Mingzhe Fan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Mingzhe Fan has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Guanzhen Zhang
Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China
2 shared publications - Xiang Li
Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China
2 shared publications - Chi Zhang
Key Laboratory for Advanced Materials of Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing, China
1 shared publication - Guang Li
Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China
1 shared publication - Guang Li
Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China
1 shared publication - Pengtao Liu
School of Materials Science and Engineering, Dalian Jiaotong University, Dalian 116028, China
1 shared publication
Latest Publications
- Open Access
Microstructural Evolution of Pearlitic Wheel Steel Under Thermal–Mechanical Fatigue
Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.
Open AccessMicrostructural Evolution of Pearlitic Wheel Steel Under Thermal–Mechanical Fatigue
Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.
- Open Access
Experimental Investigation of Microstructural Evolution and Fatigue Damage of Pearlite Wheel Steel During Tread Braking Based on a Full-Size Wheel–Rail Test Rig
This study investigated the relationship between the surface microstructure of pearlite steel wheels and the formation of fatigue cracks during the braking process by using a full-size wheel braking test rig. After fatigue failure, the surface microstructural evolution and fatigue crack initiation and propagation of the wheel sample were systematically analyzed by optical microscope (OM), scanning electron microscope (SEM), and transmission electron microscope (TEM). The results showed that after braking of 1572 cycles, a large number of fatigue cracks formed at the wheel tread, which caused the wheel to break. After fatigue failure, some dark areas formed at the wheel tread, which were composed of Fe3O4 compounds. This indicates that severe oxidation was produced at the wheel tread during braking due to the high temperature. After fatigue failure, a continuous thermal white etching layer (T-WEL) was formed in some areas of the wheel tread, while crescent-shaped T-WEL was found in other areas. The microstructure of the T-WEL was composed of martensite phase. The rapid increase and decrease in temperature at the wheel tread during the braking process caused martensitic transformation at the wheel tread. The hardness of the sample reached to about 900 HV in WEL and it reduced with the increase in distance from the surface. The cracks were initiated from the surface and gradually propagated into the matrix. However, the crack propagation mode in the continuous T-WEL and crescent-shaped T-WEL was different. In the continuous T-WEL, the continuous T-WEL of the wheel can be peeled off during the braking wear process, and then the crack was gradually propagated into the matrix in the T-WEL peeled area. As for the crescent-shaped T-WEL, due to the large hardness difference between T-WEL and pearlite, the crack initiated at the interface between the T-WEL and pearlite and gradually propagated into the matrix.
Open AccessExperimental Investigation of Microstructural Evolution and Fatigue Damage of Pearlite Wheel Steel During Tread Braking Based on a Full-Size Wheel–Rail Test Rig
This study investigated the relationship between the surface microstructure of pearlite steel wheels and the formation of fatigue cracks during the braking process by using a full-size wheel braking test rig. After fatigue failure, the surface microstructural evolution and fatigue crack initiation and propagation of the wheel sample were systematically analyzed by optical microscope (OM), scanning electron microscope (SEM), and transmission electron microscope (TEM). The results showed that after braking of 1572 cycles, a large number of fatigue cracks formed at the wheel tread, which caused the wheel to break. After fatigue failure, some dark areas formed at the wheel tread, which were composed of Fe3O4 compounds. This indicates that severe oxidation was produced at the wheel tread during braking due to the high temperature. After fatigue failure, a continuous thermal white etching layer (T-WEL) was formed in some areas of the wheel tread, while crescent-shaped T-WEL was found in other areas. The microstructure of the T-WEL was composed of martensite phase. The rapid increase and decrease in temperature at the wheel tread during the braking process caused martensitic transformation at the wheel tread. The hardness of the sample reached to about 900 HV in WEL and it reduced with the increase in distance from the surface. The cracks were initiated from the surface and gradually propagated into the matrix. However, the crack propagation mode in the continuous T-WEL and crescent-shaped T-WEL was different. In the continuous T-WEL, the continuous T-WEL of the wheel can be peeled off during the braking wear process, and then the crack was gradually propagated into the matrix in the T-WEL peeled area. As for the crescent-shaped T-WEL, due to the large hardness difference between T-WEL and pearlite, the crack initiated at the interface between the T-WEL and pearlite and gradually propagated into the matrix.