Estimating the Number of Defects in a Single Breakdown Spot of a Gate Dielectric
- 14 March 2024
- journal article
- research article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 45 (5) , 809-812
Abstract
Conduction Atomic Force Microscopy (CAFM) is used to locally stress a 3.5 nm thick SiO2 film to induce soft dielectric breakdown (SBD). The tip-to-surface adhesion and current-voltage ( I-V ) characteristic at the breakdown location are measured by the CAFM before and after the SBD event. The adhesion force is enhanced after SBD because oxygen ion and charged defects are created at the SBD location during stressing which increases the adhesion via image charge forces. We show that the change in adhesion force, supported by charge transport modeling of the I-V data, can be effectively used to estimate the density and number of defects (~20-30) generated during SBD at a single breakdown spot. The information could be useful to assess the post-breakdown reliability and performance variability of the device.Keywords
This publication has 37 references indexed in Scilit:
- A Review on Dielectric Breakdown in Thin Dielectrics: Silicon Dioxide, High‐k, and Layered DielectricsAdvanced Functional Materials, 2019
- Silicon Oxide (SiOx): A Promising Material for Resistance Switching?Advanced Materials, 2018
- Direct Observations of Nanofilament Evolution in Switching Processes in HfO2‐Based Resistive Random Access Memory by In Situ TEM StudiesAdvanced Materials, 2017
- Nanoscale Transformations in Metastable, Amorphous, Silicon‐Rich SilicaAdvanced Materials, 2016
- Fabrication and characterization of boron-doped nanocrystalline diamond-coated MEMS probesApplied Physics A, 2016
- A simulation framework for modeling charge transport and degradation in high-k stacksJournal of Computational Electronics, 2013
- UHV CAFM characterization of high-k dielectrics: Effect of the technique resolution on the pre- and post-breakdown electrical measurementsMicroelectronics Reliability, 2010
- Force measurements with the atomic force microscope: Technique, interpretation and applicationsSurface Science Reports, 2005
- Breakdown spots of ultra-thin (EOT<1.5nm) HfO2/SiO2 stacks observed with enhanced—CAFMMicroelectronics Reliability, 2005
- A General Equation for Fitting Contact Area and Friction vs Load MeasurementsJournal of Colloid and Interface Science, 1999