Rui Deng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Rui Deng has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Haoyu Cai
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, 30th Xueyuan Road, Haidian district, Beijing 100083, China
1 shared publication - Jianliang Zhang
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing, PR China
1 shared publication - Jixiang Han
China Sinosteel Equipment and Engineering Co., Ltd., Beijing 100080, China
1 shared publication - Yaozu Wang
School of Intelligence Science and Technology, University of Science and Technology Beijing, Beijing, P.R. China
1 shared publication - Zhengjian Liu
School of Metallurgical and Ecological Engineering University of Science and Technology Beijing 30th Xueyuan Road Haidian district Beijing 100083 P. R. China
1 shared publication
Latest Publications
- Open Access
Effect of Basicity on Consolidation Behavior and Phase Evolution of Mg-Bearing Medium Silica Fluxed Pellets
Against the background of blast furnace burden optimization and the low-carbon transition of the steel industry, the development of high-quality Mg-bearing fluxed pellets is of great significance for the efficient utilization of medium-high silica iron ore concentrates. In this study, Mg-bearing medium-high silica fluxed pellets with a fixed SiO2 content of 5.5% were prepared, and the effect of basicity in the range of R = 1.0–1.4 on compressive strength, liquid phase behavior, slag phase composition, and pore structure evolution was systematically investigated. The results showed that the compressive strength of the pellets decreased from 2527 N/pellet to 2079 N/pellet as the basicity increased from 1.0 to 1.4. At 1250 °C, the liquid phase content first decreased from 2.66% to 1.30% and then increased to 7.38%, while the liquid phase viscosity decreased continuously. Meanwhile, the liquid phase composition evolved from a SiO2-rich calcium–iron silicate system to a Fe2O3− and CaO-rich system. XRD results indicated that Fe2O3 was the dominant crystalline phase in the pellets, accompanied by a small amount of Fe3O4, whereas no distinct highly crystalline slag phase was detected. The slag phase was mainly a Fe-Ca-Si composite slag, in which the Fe2O3 content increased and the SiO2 content decreased with increasing basicity. At higher basicity, the number and size of pores increased, and the pore morphology evolved from dispersed fine pores to irregular large pores and locally connected pores. Meanwhile, the slag phase became more widely distributed and locally enriched, weakening the continuity of the iron oxide load-bearing skeleton, which was the main reason for the decrease in compressive strength. This study provides a theoretical basis for preparing high-quality Mg-bearing fluxed pellets from medium-high silica iron ore concentrates.
Open AccessEffect of Basicity on Consolidation Behavior and Phase Evolution of Mg-Bearing Medium Silica Fluxed Pellets
Against the background of blast furnace burden optimization and the low-carbon transition of the steel industry, the development of high-quality Mg-bearing fluxed pellets is of great significance for the efficient utilization of medium-high silica iron ore concentrates. In this study, Mg-bearing medium-high silica fluxed pellets with a fixed SiO2 content of 5.5% were prepared, and the effect of basicity in the range of R = 1.0–1.4 on compressive strength, liquid phase behavior, slag phase composition, and pore structure evolution was systematically investigated. The results showed that the compressive strength of the pellets decreased from 2527 N/pellet to 2079 N/pellet as the basicity increased from 1.0 to 1.4. At 1250 °C, the liquid phase content first decreased from 2.66% to 1.30% and then increased to 7.38%, while the liquid phase viscosity decreased continuously. Meanwhile, the liquid phase composition evolved from a SiO2-rich calcium–iron silicate system to a Fe2O3− and CaO-rich system. XRD results indicated that Fe2O3 was the dominant crystalline phase in the pellets, accompanied by a small amount of Fe3O4, whereas no distinct highly crystalline slag phase was detected. The slag phase was mainly a Fe-Ca-Si composite slag, in which the Fe2O3 content increased and the SiO2 content decreased with increasing basicity. At higher basicity, the number and size of pores increased, and the pore morphology evolved from dispersed fine pores to irregular large pores and locally connected pores. Meanwhile, the slag phase became more widely distributed and locally enriched, weakening the continuity of the iron oxide load-bearing skeleton, which was the main reason for the decrease in compressive strength. This study provides a theoretical basis for preparing high-quality Mg-bearing fluxed pellets from medium-high silica iron ore concentrates.