Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jeongung Park has a total of 41 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effect of Material Property Factors on the Interfacial Residual Stress Gradient in High-Manganese Steel/STS304 Dissimilar Butt Welds

    by Jeong-Ung Park, Gyubaek An

    Cryogenic high-manganese austenitic steel is used in liquefied natural gas (LNG) storage tanks and has a lower thermal expansion coefficient than other cryogenic steels. Because it is joined to stainless steel in the loading system, dissimilar welding is required. Three-dimensional thermal elastic–plastic finite element analysis and sectioning measurements were performed on 15-mm-thick high-manganese steel/STS304 dissimilar butt welds, and the residual stress was analysed separately in the longitudinal and transverse components. The analysis predicted a steep gradient at the weld metal–STS304 interface 8.5 mm from the weld centre, where the transverse stress falls to about −230 MPa. The longitudinal peak differed from the homogeneous joint by only 77 MPa (−11.7%), within the analysis–measurement deviation (RMSE 103–127 MPa). Of the four properties substituted individually, the expansion coefficient gave the highest reproduction ratio (57.9% on average) and alone reproduced the interfacial compression; substituting all four reproduced the effect almost completely (102.4%). The transverse stress range increased linearly with the expansion mismatch (R2 = 0.978), whereas the longitudinal range did not (R2 = 0.002). Assessment by peak residual stress alone therefore misses the interfacial gradient and the compressive zone specific to dissimilar joints.

  • Open Access

    The Effect of Hydrogen Embrittlement on Fracture Toughness of Cryogenic Steels

    by Junggoo Park, Gyubaek An, Jeongung Park, Daehee Seong, Wonjun Jo

    This study investigates the effect of hydrogen embrittlement on the fracture toughness of 9% Ni steel and STS 316L stainless steel under cryogenic conditions ranging from −80 °C to −253 °C. Hydrogen charging was performed using electrochemical methods, and hydrogen uptake was quantitatively analyzed using thermal desorption spectroscopy (TDS). Fracture toughness was evaluated using crack tip opening displacement (CTOD) testing per ISO 12135, both without hydrogen (WO-H) and with hydrogen (W-H). The results showed a gradual decrease in CTOD values with decreasing temperature in both steels under hydrogen-free conditions, with ductile fracture maintained even at −253 °C. In contrast, hydrogen-charged specimens exhibited significant toughness degradation at intermediate subzero temperatures (−80 °C to −130 °C), particularly in 9% Ni steel due to its BCC crystal structure. However, at −160 °C and below, the effect of hydrogen embrittlement was suppressed mainly owing to the reduced hydrogen diffusivity. Scanning electron microscopy (SEM) analysis confirmed the transition from ductile to brittle fracture with decreasing temperature and hydrogen influences. At −253 °C, fully brittle fracture surfaces were observed in all specimens, confirming that at ultra-low temperatures, fracture behavior is dominated by temperature effects rather than hydrogen. These findings identify a practical temperature limit (approximately −160 °C) below which hydrogen embrittlement becomes negligible, providing critical insights for the design and application of structural materials in hydrogen cryogenic environments.


  • Open Access

    Fracture Toughness Estimate of H-Section Steel for Offshore Structure

    by Gyubaek An, Jiseung Lee, Wonjun Jo, Chiung Sun, Jeongung Park

    In this study, a novel estimating equation based on the WES2808 standard was proposed to predict fracture toughness through the transition temperature of Charpy impact toughness and CTOD (Crack Tip Opening Displacement) fracture toughness. This equation was specifically developed for 460MPa class H-section steel materials used in marine structures, including the base material (BM), heat-affected zone (HAZ), and weld metal (WM). The experimental results confirmed that the proposed estimation equation accurately predicted the fracture toughness across these different material regions. These findings demonstrate the reliability and applicability of the proposed equation in estimated fracture toughness for marine structure materials, thereby contributing to improved safety and performance in harsh environmental conditions.


