Mechanical properties and microstructure evolution of KD‐SA SiC f /BN/SiC CMCs oxidized at different temperatures

Authors:

Abstract
Silicon carbide fiber‐reinforced SiC ceramic matrix composites (SiC f /SiC CMCs) based on a domestic KD‐SA SiC fiber were exposed to a wet oxygen atmosphere for 135 h at 800, 1100, and 1300°C. The evolution of the microstructure and mechanical properties of SiC f /SiC CMCs have been systematically investigated following oxidation. For weight change, CMC‐1300 showed the greatest gain (0.394%), followed by CMC‐1100 (0.356%) and CMC‐800 (0.149%). The volatilization of boron oxide (B 2 O 3 ) combined with the slight oxidation of the SiC matrix at 800°C caused crack deflection and fiber pull‐out. The complete dissipation of the interphase could be found when the oxidation temperature increases to 1100°C, generated a fracture surface with brittle fracture characteristics. At 1300°C, crystalline SiO 2 hindered oxygen diffusion, with evidence of fiber pull‐out. Based on thermodynamic calculations and microscopic observations, we propose a mechanism to explain the thermal degradation of SiC f /SiC CMCs. This work offers valuable guidance for the fabrication of SiC f /SiC CMCs that are suitable for high‐temperature applications.
Funding Information
  • National Key Research and Development Program of China (2022YFB3707700)
  • National University of Defense Technology (WDZC20235250503)

This publication has 33 references indexed in Scilit: