Yonghua Han
Research Subjects
Yonghua Han has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Honghui Liu
Key Laboratory of Green and High-End Utilization of Salt Lake Resources, Key Laboratory of Salt Lake Resources Chemistry of Qinghai Province, Qinghai Institute of Salt Lakes, Chinese Academy of Sciences, Xining 810008, China
1 shared publication - Hongyan Kang
AECC Harbin Dongan Engine Co., Ltd., Harbin 150066, China
1 shared publication - Jingya Cui
Qinghai Provincial Key Laboratory of Nanomaterials and Technology, School of Chemistry and Materials Science, Qinghai Minzu University, Xining 810007, China
1 shared publication - Jinhui Wang
Qinghai Provincial Key Laboratory of New Light Alloys, Qinghai Provincial Engineering Research Center of High-Performance Light Metal Alloys and Forming, Qinghai University, Xining 810016, China
1 shared publication - Tong Mu
Key Laboratory of Green and High-End Utilization of Salt Lake Resources, Key Laboratory of Salt Lake Resources Chemistry of Qinghai Province, Qinghai Institute of Salt Lakes, Chinese Academy of Sciences, Xining 810008, China
1 shared publication - Xiaoming Wang
AECC Harbin Dongan Engine Co., Ltd., Harbin 150066, China
1 shared publication
Latest Publications
- Open Access
Effect of Sr Microalloying on the Microstructure, Solution-Treatment Response, and Age-Hardening Behavior of Mg-Nd-Gd-Zn-Zr Alloy
Mg-Nd-Gd-Zn-Zr alloys containing 0, 0.20, and 0.75 wt.% Sr were prepared by gravity casting to investigate the effects of Sr microalloying on as-cast microstructure, solution-treatment response, and age-hardening behavior. The alloys were characterized by XRD, OM, SEM/EDS, DSC, and Brinell hardness testing. Sr was mainly enriched at grain boundaries and in secondary-phase regions, and Mg17Sr2-related diffraction peaks appeared in the Sr-containing alloys. The as-cast grain size varied non-monotonically among the three compositions investigated, with the 0.20 wt.% Sr alloy exhibiting the finest grains, whereas the area fraction of secondary phases increased continuously with Sr content. Under the selected solution-treatment conditions, the Sr-containing alloys retained smaller grains but contained larger amounts of residual secondary phases. Under the respective selected solution-treated starting states, the 0Sr alloy achieved the highest measured hardness at 200 °C, while the 0.20Sr alloy showed an earlier hardening response and a more gradual subsequent hardness evolution; the 0.75Sr alloy showed a more pronounced post-peak hardness decrease. The retained Sr-containing secondary phases may indicate incomplete dissolution of part of the Nd, Gd, and Zn, potentially reducing the effective solute reservoir in α-Mg available for subsequent aging. Within the three compositions investigated, the results indicate a trade-off between grain refinement/retention and age-hardening potential.
Open AccessEffect of Sr Microalloying on the Microstructure, Solution-Treatment Response, and Age-Hardening Behavior of Mg-Nd-Gd-Zn-Zr Alloy
Mg-Nd-Gd-Zn-Zr alloys containing 0, 0.20, and 0.75 wt.% Sr were prepared by gravity casting to investigate the effects of Sr microalloying on as-cast microstructure, solution-treatment response, and age-hardening behavior. The alloys were characterized by XRD, OM, SEM/EDS, DSC, and Brinell hardness testing. Sr was mainly enriched at grain boundaries and in secondary-phase regions, and Mg17Sr2-related diffraction peaks appeared in the Sr-containing alloys. The as-cast grain size varied non-monotonically among the three compositions investigated, with the 0.20 wt.% Sr alloy exhibiting the finest grains, whereas the area fraction of secondary phases increased continuously with Sr content. Under the selected solution-treatment conditions, the Sr-containing alloys retained smaller grains but contained larger amounts of residual secondary phases. Under the respective selected solution-treated starting states, the 0Sr alloy achieved the highest measured hardness at 200 °C, while the 0.20Sr alloy showed an earlier hardening response and a more gradual subsequent hardness evolution; the 0.75Sr alloy showed a more pronounced post-peak hardness decrease. The retained Sr-containing secondary phases may indicate incomplete dissolution of part of the Nd, Gd, and Zn, potentially reducing the effective solute reservoir in α-Mg available for subsequent aging. Within the three compositions investigated, the results indicate a trade-off between grain refinement/retention and age-hardening potential.