This study evaluated how the polymerization mechanism affects depth-dependent microhardness and shear bond strength to primary molar dentin. Three materials were tested: a conventional light-cured flowable composite, a light-cured bulk-fill composite and a self-cured bulk-fill composite. Each material was placed as a single increment, and Vickers microhardness was measured at 2.0, 3.0, and 4.0 mm (n = 10 per group). For shear bond strength testing, forty primary molars were assigned to four bonding groups (n = 10): the two light-cured composites were bonded with a universal adhesive, and the self-cured composite with either the universal adhesive combined with a dual cure activator or its dedicated primer. The interaction between material and depth was significant: microhardness decreased substantially with depth in the conventional composite, whereas the decrease was smaller in both bulk-fill materials and did not differ between them. Shear bond strength differed significantly among the groups (p < 0.0001), being highest in the self-cured composite with its dedicated primer (median 20.4 MPa) and lowest for the conventional composite (8.9 MPa), while the light-cured bulk-fill composite and the self-cured composite with the universal adhesive did not differ. Within the limitations of this study, the microhardness of the self-cured composite appeared less dependent on depth than that of the conventional composite and comparable with that of the lightcured bulk-fill composite, and its bond strength depended on the adhesive system used. This material may be of interest for restorations of primary molars in which light delivery is limited.