Smelting, homogenizing annealing, traditional extrusion, extrusion-Bc integrated large strain technology, and solid solution aging process were sequentially adopted for an independently designed aluminum alloy. The microstructure and properties of the material were characterized by metallographic microscopy, field emission scanning electron microscope (SEM), EBSD tester of EDAX TEAM, X-ray diffraction (XRD), HV-1000 microhardness tester, and domestic WDW-200 microcomputer-controlled universal testing machine. Experimental results show that the grain size of the aluminum alloy was obviously reduced after the extrusion-Bc ECA processing. The average grain size was reduced from 12.1 μm to 6.9 μm. Although the tensile strength of the alloy was reduced, the plasticity was greatly improved. Moreover, the intergranular corrosion resistance of the alloy was greatly improved. The depth of intergranular corrosion was reduced from 245.0 μm to 39.7 μm, and the grade of intergranular corrosion of the alloy is from grade 4 to grade 3. The extrusion-Bc ECA processing of Al-Zn-Mg-Cu-Zr Alloy followed by solution-aging greatly improves the toughness, intergranular corrosion resistance and decreases grain size of the alloy.