Hydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics
Authors:
- Dayanne Monielle Duarte MouraDMDayanne Monielle Duarte Moura
- Arthur Magno Medeiros de AraújoArthur Magno Medeiros de Araújo
- Karina Barbosa de SouzaKSKarina Barbosa de Souza
- Aretha Heitor VeríssimoAVAretha Heitor Veríssimo
- João Paulo Mendes TribstJoão Paulo Mendes Tribst
- Rodrigo Othávio de Assunção e SouzaRSRodrigo Othávio de Assunção e Souza
Open Access
- 1 January 2020
- journal article
- research article
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 34, e018
Abstract
The objective of this study was to evaluate the influence of hydrofluoric acid (HF) concentration, etching time, and application of phosphoric acid (PA) followed by neutralization with sodium bicarbonate on the bond strength between a feldspar ceramic and resin cement. Thus, 80 blocks (10 x 12 x 2 mm) of glass ceramic (VM - Vita Mark II - Vita Zahnfabrik) were made and randomly assigned to eight groups (n =10) according to the factors: HF concentration (5 and 10%), etching time (60 and 120 s), and use of phosphoric acid (PA) (with and without). According to the experimental group, 37% PA (Condac, FGM) was applied after HF etching for 60s. Afterwards, samples were immersed in sodium bicarbonate for 1 min then in an ultrasonic bath in distilled water (5 min) for cleaning. After surface bonding treatment, cylinders (empty set = 2 mm; h = 2 mm) of dual resin cement (AllCem / FGM) were made in the center of each block. The samples were then stored in water (37 degrees C) for 90 days and submitted to the shear bond test (50 KgF, 1 mm/min). Failure analysis was performed by stereomicroscope and scanning electron microscopy. Data (MPa) were analyzed with 3-way ANOVA and Tukey's test. Only the factor "HF concentration" was significant (p = 0.02). Most failures were of cohesive in ceramic (40%) and mixed types (42.5%). The 10% HF resulted in higher shear bond strength value than the 5% HF. Surface cleaning with phosphoric acid followed by sodium bicarbonate and HF time (60 or 120 seconds) did not influence the resin bond strength to feldspar ceramic.Keywords
This publication has 29 references indexed in Scilit:
- Effect of the Etching Duration and Ultrasonic Cleaning on Microtensile Bond Strength Between Feldspathic Ceramic and Resin CementThe Journal of Adhesion, 2013
- Clinical results of lithium-disilicate crowns after up to 9 years of serviceClinical Oral Investigations, 2012
- Clinical evaluation on porcelain laminate veneers bonded with light-cured composite: results up to 7 yearsClinical Oral Investigations, 2011
- Surface/Interface Morphology and Bond Strength to Glass Ceramic Etched for Different PeriodsOperative Dentistry, 2010
- The effect of different surface treatments on bond strength between leucite reinforced feldspathic ceramic and composite resinJournal of Dentistry, 2010
- Effect of Acid Neutralization and Mechanical Cycling on the Microtensile Bond Strength of Glass-ceramic InlaysOperative Dentistry, 2009
- The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative materialDental Materials, 2007
- Influence of post-etching cleaning and connecting porcelain on the microtensile bond strength of composite resin to feldspathic porcelainThe Journal of Prosthetic Dentistry, 2006
- The influence of cement lute, thermocycling and surface preparation on the strength of a porcelain laminate veneering materialDental Materials, 2004
- Adhesion of composite to porcelain with various surface conditionsThe Journal of Prosthetic Dentistry, 1995