Pauline Audigié
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Pauline Audigié has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
- Alina Agüero
Instituto Nacional de Técnica Aeroespacial, Área de Materiales Metálicos, Ctra. Ajalvir Km 4, 28850 Torrejón de Ardoz, Spain
10 shared publications - Sergio Rodríguez
Department of Materials and Structures, Instituto Nacional de Técnica Aeroespacial (INTA), Torrejón de Ardoz, Madrid, Spain
5 shared publications André Malié
4 shared publicationsAurélie Rouaix-Vande Put
4 shared publicationsDaniel Monceau
4 shared publications- Jon Pascual
Department of Materials and Structures, Instituto Nacional de Técnica Aeroespacial (INTA), Torrejón de Ardoz, Madrid, Spain
4 shared publications
Latest Publications
- 11 October 2026
- Published by European Powder Metallurgy Association
Spark-Plasma-Sintered AlCoCrFeNiTiSi HEAs As Bond Coats For Advanced Thermal Barrier Coatings
Industry is raising turbine inlet temperatures to boost aircraft engine efficiency, especially for future hydrogen-fuelled propulsion. These harsher conditions demand robust protection of high-pressure turbine blades and vanes against high-temperature oxidation and corrosion. High-entropy alloys (HEAs) used as bond coats in advanced thermal barrier coatings (TBCs) offer a promising route to mitigate interfacial instabilities from high-temperature interdiffusion, yet their high-temperature phase stability and coupled thermo-mechanical behaviour remain poorly understood.Here, we design a series of spark-plasma-sintered AlCoCrFeNiTiSi HEAs engineered for high-temperature phase stability, oxidation resistance and spallation resistance. From a single nominal composition, varying SPS conditions produce samples with different phase assemblages, which have allowed us to study how phase composition and thermodynamics control the evolution of the oxide scale over 500 h at 1100 °C.
- 11 October 2026
- Published by European Powder Metallurgy Association
Spark-Plasma-Sintered AlCoCrFeNiTiSi HEAs As Bond Coats For Advanced Thermal Barrier Coatings
Industry is raising turbine inlet temperatures to boost aircraft engine efficiency, especially for future hydrogen-fuelled propulsion. These harsher conditions demand robust protection of high-pressure turbine blades and vanes against high-temperature oxidation and corrosion. High-entropy alloys (HEAs) used as bond coats in advanced thermal barrier coatings (TBCs) offer a promising route to mitigate interfacial instabilities from high-temperature interdiffusion, yet their high-temperature phase stability and coupled thermo-mechanical behaviour remain poorly understood.Here, we design a series of spark-plasma-sintered AlCoCrFeNiTiSi HEAs engineered for high-temperature phase stability, oxidation resistance and spallation resistance. From a single nominal composition, varying SPS conditions produce samples with different phase assemblages, which have allowed us to study how phase composition and thermodynamics control the evolution of the oxide scale over 500 h at 1100 °C.
- Open Access
- 1 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Corrosion degradation of slurry aluminized IN617 after 1000 h of exposure in molten chlorides at 700 °C
- 1 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Open AccessCorrosion degradation of slurry aluminized IN617 after 1000 h of exposure in molten chlorides at 700 °C
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Modélisation de l'interdiffusion et du comportement en oxydation cyclique de superalliages monocristallins à base de nickel revêtus d'une sous-couche γ-γ’ riche en platine. Extension aux systèmes barrière thermique
Les systèmes barrière thermique actuels connaissent une importante dispersion de durées de vie liée principalement aux ondulations de surface du revêtement métallique β-(Ni,Pt)Al provoquant l’écaillage du dépôt céramique. Les revêtements γ-γ’ riches en platine sont étudiés en tant qu’alternative au système actuel. Ce travail de thèse s’est intéressé à l’élaboration des revêtements γ-γ’ riches en platine sur un superalliage à base de nickel, l’AM1 à partir de procédés conventionnels : dépôt électrolytique de platine et aluminisation courte. Les mécanismes de dégradation par oxydation cyclique à 1100°C ont été étudiés sur des systèmes revêtement/AM1 et sur des systèmes barrière thermique. Pour comparaison, trois types de revêtement ont été élaborés : γ-γ’ Pt seul, γ-γ’ Pt+Al et β-(Ni,Pt)Al. Ces essais ont mis en évidence une meilleure tenue à l’oxydation cyclique des systèmes revêtus γ-γ’ Pt+Al comparée aux deux autres systèmes revêtus. L’importance de l’ajout d’aluminium dès l’élaboration sur la tenue à l’oxydation cyclique a été soulignée. La modélisation p-kp a mis en avant une augmentation de la proportion d’écaillage au cours du temps du fait de la dégradation de l’interface métal/oxyde et une augmentation du kp du fait de la formation d’un oxyde à croissance plus rapide. Outre l’oxydation, les phénomènes d’interdiffusion lors des tous premiers instants à haute température ont été étudiés à partir de matériaux modèles (Ni13Al et Ni11Al10Cr) et de revêtements de Pt et/ou de Pt-Ir. Ces essais ont mis en avant la rapide formation de la phase α-NiPtAl, les transformations de phases et les chemins de diffusion à 1100°C dans les systèmes Ni-Al-Pt et Ni-Al-Cr-Pt. L’effet du chrome et de l’iridium sur les cinétiques de diffusion a été évalué. La modélisation de l’interdiffusion a mis en évidence les interactions chimiques entre les espèces et une sursaturation en lacunes dans la zone d’interdiffusion prouvant que l’effet Kirkendall est responsable de la formation des pores.
