
The failure of sintered steels differs from the behaviour of wrought steels because of factors such as porosity, remnants of previous particle surfaces and generally more complex microstructures. All these factors influence initiation, growth and propagation of microcracks when the sintered microstructure is mechanically loaded. Fracture paths and fracture resistance are shown to be related to details of the microstructures comprising ferrite, austenite, bainite, martensite, pores and weak interfaces. All these have characteristic fracture resistance properties resulting in, frequently combinations of, dimple rupture, cleavage, intergranular and interparticle failure micromechanisms. Results are presented of systematic studies, enabling identification of relevant stresses, in static and dynamic three-point loading, as the cracking process progresses. In static loading, microcracking has been detected in some steels below the macroscopic yield stress and in the first 100 cycles in fatigue. Microcracks nucleate, grow and coalesce, in a step-wise manner, before achieving a catastrophic size – for which conventional fracture mechanics holds. Thus, application of Paris-type analysis to Stage II fatigue is therefore inappropriate. The review focuses on failure micromechanisms and interpretation of fracture surface composition of sintered steels, particularly of those based on Distaloy AE and Astaloy CrL powders. The relationships between microstructure and mechanical properties are discussed.
- 1 January 2011
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 672, 31-38
Improvement of Mechanical Properties of Fe-Cr-Mo-[Cu-Ni]-C Sintered Sintered Steels by Sinter Hardening
The effect of high temperature sintering and high cooling rate on shifting the microstructural composition to the favourably of martensite-bainite structures and thus effective improvement of mechanical properties of sintered steels based on Astaloy CrL powder with an addition of 1 and 2% Cu or 50% Distaloy AB powder and 0.65% C was investigated. All the systems were processed by both sinter-hardening and conventional sintering. The vacuum sintering at high-temperature of 1240 0C and at common temperature of 1180 0C were integrated with high (6 0C/s), medium (3 0C/s) and slow (0.1 0C/s) cooling rates; conventional sintering at 1180 0C with cooling rate of ~0.17 0C/s was carried out in a N2+10%H2 atmosphere. In dependence on chemical composition, the yield and tensile strengths of 890-1150 MPa and 913-1230 MPa respectively and impact energy of 10-15 J were achieved by sinter-hardening. The yield and tensile strengths are approximately double than those resulting from conventional sintering.
- 1 January 2011
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 672, 31-38
Improvement of Mechanical Properties of Fe-Cr-Mo-[Cu-Ni]-C Sintered Sintered Steels by Sinter Hardening
The effect of high temperature sintering and high cooling rate on shifting the microstructural composition to the favourably of martensite-bainite structures and thus effective improvement of mechanical properties of sintered steels based on Astaloy CrL powder with an addition of 1 and 2% Cu or 50% Distaloy AB powder and 0.65% C was investigated. All the systems were processed by both sinter-hardening and conventional sintering. The vacuum sintering at high-temperature of 1240 0C and at common temperature of 1180 0C were integrated with high (6 0C/s), medium (3 0C/s) and slow (0.1 0C/s) cooling rates; conventional sintering at 1180 0C with cooling rate of ~0.17 0C/s was carried out in a N2+10%H2 atmosphere. In dependence on chemical composition, the yield and tensile strengths of 890-1150 MPa and 913-1230 MPa respectively and impact energy of 10-15 J were achieved by sinter-hardening. The yield and tensile strengths are approximately double than those resulting from conventional sintering.
