Liquid Hydrogen Properties Affecting Fracture Toughness
Open Access
- 31 August 2024
- journal article
- Published by The Korean Welding and Joining Society in Journal of Welding and Joining
- Vol. 42 (4) , 414-427
Abstract
In this study, fracture toughness with the base metal of 9% Ni steel, a cryogenic steel, was evaluated under conditions without hydrogen charging (WO-H) and with hydrogen charging (W-H). Hydrogen charging was performed using an electrochemical cathodic charging method in a electrolyte of 3% NaCl + 0.3% NH4SCN at 19℃ with a current density of 50 A/m². Fracture toughness was assessed at -80℃, -100℃, -130℃, and -160℃ using CTOD (Crack Tip Opening Displacement) tests. The results for WO-H indicated a decrease in fracture toughness values with decreasing temperature, while the results for W-H showed an increase in fracture toughness values as the temperature decreased. In addition, the fracture surfaces and fracture toughness of WO-H and W-H became increasingly similar as the temperature decreased, as observed through scanning electron microscopy (SEM). At -80℃, there was a significant difference in fracture toughness between the WO-H and W-H conditions. WO-H was influenced only by the low temperature, whereas W-H was affected by both low temperature and hydrogen, showing combined effects that led to a decrease in fracture toughness due to hydrogen embrittlement. However, at -160℃, the fracture toughness values for both WO-H and W-H conditions were nearly identical. This suggests that the temperature effect on fracture toughness reduction is greater than hydrogen embrittlement at very low temperatures.Keywords
Funding Information
- Ministry of Education
- National Research Foundation of Korea (2021RIS-002)
This publication has 29 references indexed in Scilit:
- Hydrogen production, storage, utilisation and environmental impacts: a reviewEnvironmental Chemistry Letters, 2021
- Role of Hydrogen and Temperature in Hydrogen Embrittlement of Equimolar CoCrFeMnNi High-entropy AlloyMetals and Materials International, 2020
- Review of Hydrogen Embrittlement in Metals: Hydrogen Diffusion, Hydrogen Characterization, Hydrogen Embrittlement Mechanism and PreventionActa Metallurgica Sinica (English Letters), 2020
- First-Principles Study on Hydrogen Diffusivity in BCC, FCC, and HCP IronMetallurgical and Materials Transactions A, 2018
- Understanding and mitigating hydrogen embrittlement of steels: a review of experimental, modelling and design progress from atomistic to continuumJournal of Materials Science, 2018
- Review of fracture toughness (G, K, J, CTOD, CTOA) testing and standardizationEngineering Fracture Mechanics, 2012
- Hydrogen effects on deformation — Relation between dislocation behavior and the macroscopic stress-strain behaviorScripta Metallurgica et Materialia, 1994
- Hydrogen embrittlement of α titanium: In situ tem studiesActa Metallurgica, 1988
- Hydrogen trapping phenomena in metals with B.C.C. and F.C.C. crystals structures by the desorption thermal analysis techniqueSurface and Coatings Technology, 1986
- A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)Metallurgical Transactions, 1972