Haodong He
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Haodong He has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Chitengfei Zhang
Hubei Longzhong Laboratory, Xiangyang 441000, China
1 shared publication - Gao Tenghua
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China
1 shared publication - Jiangxin Yang
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China
1 shared publication - Lianmeng Zhang
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China
1 shared publication - Qingfang Xu
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China
1 shared publication - Rong Tu
Wuhan University of Technology
1 shared publication
Latest Publications
- Open Access
Deposition Temperature-Driven Structural Evolution and Wet-Oxygen Corrosion Behavior of a-SiOC Coatings on Optical Fibers
Optical fiber sensors deployed in harsh industrial fields, e.g., high-temperature wet-oxygen, face severe challenges in signal attenuation and mechanical degradation. While amorphous silicon oxycarbide (a-SiOC) coatings offer a promising solution due to their adjustable thermo-mechanical properties, balancing their structural density with environmental stability remains a critical technical bottleneck. In this study, a-SiOC coatings were deposited on optical fibers using hexamethyldisilane (HMDS) and trace oxygen via radio-frequency capacitively coupled plasma-enhanced chemical vapor deposition (PECVD). A systematic investigation was conducted to determine the impact of deposition temperature (70–420 °C) on the precursor dissociation kinetics, microstructural evolution, and corrosion resistance of the coatings. An elevation in temperature promotes the elimination of organic terminal groups (–CH3, –H) and enhances surface diffusion, driving the coating from a loose, carbon-rich “polymer-like” structure (dominated by Si–C bonds) to a dense, inorganic “silica-like” skeleton (dominated by Si–O–Si bonds). High-temperature corrosion tests in a wet-oxygen environment (500–900 °C) demonstrate that the failure mechanism is highly dependent on deposition temperature. Coatings deposited at low temperatures suffer catastrophic cracking due to pronounced oxidative shrinkage and the release of volatile species, whereas coatings deposited at 420 °C exhibit microcracking caused by severe carbon phase separation and stress concentration within the rigid inorganic network. In the present system, 350 °C is identified as the optimal deposition temperature, as it achieves the best balance of network densification and structural flexibility, while exhibiting the best mechanical performance.
Open AccessDeposition Temperature-Driven Structural Evolution and Wet-Oxygen Corrosion Behavior of a-SiOC Coatings on Optical Fibers
Optical fiber sensors deployed in harsh industrial fields, e.g., high-temperature wet-oxygen, face severe challenges in signal attenuation and mechanical degradation. While amorphous silicon oxycarbide (a-SiOC) coatings offer a promising solution due to their adjustable thermo-mechanical properties, balancing their structural density with environmental stability remains a critical technical bottleneck. In this study, a-SiOC coatings were deposited on optical fibers using hexamethyldisilane (HMDS) and trace oxygen via radio-frequency capacitively coupled plasma-enhanced chemical vapor deposition (PECVD). A systematic investigation was conducted to determine the impact of deposition temperature (70–420 °C) on the precursor dissociation kinetics, microstructural evolution, and corrosion resistance of the coatings. An elevation in temperature promotes the elimination of organic terminal groups (–CH3, –H) and enhances surface diffusion, driving the coating from a loose, carbon-rich “polymer-like” structure (dominated by Si–C bonds) to a dense, inorganic “silica-like” skeleton (dominated by Si–O–Si bonds). High-temperature corrosion tests in a wet-oxygen environment (500–900 °C) demonstrate that the failure mechanism is highly dependent on deposition temperature. Coatings deposited at low temperatures suffer catastrophic cracking due to pronounced oxidative shrinkage and the release of volatile species, whereas coatings deposited at 420 °C exhibit microcracking caused by severe carbon phase separation and stress concentration within the rigid inorganic network. In the present system, 350 °C is identified as the optimal deposition temperature, as it achieves the best balance of network densification and structural flexibility, while exhibiting the best mechanical performance.