Shuai Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shuai Li has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Delin Liu
AECC Beijing Institute of Aeronautical Materials, Beijing, China
2 shared publications - Huangyue Cai
School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
2 shared publications - Limin He
Surface Engineering Institution, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2 shared publications - Rende Mu
AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2 shared publications - Wenhui Yang
Surface Engineering Institution, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2 shared publications - Xiaofeng Zhao
Shanghai Key Laboratory of advanced High-temperature Materials and precision Forming, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
1 shared publication
Latest Publications
- Open Access
Effects of Al2O3 Particle Size on Multi-Mode Erosion Failure Mechanisms of EB-PVD YSZ Thermal Barrier Coatings Under Simulated Aero-Engine Conditions
To investigate the influence of particle size on the erosion damage behavior and failure mechanisms of thermal barrier coatings (TBCs) in a simulated aero-engine erosion environment, erosion tests were conducted using Al2O3 particles of different sizes (65 μm, 120 μm, and 175 μm) under a nominal gas-flow condition of Mach 0.4 at 1150 °C with custom-built multi-factor coupled erosion test equipment. TBCs were prepared using electron beam physical vapor deposition (EB-PVD). By combining macroscopic/microscopic morphology, composition, white-light interferometry, and Raman residual stress testing, the damage evolution and failure behavior of TBCs under different particle size conditions were analyzed. The results indicate that particle size has a significant effect on the erosion behavior of thermal barrier coatings. Under erosion conditions involving 65, 120, and 175 μm particles, the erosion rates were 10.83, 4.19, and 2.05 g/kg, with corresponding coating lifetimes of approximately 3, 12, and 22 h. As particle size increases, the erosion rate decreases and the coating lifetime increases. Under small 65 μm particles, the coating exhibits high-frequency continuous micro-cutting. The ceramic layer rapidly thins, leading to localized penetration. Under erosion by 120 μm particles, the coating exhibits a composite damage mechanism involving cutting, compaction, and brittle fracture. Under large-particle impacts of 175 μm, the damage mechanism is dominated by localized brittle fracture and spalling induced by high-energy impacts. Although the single-impact energy of large-particle impacts is higher, the lower particle number density results in a discrete distribution of damage zones, leading to a lower material removal rate. The Raman test results further indicate that, after 2 h of erosion, the differences in residual stress in the TGO layer were relatively small across different particle size conditions, suggesting that the early degradation process of the coating is primarily controlled by the mechanical removal of the ceramic surface layer rather than by the evolution of TGO stress. No statistically significant difference in TGO residual stress was observed among different particle sizes after 2 h of erosion (p > 0.05). Not only is the erosion life of EB-PVD YSZ TBCs is influenced by the impact energy of individual particles, but more importantly, it is also closely related to particle number density, impact frequency, and the spatial distribution of damage.
Open AccessEffects of Al2O3 Particle Size on Multi-Mode Erosion Failure Mechanisms of EB-PVD YSZ Thermal Barrier Coatings Under Simulated Aero-Engine Conditions
To investigate the influence of particle size on the erosion damage behavior and failure mechanisms of thermal barrier coatings (TBCs) in a simulated aero-engine erosion environment, erosion tests were conducted using Al2O3 particles of different sizes (65 μm, 120 μm, and 175 μm) under a nominal gas-flow condition of Mach 0.4 at 1150 °C with custom-built multi-factor coupled erosion test equipment. TBCs were prepared using electron beam physical vapor deposition (EB-PVD). By combining macroscopic/microscopic morphology, composition, white-light interferometry, and Raman residual stress testing, the damage evolution and failure behavior of TBCs under different particle size conditions were analyzed. The results indicate that particle size has a significant effect on the erosion behavior of thermal barrier coatings. Under erosion conditions involving 65, 120, and 175 μm particles, the erosion rates were 10.83, 4.19, and 2.05 g/kg, with corresponding coating lifetimes of approximately 3, 12, and 22 h. As particle size increases, the erosion rate decreases and the coating lifetime increases. Under small 65 μm particles, the coating exhibits high-frequency continuous micro-cutting. The ceramic layer rapidly thins, leading to localized penetration. Under erosion by 120 μm particles, the coating exhibits a composite damage mechanism involving cutting, compaction, and brittle fracture. Under large-particle impacts of 175 μm, the damage mechanism is dominated by localized brittle fracture and spalling induced by high-energy impacts. Although the single-impact energy of large-particle impacts is higher, the lower particle number density results in a discrete distribution of damage zones, leading to a lower material removal rate. The Raman test results further indicate that, after 2 h of erosion, the differences in residual stress in the TGO layer were relatively small across different particle size conditions, suggesting that the early degradation process of the coating is primarily controlled by the mechanical removal of the ceramic surface layer rather than by the evolution of TGO stress. No statistically significant difference in TGO residual stress was observed among different particle sizes after 2 h of erosion (p > 0.05). Not only is the erosion life of EB-PVD YSZ TBCs is influenced by the impact energy of individual particles, but more importantly, it is also closely related to particle number density, impact frequency, and the spatial distribution of damage.