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Modélisation de l'interdiffusion et du comportement en oxydation cyclique de superalliages monocristallins à base de nickel revêtus d'une sous-couche γ-γ’ riche en platine. Extension aux systèmes barrière thermique
Les systèmes barrière thermique actuels connaissent une importante dispersion de durées de vie liée principalement aux ondulations de surface du revêtement métallique β-(Ni,Pt)Al provoquant l’écaillage du dépôt céramique. Les revêtements γ-γ’ riches en platine sont étudiés en tant qu’alternative au système actuel. Ce travail de thèse s’est intéressé à l’élaboration des revêtements γ-γ’ riches en platine sur un superalliage à base de nickel, l’AM1 à partir de procédés conventionnels : dépôt électrolytique de platine et aluminisation courte. Les mécanismes de dégradation par oxydation cyclique à 1100°C ont été étudiés sur des systèmes revêtement/AM1 et sur des systèmes barrière thermique. Pour comparaison, trois types de revêtement ont été élaborés : γ-γ’ Pt seul, γ-γ’ Pt+Al et β-(Ni,Pt)Al. Ces essais ont mis en évidence une meilleure tenue à l’oxydation cyclique des systèmes revêtus γ-γ’ Pt+Al comparée aux deux autres systèmes revêtus. L’importance de l’ajout d’aluminium dès l’élaboration sur la tenue à l’oxydation cyclique a été soulignée. La modélisation p-kp a mis en avant une augmentation de la proportion d’écaillage au cours du temps du fait de la dégradation de l’interface métal/oxyde et une augmentation du kp du fait de la formation d’un oxyde à croissance plus rapide. Outre l’oxydation, les phénomènes d’interdiffusion lors des tous premiers instants à haute température ont été étudiés à partir de matériaux modèles (Ni13Al et Ni11Al10Cr) et de revêtements de Pt et/ou de Pt-Ir. Ces essais ont mis en avant la rapide formation de la phase α-NiPtAl, les transformations de phases et les chemins de diffusion à 1100°C dans les systèmes Ni-Al-Pt et Ni-Al-Cr-Pt. L’effet du chrome et de l’iridium sur les cinétiques de diffusion a été évalué. La modélisation de l’interdiffusion a mis en évidence les interactions chimiques entre les espèces et une sursaturation en lacunes dans la zone d’interdiffusion prouvant que l’effet Kirkendall est responsable de la formation des pores.
- Open Access
- 13 February 2026
- Published by Elsevier in SSRN Electronic Journal
Corrosion degradation of slurry aluminized IN617after 1000 h of exposure in molten chlorides at 700 °C
The performance of aluminide-coated IN617 nickel based alloy has been investigated in a molten chloride mixture (53.41 MgCl2–25.62 KCl–20.97 NaCl in wt.%) at 700°C up to 1000h for combatting hot corrosion of materials in thermal energy storage systems in concentrated solar power plants. The aluminide coating was applied using an environmentally benign Al slurry and heat treated at high temperature. The resulting coating has several zones based on NiAl intermetallics and Co-, Cr- and Mo-rich precipitates. After 100 h, a thick oxide layer with Al and some Mg was observed, and XRD confirmed α-Al₂O₃ and MgAl₂O₄. The coating became porous with significant Al depletion in the upper region, while the remaining Al was concentrated near the original interdiffusion zone. Despite this degradation, no substrate attack was observed.After 500 h, the coating is almost fully depleted in Al (2 wt.%), depleted in Cr, while maintaining high Co (10 wt.%) and showing Fe enrichment (30 wt.%).After 1000 h, Al had disappeared, leaving a porous metallic zone beneath the corrosion products. The coating does not provide sufficient corrosion resistance under these conditions. The molten chloride mixture rapidly leaches Al from the coating, forming a non-protective, multilayered and thick oxide.
- 13 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessCorrosion degradation of slurry aluminized IN617after 1000 h of exposure in molten chlorides at 700 °C
The performance of aluminide-coated IN617 nickel based alloy has been investigated in a molten chloride mixture (53.41 MgCl2–25.62 KCl–20.97 NaCl in wt.%) at 700°C up to 1000h for combatting hot corrosion of materials in thermal energy storage systems in concentrated solar power plants. The aluminide coating was applied using an environmentally benign Al slurry and heat treated at high temperature. The resulting coating has several zones based on NiAl intermetallics and Co-, Cr- and Mo-rich precipitates. After 100 h, a thick oxide layer with Al and some Mg was observed, and XRD confirmed α-Al₂O₃ and MgAl₂O₄. The coating became porous with significant Al depletion in the upper region, while the remaining Al was concentrated near the original interdiffusion zone. Despite this degradation, no substrate attack was observed.After 500 h, the coating is almost fully depleted in Al (2 wt.%), depleted in Cr, while maintaining high Co (10 wt.%) and showing Fe enrichment (30 wt.%).After 1000 h, Al had disappeared, leaving a porous metallic zone beneath the corrosion products. The coating does not provide sufficient corrosion resistance under these conditions. The molten chloride mixture rapidly leaches Al from the coating, forming a non-protective, multilayered and thick oxide.
- Open Access
- 18 November 2025
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 3
Hot Corrosion and Mechanical Performance of Aluminide Coated Austenitic Steel
The present study aims at improving coatings to allow higher operating temperatures – up to 700 °C – while resisting hot corrosion in future heat transfer fluids and storage systems for CSP technology. An aluminide coating was produced onto a 347H austenitic alloy to resist Li-Na-K molten carbonate corrosion at 700 °C. Multiple surface preparations were investigated and, after optimization, a new diffusion heat treatment was selected. A homogeneous 3-layer coating was formed with Al content reaching up to 69 at.% at the top surface. Corrosion was significantly decreased by the coating compared to the uncoated material. After 500h-exposure, a 100 µm-thick multi-layered and non-adhesive alkali elements rich oxide formed at the surface of uncoated 347H alloy. On the contrary, the coated material preserved its morphology and a mix of α-LiAlO2 and γ-LiAlO2 formed on the top coating. From the mechanical perspective, local hardness measurements highlighted a broad variation along the different layers of the coating. 3-point bending tests showed that deformation in the plastic domain was required to cause crack formation. Cracks remained in the two outermost layers of the coating and did not reach the underneath substrate.
- 18 November 2025
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 3
Open AccessHot Corrosion and Mechanical Performance of Aluminide Coated Austenitic Steel
The present study aims at improving coatings to allow higher operating temperatures – up to 700 °C – while resisting hot corrosion in future heat transfer fluids and storage systems for CSP technology. An aluminide coating was produced onto a 347H austenitic alloy to resist Li-Na-K molten carbonate corrosion at 700 °C. Multiple surface preparations were investigated and, after optimization, a new diffusion heat treatment was selected. A homogeneous 3-layer coating was formed with Al content reaching up to 69 at.% at the top surface. Corrosion was significantly decreased by the coating compared to the uncoated material. After 500h-exposure, a 100 µm-thick multi-layered and non-adhesive alkali elements rich oxide formed at the surface of uncoated 347H alloy. On the contrary, the coated material preserved its morphology and a mix of α-LiAlO2 and γ-LiAlO2 formed on the top coating. From the mechanical perspective, local hardness measurements highlighted a broad variation along the different layers of the coating. 3-point bending tests showed that deformation in the plastic domain was required to cause crack formation. Cracks remained in the two outermost layers of the coating and did not reach the underneath substrate.
