Dayanne Monielle Duarte Moura
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Dayanne Monielle Duarte Moura has a total of 62 co-authors. Here are the top co-authors by number of shared publications:
- Rodrigo Othavio de Assuncao E Souza
Department of Dentistry Federal University of Rio Grande do Norte (UFRN) Natal Brazil
17 shared publications - Mutlu Özcan
Center for Dental Medicine, Clinic of Masticatory Disorders and Dental Biomaterials, University of Zurich, Zurich, Switzerland
8 shared publications - Marco Antonio Bottino
Department of Cariology, Restorative Sciences, and Endodontics, School of Dentistry, University of Michigan, Ann Arbor, MI 48109, USA
6 shared publications - Aretha Heitor Veríssimo
Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Natal, Brazil
4 shared publications Ana Beatriz Do Nascimento Januário
Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Natal, Brazil
3 shared publications- Fabíola Pessôa Pereira Leite
Universidade Federal de Juiz de Fora, Brazil
3 shared publications
Latest Publications
- 17 October 2022
- Published by Springer Nature in Journal of Orofacial Orthopedics / Fortschritte der Kieferorthopädie
- Vol. 84 (S3) , 210-221
Bond strength, degree of conversion, and microorganism adhesion using different bracket-to-enamel bonding protocols
Purpose This study aimed to evaluate the effect of bonding protocols and the type of orthodontic resin on the adhesion of microorganisms, degree of conversion (DC), and shear bond strength (SBS) of metallic brackets to enamel. Methods A total of 60 bovine incisors were prepared and randomly divided into 6 groups (n = 10): “bonding protocol” (A: phosphoric acid; AXT: A+Transbond™ XT primer adhesive [all Transbond™ products from 3M Unitek, Monrovia, CA, USA]; and SE: Transbond™ Plus Self Etching Primer) and “orthodontic resin” (XT: Transbond™ XT adhesive paste and CC: Transbond™ Plus Color Change). After bonding, the samples were subjected to thermocycling (5000 cycles) and to the SBS test. Bond failures were classified according to the adhesive remnant index (ARI). Next, 60 enamel blocks were sterilized in ethylene oxide in order to perform the CFU (Streptococcus mutans) assay in vitro to analyze the colony forming units (CFU/mL). Then, 60 discs of each orthodontic resin were made to measure the DC. The SBS (MPa), CFU/mL, and DC (%) data were statistically analyzed by two-way analysis of variance and Tukey’s test (5%) was performed for the DC. Results CFU and SBS revealed no significance for all factors (P > 0.05). Tukey’s test showed that A_XT (acid+Transbond™ XT adhesive paste) presented the highest DC (70.38% ± 10.5), while AXT_XT (acid+Transbond™ XT primer adhesive+Transbond™ XT adhesive paste) showed the lowest (23.47% ± 10.4). An ARI score of 2 was more frequent for the CC resin and an ARI score of 4 for the XT resin. Conclusion The CC resin does not reduce adhesion of S. mutans around orthodontic brackets and the bonding protocol did not influence the SBS, although the SE and A_XT groups contributed to a better DC.
