Comparison of Thermal and Plasma-Enhanced ALD/CVD of Vanadium Pentoxide

Authors:

Abstract
Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to 200°C200°C . Above 200°C200°C , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using H2OH2O or O2O2 . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or O2O2 atmosphere. Films grown with CVD at 300°C300°C and PE O2O2 ALD at 150°C150°C were (001)-oriented V2O5V2O5 as deposited, while thermal and PE H2OH2O ALD films grown at 150°C150°C were amorphous as deposited. The crystallinity of the PE O2O2 ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into V2O5V2O5 under O2O2 .

This publication has 24 references indexed in Scilit: