J. Musschoot
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
J. Musschoot has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
J. Haemers
Department of Solid State Sciences, Ghent University, Krijgslaan 281/S1, B-9000 Ghent, Belgium
4 shared publications- Christophe Detavernier
Ghent University
3 shared publications D. Deduytsche
Department of Solid State Sciences, Ghent University, Krijgslaan 281/S1, B-9000 Ghent, Belgium
3 shared publicationsH. Poelman
Department of Solid State Sciences, Ghent University, Krijgslaan 281/S1, B-9000 Ghent, Belgium
2 shared publications- Sven Van Den Berghe
European committee for standardization
2 shared publications D. Longrie
Department of Solid State Sciences, Ghent University, Krijgslaan 281/S1, B-9000 Gent, Belgium
1 shared publication
Latest Publications
- 1 January 2010
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 157 (4) , G111-P126
Conformality of Al[sub 2]O[sub 3] and AlN Deposited by Plasma-Enhanced Atomic Layer Deposition
Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to 200°C200°C . Above 200°C200°C , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using H2OH2O or O2O2 . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or O2O2 atmosphere. Films grown with CVD at 300°C300°C and PE O2O2 ALD at 150°C150°C were (001)-oriented V2O5V2O5 as deposited, while thermal and PE H2OH2O ALD films grown at 150°C150°C were amorphous as deposited. The crystallinity of the PE O2O2 ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into V2O5V2O5 under O2O2 .
- 1 January 2010
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 157 (4) , G111-P126
Conformality of Al[sub 2]O[sub 3] and AlN Deposited by Plasma-Enhanced Atomic Layer Deposition
Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to 200°C200°C . Above 200°C200°C , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using H2OH2O or O2O2 . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or O2O2 atmosphere. Films grown with CVD at 300°C300°C and PE O2O2 ALD at 150°C150°C were (001)-oriented V2O5V2O5 as deposited, while thermal and PE H2OH2O ALD films grown at 150°C150°C were amorphous as deposited. The crystallinity of the PE O2O2 ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into V2O5V2O5 under O2O2 .
- 11 November 2009
- Published by Elsevier in Microelectronic Engineering
- Vol. 87 (10) , 1879-1883
Texture of atomic layer deposited ruthenium
- 11 November 2009
- Published by Elsevier in Microelectronic Engineering
- Vol. 87 (10) , 1879-1883
Texture of atomic layer deposited ruthenium
- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (7) , P122-P126
Comparison of Thermal and Plasma-Enhanced ALD/CVD of Vanadium Pentoxide
Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to 200°C200°C . Above 200°C200°C , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using H2OH2O or O2O2 . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or O2O2 atmosphere. Films grown with CVD at 300°C300°C and PE O2O2 ALD at 150°C150°C were (001)-oriented V2O5V2O5 as deposited, while thermal and PE H2OH2O ALD films grown at 150°C150°C were amorphous as deposited. The crystallinity of the PE O2O2 ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into V2O5V2O5 under O2O2 .
- 1 January 2009
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 156 (7) , P122-P126
Comparison of Thermal and Plasma-Enhanced ALD/CVD of Vanadium Pentoxide
Vanadium pentoxide was deposited by atomic layer deposition (ALD) from vanadyl-tri-isopropoxide (VTIP). Water or oxygen was used as a reactive gas in thermal and plasma-enhanced (PE) processes. For PE ALD, there was a wide ALD temperature window from 50 to 200°C200°C . Above 200°C200°C , VTIP decomposed thermally, resulting in the chemical vapor deposition (CVD) of vanadium pentoxide. The PE ALD reactions saturated much faster than during thermal ALD, leading to a growth rate of approximately 0.7 Å/cycle during PE ALD using H2OH2O or O2O2 . Optical emission spectroscopy showed combustion-like reactions during the plasma step. X-ray diffraction was performed to determine the crystallinity of the films after deposition and after postannealing under He or O2O2 atmosphere. Films grown with CVD at 300°C300°C and PE O2O2 ALD at 150°C150°C were (001)-oriented V2O5V2O5 as deposited, while thermal and PE H2OH2O ALD films grown at 150°C150°C were amorphous as deposited. The crystallinity of the PE O2O2 ALD could be correlated to its high purity, while the other films had significant carbon contamination, as shown by X-ray photoelectron spectroscopy. Annealing under He led to oxygen-deficient films, while all samples eventually crystallized into V2O5V2O5 under O2O2 .