- 17 October 2022
- Published by Springer Nature in Journal of Orofacial Orthopedics / Fortschritte der Kieferorthopädie
- Vol. 84 (S3) , 210-221
Bond strength, degree of conversion, and microorganism adhesion using different bracket-to-enamel bonding protocols
Purpose This study aimed to evaluate the effect of bonding protocols and the type of orthodontic resin on the adhesion of microorganisms, degree of conversion (DC), and shear bond strength (SBS) of metallic brackets to enamel. Methods A total of 60 bovine incisors were prepared and randomly divided into 6 groups (n = 10): “bonding protocol” (A: phosphoric acid; AXT: A+Transbond™ XT primer adhesive [all Transbond™ products from 3M Unitek, Monrovia, CA, USA]; and SE: Transbond™ Plus Self Etching Primer) and “orthodontic resin” (XT: Transbond™ XT adhesive paste and CC: Transbond™ Plus Color Change). After bonding, the samples were subjected to thermocycling (5000 cycles) and to the SBS test. Bond failures were classified according to the adhesive remnant index (ARI). Next, 60 enamel blocks were sterilized in ethylene oxide in order to perform the CFU (Streptococcus mutans) assay in vitro to analyze the colony forming units (CFU/mL). Then, 60 discs of each orthodontic resin were made to measure the DC. The SBS (MPa), CFU/mL, and DC (%) data were statistically analyzed by two-way analysis of variance and Tukey’s test (5%) was performed for the DC. Results CFU and SBS revealed no significance for all factors (P > 0.05). Tukey’s test showed that A_XT (acid+Transbond™ XT adhesive paste) presented the highest DC (70.38% ± 10.5), while AXT_XT (acid+Transbond™ XT primer adhesive+Transbond™ XT adhesive paste) showed the lowest (23.47% ± 10.4). An ARI score of 2 was more frequent for the CC resin and an ARI score of 4 for the XT resin. Conclusion The CC resin does not reduce adhesion of S. mutans around orthodontic brackets and the bonding protocol did not influence the SBS, although the SE and A_XT groups contributed to a better DC.
- 14 June 2021
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 36 (7) , 685-700
Can enamel etching with the Er:YAG laser be an alternative to the conventional phosphoric acid for bracket bonding? A systematic review and meta-analysis
This systematic review and meta-analysis aimed to evaluate the effect of Er:YAG laser etching on shear bond strength (SBS) of brackets bonded to the enamel and compare to the phosphoric acid (control). Electronic databases (PubMed, Scopus, and Web of Science) and a manual search were conducted up to January 2021. In vitro studies comparing Er:YAG laser and phosphoric acid etching for metal bracket bonding to human teeth, that performed aging of samples submitted to SBS tests were included. The risk of bias was assessed considering specific parameters. Statistical analysis was conducted using the RStudio statistical program for meta-analysis. Among 1456 potentially eligible studies, 19 were selected for full-text analysis, and 12 were included for qualitative and quantitative analysis. In the general meta-analysis, phosphoric acid etching showed higher SBS (n = 516; p = 0.02; I2 = 95.4%). The 100 mJ (p = 0.05; I2 = 76.2%) and p < 0.01; I2 = 89.5%) showed a significant difference, favoring phosphoric acid etching, however, there was no significant difference in the >100 mJ subgroup (p < 0.32; I2 = 93.3%). In the 500-thermocycle subgroup, phosphoric acid etching had a significantly higher SBS (p < 0.01; I2 = 96.2%), however, there was no significant difference in etching techniques for the 5000-cycle subgroup (p = 0.10; I2 = 69.1%). Although Er:YAG laser provides lower SBS than phosphoric acid etching, it provides an adequate bracket bonding. Further investigations to establish a laser protocol and clinical evidence are important for the consolidation of Er:YAG laser as a viable alternative to phosphoric acid.
- 14 June 2021
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 36 (7) , 685-700
Can enamel etching with the Er:YAG laser be an alternative to the conventional phosphoric acid for bracket bonding? A systematic review and meta-analysis
This systematic review and meta-analysis aimed to evaluate the effect of Er:YAG laser etching on shear bond strength (SBS) of brackets bonded to the enamel and compare to the phosphoric acid (control). Electronic databases (PubMed, Scopus, and Web of Science) and a manual search were conducted up to January 2021. In vitro studies comparing Er:YAG laser and phosphoric acid etching for metal bracket bonding to human teeth, that performed aging of samples submitted to SBS tests were included. The risk of bias was assessed considering specific parameters. Statistical analysis was conducted using the RStudio statistical program for meta-analysis. Among 1456 potentially eligible studies, 19 were selected for full-text analysis, and 12 were included for qualitative and quantitative analysis. In the general meta-analysis, phosphoric acid etching showed higher SBS (n = 516; p = 0.02; I2 = 95.4%). The 100 mJ (p = 0.05; I2 = 76.2%) and p < 0.01; I2 = 89.5%) showed a significant difference, favoring phosphoric acid etching, however, there was no significant difference in the >100 mJ subgroup (p < 0.32; I2 = 93.3%). In the 500-thermocycle subgroup, phosphoric acid etching had a significantly higher SBS (p < 0.01; I2 = 96.2%), however, there was no significant difference in etching techniques for the 5000-cycle subgroup (p = 0.10; I2 = 69.1%). Although Er:YAG laser provides lower SBS than phosphoric acid etching, it provides an adequate bracket bonding. Further investigations to establish a laser protocol and clinical evidence are important for the consolidation of Er:YAG laser as a viable alternative to phosphoric acid.
- 9 September 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 35 (6) , 1-10
The number of specimens in a furnace affects the biaxial flexural strength of veneered zirconia specimens after sintering
This study evaluated the effect of the number of specimens in a furnace during the firing of porcelain-zirconia (Y-TZP) discs on their biaxial flexural strength. Eighty bilayer disc-shaped specimens (∅: 15mm; thickness: 1.2 mm, ISO 6872) of zirconia (Vita In-Ceram YZ Cubes/Vita) and porcelain (Vita VM9) ceramics, were prepared and divided into four groups (n = 20) according to the number of specimens in a furnace for each porcelain sintering: G1- one disc/20 sintering cycles.; G2 – two discs/10 sintering cycles.; G5-five discs/4 sintering cycles; and G10 – ten discs/2 sintering cycles. Then, the specimens were submitted to biaxial flexure testing (BFS) (1 mm/min, water). The data (MPa) were analyzed with Kruskal-Wallis test followed by the Dunn's post hoc analysis at a 95% level of confidence (α = 0.05). Kruskal-Wallis showed that the number of samples in the furnace affected flexural strength (p < 0.0001). The highest BFS was observed for the G5 (132.3 MPa)A, which was significantly higher than G1 (53.6 MPa)B. No significant difference was observed for the Weibull moduli and characteristic strength among the groups. In terms of flexural strength, approximately five specimens at a time can be placed in a furnace for sintering.
- 9 September 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 35 (6) , 1-10
The number of specimens in a furnace affects the biaxial flexural strength of veneered zirconia specimens after sintering
This study evaluated the effect of the number of specimens in a furnace during the firing of porcelain-zirconia (Y-TZP) discs on their biaxial flexural strength. Eighty bilayer disc-shaped specimens (∅: 15mm; thickness: 1.2 mm, ISO 6872) of zirconia (Vita In-Ceram YZ Cubes/Vita) and porcelain (Vita VM9) ceramics, were prepared and divided into four groups (n = 20) according to the number of specimens in a furnace for each porcelain sintering: G1- one disc/20 sintering cycles.; G2 – two discs/10 sintering cycles.; G5-five discs/4 sintering cycles; and G10 – ten discs/2 sintering cycles. Then, the specimens were submitted to biaxial flexure testing (BFS) (1 mm/min, water). The data (MPa) were analyzed with Kruskal-Wallis test followed by the Dunn's post hoc analysis at a 95% level of confidence (α = 0.05). Kruskal-Wallis showed that the number of samples in the furnace affected flexural strength (p < 0.0001). The highest BFS was observed for the G5 (132.3 MPa)A, which was significantly higher than G1 (53.6 MPa)B. No significant difference was observed for the Weibull moduli and characteristic strength among the groups. In terms of flexural strength, approximately five specimens at a time can be placed in a furnace for sintering.
- Open Access
- 1 June 2020
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 31 (3) , 272-280
Influence of Acid Etching and Universal Adhesives on the Bond Strength to Dentin
The purpose of this study was to evaluate the influence of the application mode of three universal adhesive systems on interfacial physical properties of indirect composite restorations adhesively cemented to dentin cavities. Seventy-eight bovine lower incisors were selected and a slice of dentin (thickness: 2 mm) between the buccal surface and pulp chamber was obtained for each tooth. Conical cavities were made on this surface. The internal walls of the cavities were then coated with a hydrophilic gel, filled with composite resin and photopolymerized. The dentin/cone sets were divided into 6 groups (n=10) according to type of universal adhesive (TETRI: Tetric N Bond, FUT: Futura Bond U, SBU: Single Bond Universal) and acid etching on dentin (A: with acid etching; WA: without acid etching). The acid etching and the adhesive systems were applied to the surface of the dentin. All composite resin cones were sandblasted (Al2O3, 20 s) and silanized. After surface treatment, the cones were cemented (RelyX Ultimate) into the dentin cavity and photopolymerized. After thermocycling (10,000 cycles), samples were submitted to marginal adaptation analysis (using caries detector dye), push-out test (0.5 mm/min), and failure mode analysis. Additional samples were prepared for nanoleakage analysis (SEM). The data (MPa) were analyzed by two-way ANOVA and Tukey’s post-test (5%). The groups in which the dentin was acid etched showed significantly lower bond strength values in the push-out test (p<0.01). Dentin acid etching significantly reduced the bond strength between universal adhesive systems and dentin in indirect restorative procedures.
- 1 June 2020
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 31 (3) , 272-280
Open AccessInfluence of Acid Etching and Universal Adhesives on the Bond Strength to Dentin
The purpose of this study was to evaluate the influence of the application mode of three universal adhesive systems on interfacial physical properties of indirect composite restorations adhesively cemented to dentin cavities. Seventy-eight bovine lower incisors were selected and a slice of dentin (thickness: 2 mm) between the buccal surface and pulp chamber was obtained for each tooth. Conical cavities were made on this surface. The internal walls of the cavities were then coated with a hydrophilic gel, filled with composite resin and photopolymerized. The dentin/cone sets were divided into 6 groups (n=10) according to type of universal adhesive (TETRI: Tetric N Bond, FUT: Futura Bond U, SBU: Single Bond Universal) and acid etching on dentin (A: with acid etching; WA: without acid etching). The acid etching and the adhesive systems were applied to the surface of the dentin. All composite resin cones were sandblasted (Al2O3, 20 s) and silanized. After surface treatment, the cones were cemented (RelyX Ultimate) into the dentin cavity and photopolymerized. After thermocycling (10,000 cycles), samples were submitted to marginal adaptation analysis (using caries detector dye), push-out test (0.5 mm/min), and failure mode analysis. Additional samples were prepared for nanoleakage analysis (SEM). The data (MPa) were analyzed by two-way ANOVA and Tukey’s post-test (5%). The groups in which the dentin was acid etched showed significantly lower bond strength values in the push-out test (p<0.01). Dentin acid etching significantly reduced the bond strength between universal adhesive systems and dentin in indirect restorative procedures.
- 1 May 2020
- Vol. 22 (3) , 275-283
Repair Bond Strength of a CAD/CAM Nanoceramic Resin and Direct Composite Resin: Effect of Aging and Surface Conditioning Methods
Purpose: To evaluate the effect of surface conditioning methods and aging on the repair bond strength between resin composite and nanoceramic CAD/CAM resin. Materials and Methods: Twenty-four blocks of nanoceramic CAD/CAM resin (NCR) (Lava Ultimate, 3M Oral Care) (10 x 5 x 2 mm(3)) and resin composite (Filtek Z350, 3M Oral Care) (RC) were made, embedded in acrylic resin, polished (#600, #800, #1200) and randomly divided into 8 groups (n = 12 each) according to surface conditioning methods (air abrasion with 30-mu m CoJet [CJ] or air abrasion with 50-mu m Al2O3 [AB]) and aging prior to repair (without aging, 24 h in water at 37 degrees C; with aging 6 months in water at 37 degrees C). The blocks were air abraded (20 s, 2.5 bar, 10 mm) using a standardized device. A layer of adhesive resin (Scotchbond Universal) was applied (20 s) and photopolymerized for 20 s. RC cylinders (O = 2 mm; h = 2 mm) were then bonded to the NCR substrates using a Teflon matrix and photopolymerized for 40 s. All specimens were thermocycled (10,000 cycles, 5 degrees C-55 degrees C) and submitted to the shear bond test (50 kgf, 0.5 mm/min) to measure repair strength. Data (MPa) were analyzed using 3-way ANOVA and Tukey's test (a = 0.05). Failure analysis was performed using stereomicroscopy (20X). Results: ANOVA revealed a significant effect of only the " material" factor (p = 0.00). The group NCR6mCJ presented bond strengths (29.37 +/- 5.41) which were significantly higher than those of the NCR24hCJ (20.88 +/- 5.74) and RC groups (p < 0.05). The group RC24hCJ (19.71 +/- 4.21) presented the lowest shear bond strength (p < 0.05). Failure analysis revealed predominantly type B mixed failures (adhesive+cohesive in the substrate material) except for the groups NCR24hCJ and NCR6mAB, where mainly type C failure (adhesive+cohesive at the RC) was observed. Conclusion: Air abrasion with Al2O3 particles or silicatization with CoJet followed by adhesive resin application are effective surface conditioning methods for the repair of nanoceramic CAD/CAM resin with resin composite.
- 1 May 2020
- Vol. 22 (3) , 275-283
Repair Bond Strength of a CAD/CAM Nanoceramic Resin and Direct Composite Resin: Effect of Aging and Surface Conditioning Methods
Purpose: To evaluate the effect of surface conditioning methods and aging on the repair bond strength between resin composite and nanoceramic CAD/CAM resin. Materials and Methods: Twenty-four blocks of nanoceramic CAD/CAM resin (NCR) (Lava Ultimate, 3M Oral Care) (10 x 5 x 2 mm(3)) and resin composite (Filtek Z350, 3M Oral Care) (RC) were made, embedded in acrylic resin, polished (#600, #800, #1200) and randomly divided into 8 groups (n = 12 each) according to surface conditioning methods (air abrasion with 30-mu m CoJet [CJ] or air abrasion with 50-mu m Al2O3 [AB]) and aging prior to repair (without aging, 24 h in water at 37 degrees C; with aging 6 months in water at 37 degrees C). The blocks were air abraded (20 s, 2.5 bar, 10 mm) using a standardized device. A layer of adhesive resin (Scotchbond Universal) was applied (20 s) and photopolymerized for 20 s. RC cylinders (O = 2 mm; h = 2 mm) were then bonded to the NCR substrates using a Teflon matrix and photopolymerized for 40 s. All specimens were thermocycled (10,000 cycles, 5 degrees C-55 degrees C) and submitted to the shear bond test (50 kgf, 0.5 mm/min) to measure repair strength. Data (MPa) were analyzed using 3-way ANOVA and Tukey's test (a = 0.05). Failure analysis was performed using stereomicroscopy (20X). Results: ANOVA revealed a significant effect of only the " material" factor (p = 0.00). The group NCR6mCJ presented bond strengths (29.37 +/- 5.41) which were significantly higher than those of the NCR24hCJ (20.88 +/- 5.74) and RC groups (p < 0.05). The group RC24hCJ (19.71 +/- 4.21) presented the lowest shear bond strength (p < 0.05). Failure analysis revealed predominantly type B mixed failures (adhesive+cohesive in the substrate material) except for the groups NCR24hCJ and NCR6mAB, where mainly type C failure (adhesive+cohesive at the RC) was observed. Conclusion: Air abrasion with Al2O3 particles or silicatization with CoJet followed by adhesive resin application are effective surface conditioning methods for the repair of nanoceramic CAD/CAM resin with resin composite.
