Shubha Sarmalkar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shubha Sarmalkar has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Aradhana Nagarsekar
Department of Prosthodontics Goa Dental College and Hospital Bambolim India
1 shared publication - Meena Ajay Aras
Department of Prosthodontics Goa Dental College and Hospital Bambolim India
1 shared publication - Prajakta Raghudas Volvaikar
Department of Prosthodontics Goa Dental College and Hospital Bambolim India
1 shared publication - Ridhima Gaunkar
Department of Public Health Dentistry Goa Dental College and Hospital Bambolim Goa India
1 shared publication - Umesh Yeshwanth Pai
Department of Prosthodontics and Crown & Bridge, Manipal College of Dental Sciences Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, 576104
1 shared publication
Latest Publications
- Open Access
- 14 July 2026
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 38 (11) , 2199-2206
Effect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study
Objective: To evaluate the effect of glazing dwell time and cooling duration on the flexural strength and surface microhardness of high‐translucency 3 mol% yttria‐stabilized tetragonal zirconia polycrystal (3Y‐TZP). Materials and Methods: Total of 108 rectangular zirconia specimens (20 × 4 × 2 mm) were fabricated from preshaded monolithic blocks and sintered at 1530°C. Specimens were divided into nine groups ( n = 12). The control group (NG) remained unglazed. Experimental groups underwent conventional firing (CF;1‐min dwell) or extended firing (EF; 3‐min dwell) at 850°C, each combined with four cooling durations (4,7,9, or 12 min) between 850°C and 600°C. Flexural strength was evaluated using a four‐point bending test (ISO 6872:2015) with Weibull analysis, while surface microhardness was measured using the Vickers method (50 g, 10 s). Data were analyzed using two‐way ANOVA and Tukey's HSD test ( α = 0.05). Results: Significant differences were observed in flexural strength and microhardness ( p < 0.001). The unglazed group showed the highest strength (698 ± 18 MPa; m = 46). Among glazed groups, EF3 (3‐min dwell/9‐min cooling) exhibited the highest characteristic strength ( σ ₀ = 657 MPa). EF1 (3‐min dwell/4‐min cooling) showed the lowest strength (466 ± 23 MPa), below ISO requirements. Microhardness decreased with longer cooling durations. Conclusions: Glazing parameters significantly affect 3Y‐TZP properties. Extended firing with controlled slow cooling (9 min) optimizes strength and reliability, while rapid cooling compromises performance.
- 14 July 2026
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 38 (11) , 2199-2206
Open AccessEffect of Glazing Dwell Time and Cooling Duration on Flexural Strength and Surface Microhardness of 3 mol% Yttria‐Stabilized Tetragonal Zirconia: An In Vitro Study
Objective: To evaluate the effect of glazing dwell time and cooling duration on the flexural strength and surface microhardness of high‐translucency 3 mol% yttria‐stabilized tetragonal zirconia polycrystal (3Y‐TZP). Materials and Methods: Total of 108 rectangular zirconia specimens (20 × 4 × 2 mm) were fabricated from preshaded monolithic blocks and sintered at 1530°C. Specimens were divided into nine groups ( n = 12). The control group (NG) remained unglazed. Experimental groups underwent conventional firing (CF;1‐min dwell) or extended firing (EF; 3‐min dwell) at 850°C, each combined with four cooling durations (4,7,9, or 12 min) between 850°C and 600°C. Flexural strength was evaluated using a four‐point bending test (ISO 6872:2015) with Weibull analysis, while surface microhardness was measured using the Vickers method (50 g, 10 s). Data were analyzed using two‐way ANOVA and Tukey's HSD test ( α = 0.05). Results: Significant differences were observed in flexural strength and microhardness ( p < 0.001). The unglazed group showed the highest strength (698 ± 18 MPa; m = 46). Among glazed groups, EF3 (3‐min dwell/9‐min cooling) exhibited the highest characteristic strength ( σ ₀ = 657 MPa). EF1 (3‐min dwell/4‐min cooling) showed the lowest strength (466 ± 23 MPa), below ISO requirements. Microhardness decreased with longer cooling durations. Conclusions: Glazing parameters significantly affect 3Y‐TZP properties. Extended firing with controlled slow cooling (9 min) optimizes strength and reliability, while rapid cooling compromises performance.