Amine Herbadji
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Amine Herbadji has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Abdelmadjid Herbadji
Laboratory of Physical Chemistry of Materials, Faculty of Sciences and Technology, Chadli Bendjedid University, 36000 El Tarf, Algeria
1 shared publication - Adel Aitbara
Laboratory of Physical Chemistry of Materials, Faculty of Sciences and Technology, Chadli Bendjedid University, El Tarf, Algeria
1 shared publication - Ibrahim Yaacoub Bouderbala
Applied Optics Laboratory, Institute of Optics and Precision Mechanics, University of Ferhat Abbas, 19000 Setif, Algeria
1 shared publication - Selma Rabhi
Laboratory of Innovative Environmental Preservation Techniques, Department of Chemistry, Constantine 1 University, 25000 Constantine, Algeria
1 shared publication - Slimane Khelloufi
Laboratory: Growth and Characterization of New Semiconductors, Faculty of Sciences, University of Ferhat Abbas, 19000 Setif, Algeria
1 shared publication - Walid Bououden
Laboratory of Physical Chemistry of Materials, Faculty of Sciences and Technology, Chadli Bendjedid University, 36000 El Tarf, Algeria
1 shared publication
Latest Publications
- 3 February 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (3) , 032503
Optimizing the Photocatalytic Performance of n-Type Cu 2 O/FTO Photoanodes by Controlling Electrodeposited Film Thickness
N-Type Cu 2 O is a promising photocatalyst due to its direct bandgap, enabling strong visible-light absorption. When used as a photoelectrode, however, its performance depends critically on film thickness, which must balance light absorption with efficient charge transport. This study systematically optimized the thickness of electrodeposited Cu 2 O films on FTO substrates by varying deposition time from 5 to 40 min. As deposition time increased, the films evolved from pyramidal nanostructures to dense polycrystalline layers, with thicknesses ranging from ~150 nm to ~1200 nm. Thicker films exhibited improved visible-light absorption and a slight bandgap narrowing from 2.35 to 2.25 eV. All samples showed stable anodic photocurrents characteristic of n-type behavior. The highest photocurrent 0.118 mA occurred for the film deposited for 30 min, corresponding to an optimal thickness of ~750 nm. At this thickness, the film effectively absorbs incident photons while still allowing photogenerated carriers to reach the interface before recombining. Beyond this optimal point, photocatalytic activity declined sharply despite continued gains in light absorption, due to the thickness exceeding the charge-carrier diffusion length, which increased recombination and transport resistance. These results highlight the importance of precise thickness control for maximizing Cu 2 O/FTO photoanode efficiency.
- 3 February 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (3) , 032503
Optimizing the Photocatalytic Performance of n-Type Cu 2 O/FTO Photoanodes by Controlling Electrodeposited Film Thickness
N-Type Cu 2 O is a promising photocatalyst due to its direct bandgap, enabling strong visible-light absorption. When used as a photoelectrode, however, its performance depends critically on film thickness, which must balance light absorption with efficient charge transport. This study systematically optimized the thickness of electrodeposited Cu 2 O films on FTO substrates by varying deposition time from 5 to 40 min. As deposition time increased, the films evolved from pyramidal nanostructures to dense polycrystalline layers, with thicknesses ranging from ~150 nm to ~1200 nm. Thicker films exhibited improved visible-light absorption and a slight bandgap narrowing from 2.35 to 2.25 eV. All samples showed stable anodic photocurrents characteristic of n-type behavior. The highest photocurrent 0.118 mA occurred for the film deposited for 30 min, corresponding to an optimal thickness of ~750 nm. At this thickness, the film effectively absorbs incident photons while still allowing photogenerated carriers to reach the interface before recombining. Beyond this optimal point, photocatalytic activity declined sharply despite continued gains in light absorption, due to the thickness exceeding the charge-carrier diffusion length, which increased recombination and transport resistance. These results highlight the importance of precise thickness control for maximizing Cu 2 O/FTO photoanode efficiency.