  • Open Access

    Liquid Hydrogen Properties Affecting Fracture Toughness

    by Daehee Seong, Wonjun Jo, Jisun Roh, Junggoo Park, Jeongung Park, Donghyeon Choi, Gyubaek An

    In this study, fracture toughness with the base metal of 9% Ni steel, a cryogenic steel, was evaluated under conditions without hydrogen charging (WO-H) and with hydrogen charging (W-H). Hydrogen charging was performed using an electrochemical cathodic charging method in a electrolyte of 3% NaCl + 0.3% NH4SCN at 19℃ with a current density of 50 A/m². Fracture toughness was assessed at -80℃, -100℃, -130℃, and -160℃ using CTOD (Crack Tip Opening Displacement) tests. The results for WO-H indicated a decrease in fracture toughness values with decreasing temperature, while the results for W-H showed an increase in fracture toughness values as the temperature decreased. In addition, the fracture surfaces and fracture toughness of WO-H and W-H became increasingly similar as the temperature decreased, as observed through scanning electron microscopy (SEM). At -80℃, there was a significant difference in fracture toughness between the WO-H and W-H conditions. WO-H was influenced only by the low temperature, whereas W-H was affected by both low temperature and hydrogen, showing combined effects that led to a decrease in fracture toughness due to hydrogen embrittlement. However, at -160℃, the fracture toughness values for both WO-H and W-H conditions were nearly identical. This suggests that the temperature effect on fracture toughness reduction is greater than hydrogen embrittlement at very low temperatures.


  • Open Access

    Prediction of Laser Welding Distortion in Cylindrical Shell Structures Using Direct Application of Inherent Strain

    by Ji-Hong Yoon, Young-Soo Yang, Sung-Hoon Kim, Se Hwan Lee, Jeong-Ung Park

    In this study, a simplified analysis method by directly applying inherent strain (DIS) at integration points to predict welding distortion of cylindrical shell structures was suggested. The 3D thermo-elastoplastic method demands substantial computational time. The strain as direct boundary (SDB) simplified method using virtual temperature encounters challenges in consecutive thermal structural analysis including welding distortion. The suggested method (that is, DIS) offers the advantage of enabling continuous thermal structural analysis after welding distortion analysis, with computational efficiency. To calculate inherent strain, lap laser welding with 2 mm and 2.6 mm SUS304 plates was performed, measuring fusion and heat-affected zone sizes via cross-sectional observations. Using the calculated inherent strain and our suggested direct input method, we conducted welding analysis and welding test on cylindrical shell structures. Comparison of welding distortion under same conditions revealed radial distortion difference within approximately 10%, corresponding with the experimental result and confirming a computational time reduction by over 2,000 times than those of thermo-elastoplastic analysis. Therefore, an efficient and accurate prediction of welding distortion was achievable through the suggested method.

  • Open Access

    Brittle Crack Arrest Temperature Estimation Method Utilizing a Small-Scale Test with a Thick Steel Plate for Shipbuilding

    by Gyubaek An, Jeongung Park, Daehee Seong, Junseok Seo

    As the shipbuilding industry has emerged from an extended recession, orders for high-value-added ships, such as LNG and ultra-large container ships, are increasing. For ultra-large container ships, high-strength, thick materials are applied. Because the possibility of brittle fracture increases owing to the application of thick steel plates, the related regulations of the International Association of Classification Societies have been strengthened to prevent brittle fracture. To secure brittle fracture stability, it is necessary to secure crack arrest toughness (Kca) through large ESSO experiments or to secure a crack arrest temperature (CAT) value. Because large-scale experiments require considerable costs and efforts, efforts have increased to examine brittle fracture stability through small-scale tests. In the present study, a technology was developed to predict CAT with small specimens. The CAT prediction formula developed with small specimens makes it possible to accurately predict CAT using data obtained through large-scale experiments.


  • Open Access

    Reductions in the Laser Welding Deformation of STS304 Cylindrical Structure Using the Pre-Stress Method

    by Se-Hwan Lee, Ho-Chan Jeon, Jeong-Ung Park

    Welding deformation occurs due to non-uniform thermal expansion, thermal contraction, restraint, and phase transformation in a metal by a local welding heat source. This causes problems such as low buckling strength and the reduced workability of the production process. Correcting welding deformations in stainless steel using heat—such as by linear heating—causes metal sensitization, which should be avoided. Herein, welding deformation was reduced by applying tension stress instead of correcting the deformation by heating. A deformation-prevention jig was used to reduce welding deformation during the manufacturing of a cylinder made of STS304 by laser welding. The tensile stress was induced by pushing the cylinder shell outward using the deformation-prevention jig. A thermo-elastoplastic analysis was performed to investigate the effects of the magnitude of the tensile stress on welding deformation. Furthermore, the parametric results—which indicated a reduction in welding deformation—were verified through experiments. The thermo-elastoplastic analysis suggested that deformation did not occur when the magnitude of tensile stress was approximately 50% of the yield stress of the base metal. Moreover, the deformation was experimentally reduced by 11–20% when a tensile stress of 30 MPa was applied to the cylinder, compared with that in the absence of tensile stress.


