Jon Pascual
Research Subjects
Research Interests
Jon Pascual has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Alina Agüero
Instituto Nacional de Técnica Aeroespacial, Área de Materiales Metálicos, Ctra. Ajalvir Km 4, 28850 Torrejón de Ardoz, Spain
4 shared publications - Pauline Audigié
Instituto Nacional de Técnica Aeroespacial (INTA) Spain
4 shared publications - Sergio Rodríguez
Department of Materials and Structures, Instituto Nacional de Técnica Aeroespacial (INTA), Torrejón de Ardoz, Madrid, Spain
4 shared publications - Gustavo García-Martín
Surface Engineering and Nanostructured Materials Research Group, Complutense University of Madrid, Madrid, Spain
2 shared publications - Marcos Gutiérrez
Department of Materials and Structures, Instituto Nacional de Técnica Aeroespacial (INTA), Torrejón de Ardoz, Madrid, Spain
2 shared publications - Francisco Javier Perez
Departamento de Ingeniería Química y de Materiales, Facultad de Ciencias Químicas, Universidad Complutense de Madrid, Pl. de las Ciencias, 2, Moncloa-Aravaca, 28040 Madrid, Spain
1 shared publication
Latest Publications
- Open Access
- 1 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Corrosion degradation of slurry aluminized IN617 after 1000 h of exposure in molten chlorides at 700 °C
- 1 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Open AccessCorrosion degradation of slurry aluminized IN617 after 1000 h of exposure in molten chlorides at 700 °C
- Open Access
- 13 February 2026
- Published by Elsevier in SSRN Electronic Journal
Corrosion degradation of slurry aluminized IN617after 1000 h of exposure in molten chlorides at 700 °C
The performance of aluminide-coated IN617 nickel based alloy has been investigated in a molten chloride mixture (53.41 MgCl2–25.62 KCl–20.97 NaCl in wt.%) at 700°C up to 1000h for combatting hot corrosion of materials in thermal energy storage systems in concentrated solar power plants. The aluminide coating was applied using an environmentally benign Al slurry and heat treated at high temperature. The resulting coating has several zones based on NiAl intermetallics and Co-, Cr- and Mo-rich precipitates. After 100 h, a thick oxide layer with Al and some Mg was observed, and XRD confirmed α-Al₂O₃ and MgAl₂O₄. The coating became porous with significant Al depletion in the upper region, while the remaining Al was concentrated near the original interdiffusion zone. Despite this degradation, no substrate attack was observed.After 500 h, the coating is almost fully depleted in Al (2 wt.%), depleted in Cr, while maintaining high Co (10 wt.%) and showing Fe enrichment (30 wt.%).After 1000 h, Al had disappeared, leaving a porous metallic zone beneath the corrosion products. The coating does not provide sufficient corrosion resistance under these conditions. The molten chloride mixture rapidly leaches Al from the coating, forming a non-protective, multilayered and thick oxide.
- 13 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessCorrosion degradation of slurry aluminized IN617after 1000 h of exposure in molten chlorides at 700 °C
The performance of aluminide-coated IN617 nickel based alloy has been investigated in a molten chloride mixture (53.41 MgCl2–25.62 KCl–20.97 NaCl in wt.%) at 700°C up to 1000h for combatting hot corrosion of materials in thermal energy storage systems in concentrated solar power plants. The aluminide coating was applied using an environmentally benign Al slurry and heat treated at high temperature. The resulting coating has several zones based on NiAl intermetallics and Co-, Cr- and Mo-rich precipitates. After 100 h, a thick oxide layer with Al and some Mg was observed, and XRD confirmed α-Al₂O₃ and MgAl₂O₄. The coating became porous with significant Al depletion in the upper region, while the remaining Al was concentrated near the original interdiffusion zone. Despite this degradation, no substrate attack was observed.After 500 h, the coating is almost fully depleted in Al (2 wt.%), depleted in Cr, while maintaining high Co (10 wt.%) and showing Fe enrichment (30 wt.%).After 1000 h, Al had disappeared, leaving a porous metallic zone beneath the corrosion products. The coating does not provide sufficient corrosion resistance under these conditions. The molten chloride mixture rapidly leaches Al from the coating, forming a non-protective, multilayered and thick oxide.
- Open Access
- 13 September 2025
- Published by Springer Nature in Materials for Renewable and Sustainable Energy
- Vol. 14 (3) , 1-21
Modified high hardness steel coating for biomass corrosion protection
Biomass is a renewable and CO 2 -neutral energy source. However, the efficiency of biomass combustion plants remains lower than that of current fossil fuel-based systems. To minimize corrosion from aggressive species found in biomass combustion, these plants currently operate at a maximum temperature of 550 °C. The European project BELENUS explored new materials and coatings to raise the operating temperature to 600 °C, thereby improving plant efficiency. Among the coatings under investigation, a super high-hardness steel (SHS) modified with Al, applied by high velocity oxy-fuel (HVOF) thermal spray on ferritic steel SVM12, has demonstrated an improved performance in the laboratory, exposed to a model biomass environment containing KCl deposits for 8000 h at 600 °C. Microstructural analysis by field emission scanning electron microscopy (FESEM) and X-ray diffraction was conducted on the tested samples to examine the coating’s evolution in these environments, as well as the associated protection and degradation mechanisms. The presence of Al within the coating significantly enhanced its resistance to biomass corrosion when compared to uncoated SVM12 and the Al-free SHS coating. Possible reasons for the improved behaviour of the Al-modified coating are the reduction of porosity as well as the blocking effect of either intermetallic FeAl or Al oxide which forms at the splat boundaries prior to exposure to the corrosive atmosphere.
- 13 September 2025
- Published by Springer Nature in Materials for Renewable and Sustainable Energy
- Vol. 14 (3) , 1-21
Open AccessModified high hardness steel coating for biomass corrosion protection
Biomass is a renewable and CO 2 -neutral energy source. However, the efficiency of biomass combustion plants remains lower than that of current fossil fuel-based systems. To minimize corrosion from aggressive species found in biomass combustion, these plants currently operate at a maximum temperature of 550 °C. The European project BELENUS explored new materials and coatings to raise the operating temperature to 600 °C, thereby improving plant efficiency. Among the coatings under investigation, a super high-hardness steel (SHS) modified with Al, applied by high velocity oxy-fuel (HVOF) thermal spray on ferritic steel SVM12, has demonstrated an improved performance in the laboratory, exposed to a model biomass environment containing KCl deposits for 8000 h at 600 °C. Microstructural analysis by field emission scanning electron microscopy (FESEM) and X-ray diffraction was conducted on the tested samples to examine the coating’s evolution in these environments, as well as the associated protection and degradation mechanisms. The presence of Al within the coating significantly enhanced its resistance to biomass corrosion when compared to uncoated SVM12 and the Al-free SHS coating. Possible reasons for the improved behaviour of the Al-modified coating are the reduction of porosity as well as the blocking effect of either intermetallic FeAl or Al oxide which forms at the splat boundaries prior to exposure to the corrosive atmosphere.
- Open Access
- 17 October 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (43) , 59507-59515
Rapid α-Al2O3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O2, H2O, and KCl
In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired power boiler. The samples were exposed under model Cl-rich biomass conditions, in a KCl + O2 + H2O environment at 600 °C for 168, 2000, and 8000 h. The morphology of corrosion and the composition of the oxide scale and the coating were investigated by a combination of advanced analytical techniques such as FESEM/EDS, SEM/EBSD, and XRD. Even after short-term exposure, the coating developed a very fast-growing and up to 50 μm thick α-Al2O3 scale in contrast to the spontaneous formation of a protective, thin, dense, slow-growing, and very adhesive α-Al2O3 layer usually formed on metallic materials after high-temperature oxidation. In view of the literature on the formation of oxide scales on alloys and coatings, the formation of an α-Al2O3 scale at this relatively low temperature is very surprising in itself. The thick alumina scale was not protective as its formation resulted in fast degradation of the coating and rapid Fe2Al5 → FeAl phase transformation, which in turn generated porosity inside the coating. In all cases, the resulting thick Al2O3 scale was porous and consisted of both equiaxed α-Al2O3 grains and randomly oriented aggregated alumina whiskers. Potassium is concentrated in the outer part of the Al2O3 scale, while chlorine is concentrated close to the scale/aluminide interface. The unexpected formation of rapidly growing α-Al2O3 at relatively low temperature is attributed to the hydrolysis of aluminum chloride generated in the corrosion process.
- 17 October 2024
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 16 (43) , 59507-59515
Open AccessRapid α-Al2O3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O2, H2O, and KCl
In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired power boiler. The samples were exposed under model Cl-rich biomass conditions, in a KCl + O2 + H2O environment at 600 °C for 168, 2000, and 8000 h. The morphology of corrosion and the composition of the oxide scale and the coating were investigated by a combination of advanced analytical techniques such as FESEM/EDS, SEM/EBSD, and XRD. Even after short-term exposure, the coating developed a very fast-growing and up to 50 μm thick α-Al2O3 scale in contrast to the spontaneous formation of a protective, thin, dense, slow-growing, and very adhesive α-Al2O3 layer usually formed on metallic materials after high-temperature oxidation. In view of the literature on the formation of oxide scales on alloys and coatings, the formation of an α-Al2O3 scale at this relatively low temperature is very surprising in itself. The thick alumina scale was not protective as its formation resulted in fast degradation of the coating and rapid Fe2Al5 → FeAl phase transformation, which in turn generated porosity inside the coating. In all cases, the resulting thick Al2O3 scale was porous and consisted of both equiaxed α-Al2O3 grains and randomly oriented aggregated alumina whiskers. Potassium is concentrated in the outer part of the Al2O3 scale, while chlorine is concentrated close to the scale/aluminide interface. The unexpected formation of rapidly growing α-Al2O3 at relatively low temperature is attributed to the hydrolysis of aluminum chloride generated in the corrosion process.