- 1 April 2020
- Published by Elsevier in Dental Materials
- Vol. 36 (4) , e126-e139
Effect of finishing/polishing techniques and low temperature degradation on the surface topography, phase transformation and flexural strength of ultra-translucent ZrO2 ceramic
- 1 April 2020
- Published by Elsevier in Dental Materials
- Vol. 36 (4) , e126-e139
Effect of finishing/polishing techniques and low temperature degradation on the surface topography, phase transformation and flexural strength of ultra-translucent ZrO2 ceramic
- 1 February 2020
- Published by Elsevier in Journal of Dentistry
- Vol. 93, 103266
Effect of different repair methods on the bond strength of resin composite to CAD/CAM materials and microorganisms adhesion: An in situ study
- 1 February 2020
- Published by Elsevier in Journal of Dentistry
- Vol. 93, 103266
Effect of different repair methods on the bond strength of resin composite to CAD/CAM materials and microorganisms adhesion: An in situ study
- Open Access
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 28
Effect of different surface treatments and multimode adhesive application on the Weibull characteristics, wettability, surface topography and adhesion to CAD/CAM lithium disilicate ceramic
This paper aims to evaluate the effect of different surface treatments on surface topography, wettability, and shear bond strength of resin cement to glass ceramic. Methodology: For SBS test, 32 blocks (7x7x2 mm) of lithium disilicate were obtained and randomly divided into eight groups (four blocks per group) according to each surface treatment (HF 20 s, 60 s, 120 s + silanization/S or Scotch Bond Universal/ SBU) and the Monobond Etch & Prime - MEP application followed or not by SBU. On each treated surface ceramic block, up to four dual-curing resin cement cylinders were prepared and light-cured for 40s (N=120/n=15). The specimens were thermocycled (10,000 cycles, 5-55°C, 30 s) and the SBS test (50KgF, 0.5 mm/min) was performed. Furthermore, failure analysis, wettability, AFM, and SEM were carried out. SBS data (MPa) were analyzed using Student's t-test, two-way ANOVA, Tukey's test (5%) and Weibull's analysis. Results: For HF experimental groups, two-way ANOVA presented the factors “etching time” and “bonding agent” as significant (p<0.05). After silane application, the HF groups presented similar bond strength. SBU application compromised the SBS, except for 120s etching time (HF120sS: 23.39ᵃ±6.48 MPa; HF120sSBU: 18.76ᵃ±8.81MPa). For MEP groups, SBU application did not significantly affect the results (p=0.41). The MEP group presented the highest Weibull modulus (4.08A) and they were statistically different exclusively from the HF20sSBU (0.58B). Conclusion: The HF 20s, 60s, 120 s followed by silane, promoted similar resin-bond strength to ceramic and the SBU application after HF or MEP did not increase the SBS.
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Journal of Applied Oral Science
- Vol. 28
Open AccessEffect of different surface treatments and multimode adhesive application on the Weibull characteristics, wettability, surface topography and adhesion to CAD/CAM lithium disilicate ceramic
This paper aims to evaluate the effect of different surface treatments on surface topography, wettability, and shear bond strength of resin cement to glass ceramic. Methodology: For SBS test, 32 blocks (7x7x2 mm) of lithium disilicate were obtained and randomly divided into eight groups (four blocks per group) according to each surface treatment (HF 20 s, 60 s, 120 s + silanization/S or Scotch Bond Universal/ SBU) and the Monobond Etch & Prime - MEP application followed or not by SBU. On each treated surface ceramic block, up to four dual-curing resin cement cylinders were prepared and light-cured for 40s (N=120/n=15). The specimens were thermocycled (10,000 cycles, 5-55°C, 30 s) and the SBS test (50KgF, 0.5 mm/min) was performed. Furthermore, failure analysis, wettability, AFM, and SEM were carried out. SBS data (MPa) were analyzed using Student's t-test, two-way ANOVA, Tukey's test (5%) and Weibull's analysis. Results: For HF experimental groups, two-way ANOVA presented the factors “etching time” and “bonding agent” as significant (p<0.05). After silane application, the HF groups presented similar bond strength. SBU application compromised the SBS, except for 120s etching time (HF120sS: 23.39ᵃ±6.48 MPa; HF120sSBU: 18.76ᵃ±8.81MPa). For MEP groups, SBU application did not significantly affect the results (p=0.41). The MEP group presented the highest Weibull modulus (4.08A) and they were statistically different exclusively from the HF20sSBU (0.58B). Conclusion: The HF 20s, 60s, 120 s followed by silane, promoted similar resin-bond strength to ceramic and the SBU application after HF or MEP did not increase the SBS.