- Open Access
- 13 September 2025
- Published by Springer Nature in Materials for Renewable and Sustainable Energy
- Vol. 14 (3) , 1-21
Modified high hardness steel coating for biomass corrosion protection
Biomass is a renewable and CO 2 -neutral energy source. However, the efficiency of biomass combustion plants remains lower than that of current fossil fuel-based systems. To minimize corrosion from aggressive species found in biomass combustion, these plants currently operate at a maximum temperature of 550 °C. The European project BELENUS explored new materials and coatings to raise the operating temperature to 600 °C, thereby improving plant efficiency. Among the coatings under investigation, a super high-hardness steel (SHS) modified with Al, applied by high velocity oxy-fuel (HVOF) thermal spray on ferritic steel SVM12, has demonstrated an improved performance in the laboratory, exposed to a model biomass environment containing KCl deposits for 8000 h at 600 °C. Microstructural analysis by field emission scanning electron microscopy (FESEM) and X-ray diffraction was conducted on the tested samples to examine the coating’s evolution in these environments, as well as the associated protection and degradation mechanisms. The presence of Al within the coating significantly enhanced its resistance to biomass corrosion when compared to uncoated SVM12 and the Al-free SHS coating. Possible reasons for the improved behaviour of the Al-modified coating are the reduction of porosity as well as the blocking effect of either intermetallic FeAl or Al oxide which forms at the splat boundaries prior to exposure to the corrosive atmosphere.
- 13 September 2025
- Published by Springer Nature in Materials for Renewable and Sustainable Energy
- Vol. 14 (3) , 1-21
Open AccessModified high hardness steel coating for biomass corrosion protection
Biomass is a renewable and CO 2 -neutral energy source. However, the efficiency of biomass combustion plants remains lower than that of current fossil fuel-based systems. To minimize corrosion from aggressive species found in biomass combustion, these plants currently operate at a maximum temperature of 550 °C. The European project BELENUS explored new materials and coatings to raise the operating temperature to 600 °C, thereby improving plant efficiency. Among the coatings under investigation, a super high-hardness steel (SHS) modified with Al, applied by high velocity oxy-fuel (HVOF) thermal spray on ferritic steel SVM12, has demonstrated an improved performance in the laboratory, exposed to a model biomass environment containing KCl deposits for 8000 h at 600 °C. Microstructural analysis by field emission scanning electron microscopy (FESEM) and X-ray diffraction was conducted on the tested samples to examine the coating’s evolution in these environments, as well as the associated protection and degradation mechanisms. The presence of Al within the coating significantly enhanced its resistance to biomass corrosion when compared to uncoated SVM12 and the Al-free SHS coating. Possible reasons for the improved behaviour of the Al-modified coating are the reduction of porosity as well as the blocking effect of either intermetallic FeAl or Al oxide which forms at the splat boundaries prior to exposure to the corrosive atmosphere.
- 21 February 2025
- Published by Elsevier in Corrosion Science
- Vol. 249
Analysis of void formation in Pt-rich γ-γ’ bond-coatings for TBC system application
- 21 February 2025
- Published by Elsevier in Corrosion Science
- Vol. 249
Analysis of void formation in Pt-rich γ-γ’ bond-coatings for TBC system application
- Open Access
- 17 October 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (43) , 59507-59515
Rapid α-Al2O3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O2, H2O, and KCl
In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired power boiler. The samples were exposed under model Cl-rich biomass conditions, in a KCl + O2 + H2O environment at 600 °C for 168, 2000, and 8000 h. The morphology of corrosion and the composition of the oxide scale and the coating were investigated by a combination of advanced analytical techniques such as FESEM/EDS, SEM/EBSD, and XRD. Even after short-term exposure, the coating developed a very fast-growing and up to 50 μm thick α-Al2O3 scale in contrast to the spontaneous formation of a protective, thin, dense, slow-growing, and very adhesive α-Al2O3 layer usually formed on metallic materials after high-temperature oxidation. In view of the literature on the formation of oxide scales on alloys and coatings, the formation of an α-Al2O3 scale at this relatively low temperature is very surprising in itself. The thick alumina scale was not protective as its formation resulted in fast degradation of the coating and rapid Fe2Al5 → FeAl phase transformation, which in turn generated porosity inside the coating. In all cases, the resulting thick Al2O3 scale was porous and consisted of both equiaxed α-Al2O3 grains and randomly oriented aggregated alumina whiskers. Potassium is concentrated in the outer part of the Al2O3 scale, while chlorine is concentrated close to the scale/aluminide interface. The unexpected formation of rapidly growing α-Al2O3 at relatively low temperature is attributed to the hydrolysis of aluminum chloride generated in the corrosion process.