- 1 March 2004
- Published by SAGE Publications in Powder Metallurgy
- Vol. 47 (2) , 180-189
Industrial processing, microstructures and mechanical properties of Fe–(2–4)Mn (–0.85Mo)–(0.3–0.7)C sintered steels
The potential of PM Mn steels has been established in laboratory experiments. This paper deals with sintering of Fe–(2–4)Mn–(0.3/0.7)C, also with 0˙85%Mo addition, in an industrial pusher furnace at 1180°C in an atmosphere of 25% hydrogen plus 75% nitrogen, obtained from a cryogenic liquid, giving an inlet dew-point of −55 °C. Tensile, bend (including fatigue) and miniature Charpy specimens were sintered in flowing gases and in semiclosed containers with a getter of ferromanganese, carbon and alumina. The quenched and tem- pered state was investigated, as was sinter hardening (cooling rate of 55 K min −1), simulated for comparison with slow cooling at 10 K min −1. As there was no forma tion of oxide networks at the combination of sintering temperature and dewpoint, in accordance with the Ellingham–Richardson diagram for Mn oxidation/reduction, the use of semiclosed containers was superfluous. The quenched and tempered specimens were brittle. Sinter hardening lead to an improvement in mechanical properties. The reproducibility of tensile and TRS data was high for the sintered materials, characterised by Weibull moduli m of 12–41. All the alloy microstructures were complex and heterogeneous, consisting of, depending on the local manganese and carbon contents, the diffusive and non-diffusive transformation products (pearlite, bainite, martensite) and additionally ferrite and retained austenite. The highest mechanical properties in the entire range of compositions investigated in the furnace cooled state: yield, tensile and bend strengths of 499, 637 and 1280 MPa, respectively, with impact energy of 18 J, and tensile and bend strains of 1˙17 and 1.57%, were achieved for the Fe–2Mn–0.85Mo–0.5C alloy, marginally superior to Fe–2Mn–0.7C. For the sinter hardened Fe–4Mn–0.3C alloy yield, tensile and bend strengths were 570, 664 and 1263 MPa, respectively, at an acceptable impact energy of 14 J, with tensile and bend strains of 0.52% and 1.8%. Many of the results compare favourably with the requirements of MPIF standard 35. Mn is a more effective strengthening agent than either Ni or Cu, or their combination, though generally at reduced plasticity.
- 1 March 2004
- Published by SAGE Publications in Powder Metallurgy
- Vol. 47 (2) , 180-189
Industrial processing, microstructures and mechanical properties of Fe–(2–4)Mn (–0.85Mo)–(0.3–0.7)C sintered steels
The potential of PM Mn steels has been established in laboratory experiments. This paper deals with sintering of Fe–(2–4)Mn–(0.3/0.7)C, also with 0˙85%Mo addition, in an industrial pusher furnace at 1180°C in an atmosphere of 25% hydrogen plus 75% nitrogen, obtained from a cryogenic liquid, giving an inlet dew-point of −55 °C. Tensile, bend (including fatigue) and miniature Charpy specimens were sintered in flowing gases and in semiclosed containers with a getter of ferromanganese, carbon and alumina. The quenched and tem- pered state was investigated, as was sinter hardening (cooling rate of 55 K min −1), simulated for comparison with slow cooling at 10 K min −1. As there was no forma tion of oxide networks at the combination of sintering temperature and dewpoint, in accordance with the Ellingham–Richardson diagram for Mn oxidation/reduction, the use of semiclosed containers was superfluous. The quenched and tempered specimens were brittle. Sinter hardening lead to an improvement in mechanical properties. The reproducibility of tensile and TRS data was high for the sintered materials, characterised by Weibull moduli m of 12–41. All the alloy microstructures were complex and heterogeneous, consisting of, depending on the local manganese and carbon contents, the diffusive and non-diffusive transformation products (pearlite, bainite, martensite) and additionally ferrite and retained austenite. The highest mechanical properties in the entire range of compositions investigated in the furnace cooled state: yield, tensile and bend strengths of 499, 637 and 1280 MPa, respectively, with impact energy of 18 J, and tensile and bend strains of 1˙17 and 1.57%, were achieved for the Fe–2Mn–0.85Mo–0.5C alloy, marginally superior to Fe–2Mn–0.7C. For the sinter hardened Fe–4Mn–0.3C alloy yield, tensile and bend strengths were 570, 664 and 1263 MPa, respectively, at an acceptable impact energy of 14 J, with tensile and bend strains of 0.52% and 1.8%. Many of the results compare favourably with the requirements of MPIF standard 35. Mn is a more effective strengthening agent than either Ni or Cu, or their combination, though generally at reduced plasticity.