To clarify the foaming behavior of FeO-containing slags during pulverized coal injection, calcined anthracite powder was introduced under continuous Ar gas blowing, and the temporal change in foam height was measured. CaO–SiO2–FeO–Al2O3 and CaO–SiO2–FeO–MgO slags were used. Relatively large bubbles were formed when only Ar gas was blown, whereas after pulverized coal injection, a film-like structure formed on the slag surface and the foam height increased markedly. For the Al2O3-containing slag, injection of 0.1 g of pulverized coal resulted in maximum foam heights of approximately 30 mm in the first injection and 65 mm in the second injection. SEM observation and EDS analysis revealed phases corresponding to wüstite, gehlenite, and fine metallic Fe in the upper region of the Al2O3-containing slag, and phases corresponding to wüstite and metallic Fe in the film-like sample from the MgO-containing slag. In foaming caused only by Ar gas blowing, the foam height increased on the higher-viscosity side, whereas during pulverized coal injection, the maximum foam height increased with increasing temperature. The MgO-containing slag showed a lower foam height than the Al2O3-containing slag under Ar gas blowing alone, but exhibited rapid and pronounced foaming during pulverized coal injection. These results suggest that foaming during pulverized coal injection is likely a multiphase reaction phenomenon governed by the combined effects of liquid-phase viscosity, gas generation through the carbonaceous material–FeO reaction, dispersion of solid phases or metallic Fe particles, and gas retention within the foam films.