Zhiwei Qin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Zhiwei Qin has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
- Honggang Dong
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, PR China
4 shared publications Bin Wang
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, PR China
2 shared publicationsJiachen Li
School of Materials Science and Engineering, Dalian University of Technology, Dalian, People’s Republic of China
2 shared publicationsJilong Wang
School of Materials Science and Engineering, Dalian University of Technology, Dalian, People’s Republic of China
2 shared publicationsPeng Li
School of Materials Science and Engineering, Dalian University of Technology, Dalian, People’s Republic of China
2 shared publications- Peng Li
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, PR China
2 shared publications
Latest Publications
- Open Access
- 2 October 2026
- Published by IOP Publishing in International Journal of Extreme Manufacturing
- Vol. 9 (1) , 015010
Lattice reconstruction and dislocation recapture enhance the fracture resistance of η-Fe 2 Al 5 -bearing interfaces in dissimilar Al/steel joints
The inherent brittleness of interfacial Al-rich intermetallic compounds (IMCs) remains a major obstacle to reliable Fe-Al-based lightweight structural joints, as welding-induced residual-stress localization readily triggers crack initiation within the IMC-bearing region. Here, a two-step strategy integrating lattice reconstruction with dislocation recapture is proposed to improve the room-temperature fracture resistance of η-Fe 2 Al 5 in dissimilar Al/steel joints. Low-temperature annealing promotes rapid reconstruction of the strained η-Fe 2 Al 5 lattice and relieves long-range residual stress, while subsequent water quenching facilitates the recapture of dispersed isolated dislocations. The treated joints achieve a tensile strength of ~258.6 MPa, corresponding to an ~80.3% increase over the as-processed state, together with a ~70% increase in the fracture toughness of the η-Fe 2 Al 5 -bearing layer. In situ X-ray diffraction and first-principles calculations reveal that localized compressive strain accelerates the reverse eutectoid transformation, through which β 0 -associated transformation strain provides an additional driving force for dislocation-network decoupling and stress relief of the η-Fe 2 Al 5 layer. The retained coherent η-Fe 2 Al 5 /β 0 interface and the recaptured isolated dislocations further promote local strain accommodation in η-Fe 2 Al 5 , while crack deflection, blunting, and bridging dissipate fracture energy, as supported by molecular dynamics simulations. These results suggest a potential strategy for improving fracture-limited IMC-bearing interfaces in dissimilar-metal joints through coordinated regulation of residual stress and dislocation functionality.
- 2 October 2026
- Published by IOP Publishing in International Journal of Extreme Manufacturing
- Vol. 9 (1) , 015010
Open AccessLattice reconstruction and dislocation recapture enhance the fracture resistance of η-Fe 2 Al 5 -bearing interfaces in dissimilar Al/steel joints
The inherent brittleness of interfacial Al-rich intermetallic compounds (IMCs) remains a major obstacle to reliable Fe-Al-based lightweight structural joints, as welding-induced residual-stress localization readily triggers crack initiation within the IMC-bearing region. Here, a two-step strategy integrating lattice reconstruction with dislocation recapture is proposed to improve the room-temperature fracture resistance of η-Fe 2 Al 5 in dissimilar Al/steel joints. Low-temperature annealing promotes rapid reconstruction of the strained η-Fe 2 Al 5 lattice and relieves long-range residual stress, while subsequent water quenching facilitates the recapture of dispersed isolated dislocations. The treated joints achieve a tensile strength of ~258.6 MPa, corresponding to an ~80.3% increase over the as-processed state, together with a ~70% increase in the fracture toughness of the η-Fe 2 Al 5 -bearing layer. In situ X-ray diffraction and first-principles calculations reveal that localized compressive strain accelerates the reverse eutectoid transformation, through which β 0 -associated transformation strain provides an additional driving force for dislocation-network decoupling and stress relief of the η-Fe 2 Al 5 layer. The retained coherent η-Fe 2 Al 5 /β 0 interface and the recaptured isolated dislocations further promote local strain accommodation in η-Fe 2 Al 5 , while crack deflection, blunting, and bridging dissipate fracture energy, as supported by molecular dynamics simulations. These results suggest a potential strategy for improving fracture-limited IMC-bearing interfaces in dissimilar-metal joints through coordinated regulation of residual stress and dislocation functionality.