  • Open Access

    Welding Residual Stress Distributions in the Thickness Direction under Constraints Using Neutron Diffraction and Contour Methods

    by Daehee Seong, Gyubaek An, Jeongung Park, Wanchuck Woo

    Using high-strength steel for offshore structures with a yield stress of 500 MPa, this study evaluated the distribution characteristics of welding residual stress in the thickness direction under the influence of constrained conditions during welding using cutting, neutron diffraction, and contour methods. Welding residual stress inevitably occurs during welding and impacts fracture stability in structures. As high-strength steel better reflects the effects of phase transformation, the behavior of welding residual stress is known to differ from that of general steel. This study fabricated fully constrained and unconstrained specimens and evaluated them under identical conditions to evaluate welding residual stress according to the influence of constraints on high-strength steel welds. The results indicated that the maximum tensile residual stress of the fully constrained specimen occurred in the first layer of the weld joint, while the maximum tensile residual stress of the fully unconstrained specimen occurred in the last layer of the weld joint. Additionally, the welding residual stress of the fully constrained specimen was larger. Although some errors occurred in the residual stress values in the thickness direction depending on the measurement method, both methods applied in this study exhibited nearly identical distributions. Meanwhile, a maximum angular deformation of about 6° occurred in the fully unconstrained specimen, and we considered that the residual stress decreased owing to the occurrence of angular deformation. The maximum welding residual stress is generally the degree of yield stress. When residual stress greater than the yield stress occurs, it changes to the plastic range and appears in the form of angular, longitudinal, and lateral deformation. Under the fully unconstrained condition, reduced residual stress is considered to appear in the form of angular deformation. The welding tensile residual stress decreased to around 42% in the unconstrained specimen compared to the constrained specimen, and at that time, angular deformation of approximately 6° occurred. Therefore, it is estimated that an angular distortion of about 2.4° occurs as the stress of 100 MPa decreases.


  • Open Access

    Residual Stress and Deformation Characteristics by FSW and SAW of Wear Resistant Steel

    by Jeongung Park, Gyubaek An, Dusan Kim

    Abrasion easily occurs due to the characteristic of the usage environment such as oil sands and construction equipment, and the demand for a steel with excellent wear resistance is increasing in various industries where specific parts are frequently replaced. Recently, by controlling the amount of manganese, high manganese austenite steels with improved wear resistance and low temperature brittleness performance have been developed and widely applied to LNG fuel tanks of ships and pipes. In this study, the temperature distribution, residual stress, and weld deformation caused by welding generated by friction stir welding(FSW) and submerged arc welding(SAW) for high manganese austenite steel with strong wear resistance were analyzed through thermal elastic plastic analysis.


  • Open Access

    Effect of Transverse Restraint on Welding Residual Stress in V-Groove Butt Welding

    by Jeongung Park, Gyubaek An, Ninshu Ma, Seongjoon Kim

    When evaluating the safety of steel structures, welding residual stress is used as the secondary load and if there is any restraint, the yield stress of the base material is used for secondary load, regardless of the size of the restraint. Of late, as the yield stress of members is increasing with the increase in the use of high-strength steels, the proportion of the residual welding stress in the total load during the evaluation of the safety of structures is increasing. Therefore, it is necessary to investigate the effect of the size of the restraint on the residual welding stress, determine reasonable residual stress according to the size of the restraint, and apply the residual stress as a secondary load. To investigate the effect of constraint conditions on residual welding stress, thermoelastic–plastic analysis was performed for different member thicknesses, yield stresses, and constraint sizes. The restraint did not affect the residual stress in the direction of the weld line but did affect the residual stress in the direction perpendicular to the weld line. The restraint moved the tensile stress to the compression stress in the direction perpendicular to the weld line at the first layer of the weld and moved the compression stress to the tensile stress at the middle and final layers of the weld. The change in residual stress was the largest in the middle of the weld.