Abstract
The performance of aluminide-coated IN617 nickel based alloy has been investigated in a molten chloride mixture (53.41 MgCl2–25.62 KCl–20.97 NaCl in wt.%) at 700°C up to 1000h for combatting hot corrosion of materials in thermal energy storage systems in concentrated solar power plants. The aluminide coating was applied using an environmentally benign Al slurry and heat treated at high temperature. The resulting coating has several zones based on NiAl intermetallics and Co-, Cr- and Mo-rich precipitates. After 100 h, a thick oxide layer with Al and some Mg was observed, and XRD confirmed α-Al₂O₃ and MgAl₂O₄. The coating became porous with significant Al depletion in the upper region, while the remaining Al was concentrated near the original interdiffusion zone. Despite this degradation, no substrate attack was observed.After 500 h, the coating is almost fully depleted in Al (2 wt.%), depleted in Cr, while maintaining high Co (10 wt.%) and showing Fe enrichment (30 wt.%).After 1000 h, Al had disappeared, leaving a porous metallic zone beneath the corrosion products. The coating does not provide sufficient corrosion resistance under these conditions. The molten chloride mixture rapidly leaches Al from the coating, forming a non-protective, multilayered and thick oxide.

This publication has 16 references indexed in Scilit: