Translucency Changes of Ceramic Veneers After Aging When Cemented on Substrates With Different Saturation: Effect of Ceramic Translucency and Resin Cement Shade
Open Access
- 23 August 2026
- journal article
- research article
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
Abstract
Objective: To evaluate the effect of ceramic translucency and resin cement shade on the translucency alteration after aging over different substrates. Methods: Sixty specimens were divided into 12 groups ( n = 5) composed of lithium disilicate (IPS e.max CAD, Ivoclar Vivadent) in three translucencies (HT, MT, LT). The 0.5 mm thick specimens were cemented with Variolink Esthetic LC (Ivoclar Vivadent) Light+ (L+) and Neutral (N) over resin substrates A1 and A4. Samples were subjected to 20,000 aging thermocycles, alternating 55°C–5°C (30 s). Spectral reflectance was measured using a spectrophotometer (CM‐3700d—Konica Minolta) at four intervals: before aging (t0) and after 10,000 (t10), 15,000 (t15), and 20,000 (t20) cycles. The Translucency Parameter (TP 00 ) and the ΔTP 00 were calculated. The thresholds for translucency perceptibility (TPT 00 ) and acceptability (TAT 00 ) were set at 0.62 and 2.62, respectively. Statistical analysis was performed using four‐way repeated measures ANOVA and Tukey's post hoc test ( α = 0.05). Results: Aging time, ceramic translucency, resin cement color and substrate saturation had a significant effect ( p < 0.001) on TP 00 . While TP 00 values declined across all groups, the lowest values for each measurement moment were consistently observed in the LTL+ groups [1.70 (t0) to 0.90 (t20)]. All ΔTP 00 values remained below the acceptability threshold (TAT = 2.62). Conclusion: Aging resulted in a generalized decrease in translucency across all groups, particularly over lighter substrates and when using chromatic resin cement. However, no clinically unacceptable alterations were observed. Clinical Significance: Clinicians should select materials based on the balance between initial masking and long‐term stability. For dark substrates, LT ceramics ensure consistent optical stability during aging, regardless of the resin cement shade. While combining translucent ceramics (HT/MT) with chromatic resin cements is an effective strategy for initial masking, clinicians must be aware that ceramic translucency is the primary factor controlling the final optical outcome over time.Keywords
Funding Information
- Conselho Nacional de Desenvolvimento Científico e Tecnológico (124622/2023‐2)
- Fundação de Amparo à Pesquisa do Estado de São Paulo (2025/00187‐0)
This publication has 33 references indexed in Scilit:
- The effects of monomer type, filler size, and filler content of three resin cements on the color stability of laminate veneers exposed to accelerated agingDental Materials, 2024
- Can we use the translucency parameter to predict the CAD/CAM ceramic restoration aesthetic?Dental Materials, 2023
- 10-year practice-based evaluation of ceramic and direct composite veneersDental Materials, 2022
- Effect of finishing protocols and staining solutions on color stability of dental resin compositesClinical and Experimental Dental Research, 2022
- Influence of light-cured luting agents and associated factors on the color of ceramic laminate veneers: A systematic review of in vitro studiesDental Materials, 2018
- Translucency thresholds for dental materialsDental Materials, 2018
- Optical properties and light irradiance of monolithic zirconia at variable thicknessesDental Materials, 2015
- Color related to ceramic and zirconia restorations: A reviewDental Materials, 2011
- Influence of color parameters of resin composites on their translucencyDental Materials, 2008
- The development of the CIE 2000 colour‐difference formula: CIEDE2000Color Research & Application, 2001