Abstract
This study investigates the role of mineralizer selection in modulating the crystal structure and surface chemical states of manganese dioxide (MnO2) synthesized via a hydrothermal approach. Three oxidants—K2S2O8, KMnO4, and KClO3—were employed as mineralizers, yielding distinct phase evolution and defect concentrations. X-ray Diffraction (XRD) revealed that K2S2O8 and KClO3 favor the β-MnO2 (pyrolusite) phase, while KMnO4 drives a complete phase transition to α-MnO2 (hollandite), with average crystallite sizes ranging from 30.98 to 91.31 nm. High-resolution X-ray Photoelectron Spectroscopy (XPS) deconvolution demonstrated that KClO3 promotes the highest surface defect concentration (Odef/OH ∼ 36.46%) and Mn3+ fraction (∼ 32.44%), which are essential for enhancing faradaic charge storage. Cyclic Voltammetry (CV) measurements in 1 M Na2SO4 revealed that the KClO3-derived MnO2 achieves a maximum specific capacitance of 79.86 ± 9.46 F/g at 10 mV/s, retaining 28.3% of this value at 100 mV/s, significantly outperforming K2S2O8 (40.03 ± 27.43 F/g, 21.6% retention) and KMnO4 (20.77 ± 18.87 F/g, 19.9% retention). These results establish a comprehensive mineralizer–structure–property framework for defect-engineered MnO2 in advanced electrochemical energy storage.