- Open Access
- 15 January 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (6) , 3057-3068
A high-entropy gradient filler metal enables high-strength joints of Ti 2 AlNb and GH4169 alloys
Vacuum brazing with an innovative filler alloy is critical for manufacturing high-precision aerospace components requiring exceptional comprehensive performance, yet achieving superior strength in Ti 2 AlNb/GH4169 brazed joints remains challenging.
- 15 January 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (6) , 3057-3068
Open AccessA high-entropy gradient filler metal enables high-strength joints of Ti 2 AlNb and GH4169 alloys
Vacuum brazing with an innovative filler alloy is critical for manufacturing high-precision aerospace components requiring exceptional comprehensive performance, yet achieving superior strength in Ti 2 AlNb/GH4169 brazed joints remains challenging.
- 22 December 2025
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (3) , 1962-1979
Radial microstructural uniformity in inertia friction welded IN718/FGH96 dissimilar joints with post-weld heat treatment
- 22 December 2025
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (3) , 1962-1979
Radial microstructural uniformity in inertia friction welded IN718/FGH96 dissimilar joints with post-weld heat treatment
- Open Access
- 1 January 2025
- Published by Lab Academic Press in Materials Lab
- Vol. 4, 250104-1-250104-11
Suppressing interfacial defects toward high-perform-ance diffusion bonded FGH99 superalloy via asand-wich-structured interlayer
Interfacial voids and unbonded defects acted as stress concentration sites that significantly degraded the mechanical properties and directly compromised the structural integrity and service life of critical components. Herein, an innovatively Ni/Cr0.625-Al2.875/Ni sandwich-structured interlayer was designed to achieve high-quality diffusion bonding of FGH99 superalloy by regulating interfacial diffusion and recrystallization behavior. The results demonstrated that Ni foil effectively promoted the closure of interfacial voids and induced the formation of a graded interfacial structure, including the Ni transition zone (NTZ) and the interlayer diffusion zone (IDZ). This structure provided high-density grain boundaries as fast diffusion channels for elements, and served as an in-situ reaction container for the precipitation of γ′ strengthening phases. The shear strength of the joint with the sandwich-structured interlayer reached 857.7 MPa, which increased by 67.6 MPa compared to that of the single-layer interlayer. The fracture path of the joint transformed from the original bonding interface to the NTZ/IDZ interface. The fracture surface exhibited lots of fine dimples, indicating a transition from weak interfacial bonding to bulk strengthening and toughening of the joint. This work elucidated the mechanism of void closure and microstructural evolution mediated by the Ni interlayer, providing important theoretical support for the development of high-performance Ni-based superalloy diffusion bonding technology.
- 1 January 2025
- Published by Lab Academic Press in Materials Lab
- Vol. 4, 250104-1-250104-11
Open AccessSuppressing interfacial defects toward high-perform-ance diffusion bonded FGH99 superalloy via asand-wich-structured interlayer
Interfacial voids and unbonded defects acted as stress concentration sites that significantly degraded the mechanical properties and directly compromised the structural integrity and service life of critical components. Herein, an innovatively Ni/Cr0.625-Al2.875/Ni sandwich-structured interlayer was designed to achieve high-quality diffusion bonding of FGH99 superalloy by regulating interfacial diffusion and recrystallization behavior. The results demonstrated that Ni foil effectively promoted the closure of interfacial voids and induced the formation of a graded interfacial structure, including the Ni transition zone (NTZ) and the interlayer diffusion zone (IDZ). This structure provided high-density grain boundaries as fast diffusion channels for elements, and served as an in-situ reaction container for the precipitation of γ′ strengthening phases. The shear strength of the joint with the sandwich-structured interlayer reached 857.7 MPa, which increased by 67.6 MPa compared to that of the single-layer interlayer. The fracture path of the joint transformed from the original bonding interface to the NTZ/IDZ interface. The fracture surface exhibited lots of fine dimples, indicating a transition from weak interfacial bonding to bulk strengthening and toughening of the joint. This work elucidated the mechanism of void closure and microstructural evolution mediated by the Ni interlayer, providing important theoretical support for the development of high-performance Ni-based superalloy diffusion bonding technology.