- Open Access
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 34, e018
Hydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics
The objective of this study was to evaluate the influence of hydrofluoric acid (HF) concentration, etching time, and application of phosphoric acid (PA) followed by neutralization with sodium bicarbonate on the bond strength between a feldspar ceramic and resin cement. Thus, 80 blocks (10 x 12 x 2 mm) of glass ceramic (VM - Vita Mark II - Vita Zahnfabrik) were made and randomly assigned to eight groups (n =10) according to the factors: HF concentration (5 and 10%), etching time (60 and 120 s), and use of phosphoric acid (PA) (with and without). According to the experimental group, 37% PA (Condac, FGM) was applied after HF etching for 60s. Afterwards, samples were immersed in sodium bicarbonate for 1 min then in an ultrasonic bath in distilled water (5 min) for cleaning. After surface bonding treatment, cylinders (empty set = 2 mm; h = 2 mm) of dual resin cement (AllCem / FGM) were made in the center of each block. The samples were then stored in water (37 degrees C) for 90 days and submitted to the shear bond test (50 KgF, 1 mm/min). Failure analysis was performed by stereomicroscope and scanning electron microscopy. Data (MPa) were analyzed with 3-way ANOVA and Tukey's test. Only the factor "HF concentration" was significant (p = 0.02). Most failures were of cohesive in ceramic (40%) and mixed types (42.5%). The 10% HF resulted in higher shear bond strength value than the 5% HF. Surface cleaning with phosphoric acid followed by sodium bicarbonate and HF time (60 or 120 seconds) did not influence the resin bond strength to feldspar ceramic.
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Brazilian Oral Research
- Vol. 34, e018
Open AccessHydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics
The objective of this study was to evaluate the influence of hydrofluoric acid (HF) concentration, etching time, and application of phosphoric acid (PA) followed by neutralization with sodium bicarbonate on the bond strength between a feldspar ceramic and resin cement. Thus, 80 blocks (10 x 12 x 2 mm) of glass ceramic (VM - Vita Mark II - Vita Zahnfabrik) were made and randomly assigned to eight groups (n =10) according to the factors: HF concentration (5 and 10%), etching time (60 and 120 s), and use of phosphoric acid (PA) (with and without). According to the experimental group, 37% PA (Condac, FGM) was applied after HF etching for 60s. Afterwards, samples were immersed in sodium bicarbonate for 1 min then in an ultrasonic bath in distilled water (5 min) for cleaning. After surface bonding treatment, cylinders (empty set = 2 mm; h = 2 mm) of dual resin cement (AllCem / FGM) were made in the center of each block. The samples were then stored in water (37 degrees C) for 90 days and submitted to the shear bond test (50 KgF, 1 mm/min). Failure analysis was performed by stereomicroscope and scanning electron microscopy. Data (MPa) were analyzed with 3-way ANOVA and Tukey's test. Only the factor "HF concentration" was significant (p = 0.02). Most failures were of cohesive in ceramic (40%) and mixed types (42.5%). The 10% HF resulted in higher shear bond strength value than the 5% HF. Surface cleaning with phosphoric acid followed by sodium bicarbonate and HF time (60 or 120 seconds) did not influence the resin bond strength to feldspar ceramic.