Bingtao Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Bingtao Li has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Ang Li
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Guohao Liu
Research Institute of Advanced Materials (Shenzhen) Co., Ltd., Shenzhen 518045, China
1 shared publication - Hongyao Yu
Gaona Aero Material Co., Ltd., Beijing 100081, China
1 shared publication - Huadong Fu
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Wenhan Wang
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Yunwei Gui
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication
Latest Publications
- Open Access
Effect of Minor P and C Regulation on Microstructure Evolution and High-Temperature Properties of Selective Laser Melted GH4169 Superalloy
Selective laser melting (SLM) produces elemental segregation and nonequilibrium secondary phases in GH4169 superalloys, but the effects of P and C variations on grain-boundary phase evolution and high-temperature tensile behavior remain unclear. Alloys with primarily varied P (0.034–0.058 wt.%) and C (0.009–0.066 wt.%) contents were fabricated and heat treated identically. Microstructures were characterized by scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM), and tensile properties were evaluated at 650 °C. The as-built alloys exhibited columnar grains, cellular substructures, cell-wall segregation, and Nb-rich Laves-phase particles. After heat treatment, cellular substructures largely disappeared, γ″ precipitates formed in the γ matrix, and fine Ti/Al-rich particles were tentatively attributed to γ′; δ phase, residual Laves phase, and MC-type carbides were present at grain boundaries. Increasing P reduced the δ-phase area fraction from 2.20% to 1.38% and changed its distribution from continuous chains to semi-continuous and discrete arrangements. Increasing C raised the MC-type carbide area fraction from 0.34% to 1.48% while decreasing the δ-phase area fraction from 1.68% to 0.98%, accompanied by carbide coarsening. The 0.050P alloy exhibited the highest yield and ultimate tensile strengths, whereas the 0.009C alloy showed the best strength–ductility balance. These results reveal distinct P- and C-related changes in grain-boundary phase evolution and tensile behavior at 650 °C.
Open AccessEffect of Minor P and C Regulation on Microstructure Evolution and High-Temperature Properties of Selective Laser Melted GH4169 Superalloy
Selective laser melting (SLM) produces elemental segregation and nonequilibrium secondary phases in GH4169 superalloys, but the effects of P and C variations on grain-boundary phase evolution and high-temperature tensile behavior remain unclear. Alloys with primarily varied P (0.034–0.058 wt.%) and C (0.009–0.066 wt.%) contents were fabricated and heat treated identically. Microstructures were characterized by scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM), and tensile properties were evaluated at 650 °C. The as-built alloys exhibited columnar grains, cellular substructures, cell-wall segregation, and Nb-rich Laves-phase particles. After heat treatment, cellular substructures largely disappeared, γ″ precipitates formed in the γ matrix, and fine Ti/Al-rich particles were tentatively attributed to γ′; δ phase, residual Laves phase, and MC-type carbides were present at grain boundaries. Increasing P reduced the δ-phase area fraction from 2.20% to 1.38% and changed its distribution from continuous chains to semi-continuous and discrete arrangements. Increasing C raised the MC-type carbide area fraction from 0.34% to 1.48% while decreasing the δ-phase area fraction from 1.68% to 0.98%, accompanied by carbide coarsening. The 0.050P alloy exhibited the highest yield and ultimate tensile strengths, whereas the 0.009C alloy showed the best strength–ductility balance. These results reveal distinct P- and C-related changes in grain-boundary phase evolution and tensile behavior at 650 °C.