- Open Access
Failure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment
To simulate the erosion damage behavior of thermal barrier coatings (TBCs) under actual service conditions in an aircraft engine environment, this study developed a multi-factor coupled test setup capable of simulating combined loading under high-temperature (1150 °C), high-speed (0.4 Mach), and solid-particle erosion conditions. Yttria-stabilized zirconia (YSZ) TBCs were prepared using electron beam physical vapor deposition (EB-PVD). For different erosion durations (2 h, 5 h, 8 h, 12 h), the evolution of macroscopic and microscopic morphologies as well as the development of residual stresses in the thermally grown oxide (TGO) layer were systematically investigated. The results indicate that the erosion process of the YSZ coating can be divided into three stages. During the initial high-erosion-rate stage (8.17 g/kg), erosion damage was confined to the grain tips of the columnar crystals, primarily caused by brittle fracture at the grain tips, and the TGO stress was relatively low (−0.6 GPa). During the intermediate stage, the erosion rate was lower (2.74 g/kg). Impact stresses induced microcracks within the columnar grains, which gradually connected to form intergranular fractures. This led to the expansion of localized spalling pits. The interface began to wrinkle, and the stress rose to −2.2 GPa. In the final accelerated failure stage (5.88 g/kg), horizontal cracks fully propagated, leading to large-scale peeling of the coating. The stress was released to −0.9 GPa. The coating failure mechanism evolves from surface damage to interfacial peeling, which is closely related to the coating structure, stress evolution, and interfacial state.
Open AccessFailure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment
To simulate the erosion damage behavior of thermal barrier coatings (TBCs) under actual service conditions in an aircraft engine environment, this study developed a multi-factor coupled test setup capable of simulating combined loading under high-temperature (1150 °C), high-speed (0.4 Mach), and solid-particle erosion conditions. Yttria-stabilized zirconia (YSZ) TBCs were prepared using electron beam physical vapor deposition (EB-PVD). For different erosion durations (2 h, 5 h, 8 h, 12 h), the evolution of macroscopic and microscopic morphologies as well as the development of residual stresses in the thermally grown oxide (TGO) layer were systematically investigated. The results indicate that the erosion process of the YSZ coating can be divided into three stages. During the initial high-erosion-rate stage (8.17 g/kg), erosion damage was confined to the grain tips of the columnar crystals, primarily caused by brittle fracture at the grain tips, and the TGO stress was relatively low (−0.6 GPa). During the intermediate stage, the erosion rate was lower (2.74 g/kg). Impact stresses induced microcracks within the columnar grains, which gradually connected to form intergranular fractures. This led to the expansion of localized spalling pits. The interface began to wrinkle, and the stress rose to −2.2 GPa. In the final accelerated failure stage (5.88 g/kg), horizontal cracks fully propagated, leading to large-scale peeling of the coating. The stress was released to −0.9 GPa. The coating failure mechanism evolves from surface damage to interfacial peeling, which is closely related to the coating structure, stress evolution, and interfacial state.