- 17 October 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (43) , 59507-59515
Open AccessRapid α-Al2O3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O2, H2O, and KCl
In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired power boiler. The samples were exposed under model Cl-rich biomass conditions, in a KCl + O2 + H2O environment at 600 °C for 168, 2000, and 8000 h. The morphology of corrosion and the composition of the oxide scale and the coating were investigated by a combination of advanced analytical techniques such as FESEM/EDS, SEM/EBSD, and XRD. Even after short-term exposure, the coating developed a very fast-growing and up to 50 μm thick α-Al2O3 scale in contrast to the spontaneous formation of a protective, thin, dense, slow-growing, and very adhesive α-Al2O3 layer usually formed on metallic materials after high-temperature oxidation. In view of the literature on the formation of oxide scales on alloys and coatings, the formation of an α-Al2O3 scale at this relatively low temperature is very surprising in itself. The thick alumina scale was not protective as its formation resulted in fast degradation of the coating and rapid Fe2Al5 → FeAl phase transformation, which in turn generated porosity inside the coating. In all cases, the resulting thick Al2O3 scale was porous and consisted of both equiaxed α-Al2O3 grains and randomly oriented aggregated alumina whiskers. Potassium is concentrated in the outer part of the Al2O3 scale, while chlorine is concentrated close to the scale/aluminide interface. The unexpected formation of rapidly growing α-Al2O3 at relatively low temperature is attributed to the hydrolysis of aluminum chloride generated in the corrosion process.
- Open Access
Aluminide Coatings by Means of Slurry Application: A Low Cost, Versatile and Simple Technology
The present study focused on demonstrating the versatility of the slurry deposition technique to produce aluminide coatings to protect components from high-temperature corrosion in a broad temperature range, from 400 to 1400 °C. This is a simpler and low-cost coating technology used as an alternative to CVD and pack cementation, which also allows the coating of complex geometries and offers improved and simple repairability for a lot of industrial applications, along with avoiding the use of non-hazardous components. Slurry aluminide coatings from a proprietary water-based-Cr6+ free slurry were produced onto four different substrates: A516 carbon steel, 310H AC austenitic steel, Ti6246 Ti-based alloy and TZM, a Mo-based alloy. The resulting coatings were thoroughly characterised by FESEM and XRD, mainly so that the identification of microstructures and appropriate phases was reported for each coating. The importance of surface preparation and heat treatment as key parameters for the coating final microstructures was also evidenced, and how those parameters can be optimised to obtain stable intermetallic phases rich in Al to sustain the formation of a protective Al2O3 oxide scale. These coating systems have applications in diverse industrial environments in which high-temperature corrosion limits the lifetime of the components.
Open AccessAluminide Coatings by Means of Slurry Application: A Low Cost, Versatile and Simple Technology
The present study focused on demonstrating the versatility of the slurry deposition technique to produce aluminide coatings to protect components from high-temperature corrosion in a broad temperature range, from 400 to 1400 °C. This is a simpler and low-cost coating technology used as an alternative to CVD and pack cementation, which also allows the coating of complex geometries and offers improved and simple repairability for a lot of industrial applications, along with avoiding the use of non-hazardous components. Slurry aluminide coatings from a proprietary water-based-Cr6+ free slurry were produced onto four different substrates: A516 carbon steel, 310H AC austenitic steel, Ti6246 Ti-based alloy and TZM, a Mo-based alloy. The resulting coatings were thoroughly characterised by FESEM and XRD, mainly so that the identification of microstructures and appropriate phases was reported for each coating. The importance of surface preparation and heat treatment as key parameters for the coating final microstructures was also evidenced, and how those parameters can be optimised to obtain stable intermetallic phases rich in Al to sustain the formation of a protective Al2O3 oxide scale. These coating systems have applications in diverse industrial environments in which high-temperature corrosion limits the lifetime of the components.